Microstructure and strengthening mechanisms of 90W-7Ni-3Fe alloys prepared using laser melting deposition

被引:29
|
作者
Wang, Y. P. [1 ,3 ]
Ma, S. Y. [1 ,3 ,4 ]
Yang, X. S. [1 ]
Zhou, Y. Z. [1 ]
Liu, X. [1 ]
Li, J. F. [1 ]
Zhang, J. J. [1 ]
Li, C. [3 ]
Wang, X. Y. [1 ]
Le, G. M. [1 ]
Zhang, Y. [2 ]
机构
[1] China Acad Engn Phys, Inst Mat, Mianyang 621908, Sichuan, Peoples R China
[2] Tech Univ Denmark, Dept Mech Engn, DK-2800 Lyngby, Denmark
[3] North China Univ Technol, Dept Mat Sci & Engn, Coll Mech & Mat Engn, Beijing 100144, Peoples R China
[4] SLM Solut Shanghai Co Ltd, Shanghai 201100, Peoples R China
基金
欧洲研究理事会; 中国国家自然科学基金;
关键词
W-NI-FE; TUNGSTEN HEAVY ALLOYS; HALL-PETCH; PROCESSING PARAMETERS; GRAPHITE NODULES; FLOW-STRESS; TENSILE; CU; DENSIFICATION; EVOLUTION;
D O I
10.1016/j.jallcom.2020.155545
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The microstructure and mechanical properties of a 90W–7Ni–3Fe heavy alloy manufactured using laser melting deposition (LMD) have been investigated with a goal of understanding the LMD process and the relevant strengthening mechanisms. A reference sample prepared using liquid phase sintering (LPS) with similar composition has been used for comparison to isolate effects of the processing rate. The results show that the nearly fully-dense LMD sample consists of two periodically alternating sublayers containing different volume fractions of W particles. Compared to the reference LPS sample, the LMD sample has a higher W content in the binder matrix, a more refined microstructure, a higher dislocation density and a lower contiguity between W particles. Furthermore, the LMD sample has a yield strength of 822 ± 30 MPa, which is about 200 MPa higher than that of the reference LPS sample. This strength difference is quantitatively analyzed based on the microstructural observations. It is shown that the increased fraction of W-matrix interfaces, a higher interface bonding strength and more pronounced constraint effects, resulting from the higher processing temperature and fast cooling of LMD, provide extra strengthening. The present study provides an important basis for optimizing the LMD process for manufacture of high W content tungsten heavy alloys with improved mechanical properties. © 2020 Elsevier B.V.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Densification, Microstructure and Properties of 90W-7Ni-3Fe Fabricated by Selective Laser Melting
    Li, Junfeng
    Wei, Zhengying
    Zhou, Bokang
    Wu, Yunxiao
    Chen, Sheng-Gui
    Sun, Zhenzhong
    METALS, 2019, 9 (08)
  • [2] Densification, microstructural evolutions of 90W-7Ni-3Fe tungsten heavy alloys during laser melting deposition process
    Li, Chun
    Wang, Yingpei
    Ma, Shiyu
    Yang, Xiaoshan
    Li, Jinfeng
    Zhou, Yuzhao
    Liu, Xue
    Tang, Jingang
    Wang, Xiaoying
    Le, Guomin
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2020, 91 (91):
  • [3] Laser melting deposition of fine-grained 90W-7Ni-3Fe alloys using pre-sintered granulated powder
    Zhang, Wei
    Li, Chun
    Zhou, Yuzhao
    Yang, Xiaoshan
    Song, Jiupeng
    Wang, Dou
    Zhang, Yubin
    Le, Guomin
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2024, 119
  • [4] Microstructure and fracture behavior of 90W-7Ni-3Fe alloy fabricated by laser directed energy deposition
    Wei, Chao
    Ye, Han
    Zhao, Zhuang
    Tang, Jingang
    Shen, Xianfeng
    Le, Guomin
    Ye, Kun
    Le, Fangbin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 865
  • [5] Microstructure and strengthening mechanisms of tantalum prepared using laser melting deposition
    Guan, Baosheng
    Xu, Minggang
    Yang, Xiaoshan
    Zhou, Yuzhao
    Li, Chun
    Ji, Yaqi
    Liu, Xue
    Li, Jinfeng
    Wang, Dou
    Tang, Jingang
    Le, Guomin
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2022, 103
  • [6] 90W-7Ni-3Fe selective laser melting heat behavior analysis and experimental research
    Zhou, Bokang
    Wei, Zhengying
    Li, Junfeng
    Wu, Yunxiao
    Yang, Lixiang
    Hanjie Xuebao/Transactions of the China Welding Institution, 2020, 41 (11): : 76 - 82
  • [7] Effects of processing parameters on rapid manufacturing 90W-7Ni-3Fe parts via selective laser melting
    Li, R. D.
    Liu, J. H.
    Shi, Y. S.
    Zhang, L.
    Du, M. Z.
    POWDER METALLURGY, 2010, 53 (04) : 310 - 317
  • [8] Effect of heating mode and sintering temperature on the consolidation of 90W-7Ni-3Fe alloys
    Mondal, Avijit
    Upadhyaya, Anish
    Agrawal, Dinesh
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (02) : 301 - 310
  • [9] Influence of Heat Treatment on the Mechanical Properties of 90W-7Ni-3Fe Heavy Alloys.
    Korea Tungsten Mining Co, Daegu
    Henig, Ernst-Theo
    Petzow, Guenter
    Zeitschrift fuer Metallkunde/Materials Research and Advanced Techniques, 1987, 78 (04): : 250 - 258
  • [10] Sintering properties of nanosized 90W-7Ni-3Fe composite powder
    Ma, Yunzhu
    Liu, Wensheng
    Huang, Baiyun
    Fan, Jinglian
    JOURNAL OF NANOPARTICLE RESEARCH, 2008, 10 (06) : 1053 - 1058