Study on Low-Temperature Sintering Behavior of 90W-7Ni-3Fe Alloys: The Influence of Sn Addition

被引:0
|
作者
Wentan Zhu
Yunzhu Ma
Wensheng Liu
Qingshan Cai
Yufeng Huang
Zhongliu Wen
机构
[1] Central South University,National Key Laboratory of Science and Technology for National Defence on High–Strength Structural Materials
[2] Foshan University,School of Materials Science and Energy Engineering
关键词
intermetallic compound; low-temperature sintering behavior; mechanical properties; tin addition; tungsten heavy alloy;
D O I
暂无
中图分类号
学科分类号
摘要
In this work, we investigate low-temperature sintering behavior of the 90W-7Ni-3Fe alloy by introducing Sn. The 90W-7Ni-3Fe alloy with different Sn contents (0, 0.5, 1.0 and 1.5 wt.%) was fabricated via vacuum sintering at 1300 °C for 90 min. When 1 wt.% Sn was added, the liquidus temperature of the 90W-7Ni-3Fe alloy decreased from 1477 to 1265 °C, resulting in rapid densification (relative density increased from 77.77 to 98.59%) and an homogeneous liquid-phase sintered microstructure. Electron probe microanalysis (EPMA) and transmission electron microscopy (TEM) observations revealed that, apart from W and the γ-(Ni, Fe) phase, a new Ni3Sn2 phase appeared in the matrix phase. Furthermore, we discuss in detail the formation of the Ni3Sn2 phase based on element selection theory, which can be associated with the larger atomic radius of Sn and with the negative enthalpy of mixing Sn and Ni. Excessive Sn content (1.5 wt.%) led to the increase in Ni3Sn2 phase, and this deteriorated the relative density and tensile strength of the alloy. The 90W-7Ni-3Fe alloy with the addition of 1 wt.% Sn exhibited a maximum tensile strength value (710 MPa), which was much higher than that of the 90W-7Ni-3Fe alloy that was obtained at 1300 °C. Our findings shed light on further research directions and developed a 90W-6.3Ni-2.1Fe-1Sn alloy for low-temperature sintering.
引用
下载
收藏
页码:5894 / 5901
页数:7
相关论文
共 50 条
  • [11] Elevated temperature tensile behavior and microstructure evolution of liquid phase sintered 90W-7Ni-3Fe alloy
    Li, Mianmian
    Zu, Ming
    Yu, Yang
    Zhang, Wencong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 802 : 528 - 534
  • [12] Sintering process in hot oscillatory pressure of 90W-7Ni-3Fe refractory alloy at different time
    Zhao, Junliang
    Gao, Ka
    Liu, Dongyue
    Ma, Tianyu
    Sun, Dejian
    Gao, Yang
    Pan, Kunming
    An, Linan
    VACUUM, 2022, 195
  • [13] 90W-7Ni-3Fe selective laser melting heat behavior analysis and experimental research
    Zhou, Bokang
    Wei, Zhengying
    Li, Junfeng
    Wu, Yunxiao
    Yang, Lixiang
    Hanjie Xuebao/Transactions of the China Welding Institution, 2020, 41 (11): : 76 - 82
  • [14] Microstructure and strengthening mechanisms of 90W-7Ni-3Fe alloys prepared using laser melting deposition
    Wang, Y. P.
    Ma, S. Y.
    Yang, X. S.
    Zhou, Y. Z.
    Liu, X.
    Li, J. F.
    Zhang, J. J.
    Li, C.
    Wang, X. Y.
    Le, G. M.
    Zhang, Y.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 838
  • [15] Microstructure and fracture behavior of 90W-7Ni-3Fe alloy fabricated by laser directed energy deposition
    Wei, Chao
    Ye, Han
    Zhao, Zhuang
    Tang, Jingang
    Shen, Xianfeng
    Le, Guomin
    Ye, Kun
    Le, Fangbin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 865
  • [16] State and Distribution Characteristics of Yttrium Added in 90W-7Ni-3Fe Alloy
    Fan Jinglian
    Liu Tao
    Peng Shigao
    Qi Meigui
    Tian Jiamin
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 (08) : 1438 - 1441
  • [17] 90W-7Ni-3Fe重合金的断裂与断口分析
    王成福
    陶杰
    机械工程材料, 1986, (03) : 44 - 47
  • [18] Preparation of 90W-7Ni-3Fe Heavy Alloy Sheet by Tape-casting
    Li, Bangyi
    Wu, Fang
    Zhang, Jing
    Feng, Jian
    Shao, Jiajun
    Zhu, Yubin
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2019, 48 (08): : 2616 - 2622
  • [19] Densification, Microstructure and Properties of 90W-7Ni-3Fe Fabricated by Selective Laser Melting
    Li, Junfeng
    Wei, Zhengying
    Zhou, Bokang
    Wu, Yunxiao
    Chen, Sheng-Gui
    Sun, Zhenzhong
    METALS, 2019, 9 (08)
  • [20] Swaging of liquid phase sintered 90W-7Ni-3Fe tungsten heavy alloy