摘要
Self-heating characteristics of a complex nickel-copper sulphide ore stockpile containing pentlandite, chalcopyrite and pyrrhotite have been investigated through continuous monitoring of its inner temperature over a 7-month period (May to December). Variation of external weather parameters such as air temperature, dew point, wind velocity, air humidity and atmospheric pressure are reported. The inner temperature of the stockpile varied from 10.5 degrees C to 44 degrees C. One reason for the maximum temperature to be relatively low is related to lack of reactive surface area since amount of fines in the stockpile is limited. The inner temperatures indicated significant fluctuations due to rapid changes in ambient conditions, particularly the outside temperature, which ranged from -5 degrees C to 32 degrees C. Despite an apparent parallelism between these two types of temperatures, occasional occurrences of rapid decrease in the ambient temperature while the stockpile was still in a self-heating mode were notable. These rapid cooling effects on the stockpile had a retardation effect on trends of increasing inner temperatures. Regular rain showers that the stockpile area received may have also played a role in dissipation of heat, especially when the stockpile experienced a heavy rain. The loss of pentlandite recovery due to stockpile oxidation was about 6.2% compared to 4.0% for chalcopyrite. These losses have been attributed to over-oxidation of these minerals primarily based on development of ferric hydroxy oxide species such as goethite and precipitation of hydroxides of various metal species mobilized as a result of oxidation. Interestingly, floatability of pyrrhotite has been enhanced by stockpile-oxidation. Thus, the flotation selectivity shifts in favour of pyrrhotite for the oxidation case. This behavior was attributed to metal-activation and elemental sulphur/polysulphide formation due to oxidation of the sulphide part of these sulphide minerals. Relative amounts of hydrophilic to hydrophobic species on the surfaces are responsible for observed bench scale behavior.
引用
收藏
页码:249 / 256
页数:8
相关论文
共 50 条
  • [31] Differential flotation of chalcopyrite, pentlandite and pyrrhotite in Ni-Cu sulphide ores
    Kelebek, S
    Wells, PF
    Fekete, SO
    [J]. CANADIAN METALLURGICAL QUARTERLY, 1996, 35 (04) : 329 - 336
  • [32] Magmatic Controls on the Genesis of Ni-Cu±(PGE) Sulphide Mineralisation on Mars
    Baumgartner, Raphael
    Fiorentini, Marco
    Mickiethwaite, Steven
    McCuaig, Campbell
    Baratoux, David
    Sener, Kerim
    Lorand, Jean-Pierre
    [J]. MINERAL RESOURCES IN A SUSTAINABLE WORLD, VOLS 1-5, 2015, : 885 - 888
  • [33] Magmatic controls on the genesis of Ni-Cu± (PGE) sulphide mineralisation on Mars
    Baumgartner, R. J.
    Fiorentini, M. L.
    Baratoux, D.
    Micklethwaite, S.
    Sener, A. K.
    Lorand, J. P.
    McCuaig, T. C.
    [J]. ORE GEOLOGY REVIEWS, 2015, 65 : 400 - 412
  • [34] Effect of production conditions on self-heating propensity of torrefied sawmill residues
    Ceballos, Diana Catalina Cruz
    Hawboldt, Kelly
    Hellleur, Robert
    [J]. FUEL, 2015, 160 : 227 - 237
  • [35] Development of an experimental methodology for sulphide self-heating studies and the self-heating tendency of Vale's Voisey's Bay Concentrator products
    Dai, Zongfu
    [J]. MINERALS ENGINEERING, 2016, 92 : 125 - 133
  • [36] Autooscillations under self-heating conditions in a semiconductor
    A. V. Melkikh
    A. A. Povzner
    [J]. Technical Physics Letters, 2003, 29 : 224 - 225
  • [37] Autooscillations under self-heating conditions in a semiconductor
    Melkikh, AV
    Povzner, AA
    [J]. TECHNICAL PHYSICS LETTERS, 2003, 29 (03) : 224 - 225
  • [38] Modeling the self-heating effect in SiGeHBTs
    Mnif, H
    Zimmer, T
    Battaglia, JL
    Ardouin, B
    [J]. PROCEEDINGS OF THE 2002 BIPOLAR/BICMOS CIRCUITS AND TECHNOLOGY MEETING, 2002, : 96 - 99
  • [39] MODIFICATION OF MOST IV CHARACTERISTICS BY SELF-HEATING
    SHARMA, DK
    RAMANATHAN, KV
    [J]. SOLID-STATE ELECTRONICS, 1984, 27 (11) : 989 - 994
  • [40] HALL AND NERNST EFFECT IN NI AND NI-CU ALLOYS
    WEISER, O
    KOCH, KM
    [J]. ZEITSCHRIFT FUR NATURFORSCHUNG PART A-ASTROPHYSIK PHYSIK UND PHYSIKALISCHE CHEMIE, 1970, A 25 (12): : 1993 - &