Microstructure and strengthening mechanisms of 90W-7Ni-3Fe alloys prepared using laser melting deposition

被引:33
|
作者
Wang, Y. P. [1 ,3 ]
Ma, S. Y. [1 ,3 ,4 ]
Yang, X. S. [1 ]
Zhou, Y. Z. [1 ]
Liu, X. [1 ]
Li, J. F. [1 ]
Zhang, J. J. [1 ]
Li, C. [3 ]
Wang, X. Y. [1 ]
Le, G. M. [1 ]
Zhang, Y. [2 ]
机构
[1] China Acad Engn Phys, Inst Mat, Mianyang 621908, Sichuan, Peoples R China
[2] Tech Univ Denmark, Dept Mech Engn, DK-2800 Lyngby, Denmark
[3] North China Univ Technol, Dept Mat Sci & Engn, Coll Mech & Mat Engn, Beijing 100144, Peoples R China
[4] SLM Solut Shanghai Co Ltd, Shanghai 201100, Peoples R China
基金
欧洲研究理事会; 中国国家自然科学基金;
关键词
W-NI-FE; TUNGSTEN HEAVY ALLOYS; HALL-PETCH; PROCESSING PARAMETERS; GRAPHITE NODULES; FLOW-STRESS; TENSILE; CU; DENSIFICATION; EVOLUTION;
D O I
10.1016/j.jallcom.2020.155545
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The microstructure and mechanical properties of a 90W–7Ni–3Fe heavy alloy manufactured using laser melting deposition (LMD) have been investigated with a goal of understanding the LMD process and the relevant strengthening mechanisms. A reference sample prepared using liquid phase sintering (LPS) with similar composition has been used for comparison to isolate effects of the processing rate. The results show that the nearly fully-dense LMD sample consists of two periodically alternating sublayers containing different volume fractions of W particles. Compared to the reference LPS sample, the LMD sample has a higher W content in the binder matrix, a more refined microstructure, a higher dislocation density and a lower contiguity between W particles. Furthermore, the LMD sample has a yield strength of 822 ± 30 MPa, which is about 200 MPa higher than that of the reference LPS sample. This strength difference is quantitatively analyzed based on the microstructural observations. It is shown that the increased fraction of W-matrix interfaces, a higher interface bonding strength and more pronounced constraint effects, resulting from the higher processing temperature and fast cooling of LMD, provide extra strengthening. The present study provides an important basis for optimizing the LMD process for manufacture of high W content tungsten heavy alloys with improved mechanical properties. © 2020 Elsevier B.V.
引用
收藏
页数:10
相关论文
共 50 条
  • [41] Sintering process in hot oscillatory pressure of 90W-7Ni-3Fe refractory alloy at different time
    Zhao, Junliang
    Gao, Ka
    Liu, Dongyue
    Ma, Tianyu
    Sun, Dejian
    Gao, Yang
    Pan, Kunming
    An, Linan
    VACUUM, 2022, 195
  • [42] 90W-7Ni-3Fe激光选区熔化热行为及试验分析
    周博康
    魏正英
    李俊峰
    吴云肖
    杨理想
    焊接学报, 2020, 41 (11) : 76 - 82+101
  • [43] EFFECT OF COLD WORK AND ANNEALING ON THE MECHANICAL-PROPERTIES OF 90W-7NI-3FE HEAVY ALLOY
    SRIKANTH, V
    UPADHYAYA, GS
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1988, 7 (03) : 195 - 197
  • [44] 纳米ZrC粉末对90W-7Ni-3Fe合金组织及性能影响
    苏旭文
    何志
    闫树欣
    董龙龙
    孙国栋
    粉末冶金技术, 2025, 43 (01) : 86 - 93
  • [45] Hot Oscillation Pressure Sintered and Post Heat Treated 90W-7NI-3FE Refractory Alloy
    Ka Gao
    Wei Zhao
    Weidong Li
    Wei Liu
    Linan An
    JOM, 2023, 75 : 2535 - 2542
  • [46] INCREASING AMPLITUDE AT LOW TEMPERATURES TO OBTAIN 90W-7Ni-3Fe REFRACTORY ALLOY WITH EXCELLENT CORROSION RESISTANCE PREPARED BY HOT OSCILLATORY PRESSING
    Hu, Yanghu
    Gao, Ka
    Li, Qiang
    Ren, Chunyang
    Sun, Dejian
    Gao, Yang
    Dang, Li
    Guo, Biao
    POWDER METALLURGY AND METAL CERAMICS, 2024, 63 (5-6) : 272 - 279
  • [47] 纳米级90W-7Ni-3Fe复合粉末的低温烧结机制
    马运柱
    黄伯云
    范景莲
    熊翔
    汪登龙
    稀有金属材料与工程, 2005, (10) : 153 - 157
  • [48] Experimental studies of oxygen and carbon segregation at the interfacial boundaries of a 90W-7Ni-3Fe tungsten heavy alloy
    Fortuna, E
    Sikorski, K
    Kurzydlowski, KJ
    MATERIALS CHARACTERIZATION, 2004, 52 (4-5) : 323 - 329
  • [49] 稀土钇对纳米粉90W-7Ni-3Fe合金烧结特性的影响
    马运柱
    黄伯云
    熊翔
    中国有色金属学报, 2005, (06) : 882 - 887
  • [50] 90W-7Ni-3Fe纳米晶粉末的瞬时液相强化烧结特征
    范景莲
    汪登龙
    曹建虎
    中国有色金属学报, 2005, (02) : 217 - 223