Study on Low-Temperature Sintering Behavior of 90W-7Ni-3Fe Alloys: The Influence of Sn Addition

被引:0
|
作者
Wentan Zhu
Yunzhu Ma
Wensheng Liu
Qingshan Cai
Yufeng Huang
Zhongliu Wen
机构
[1] Central South University,National Key Laboratory of Science and Technology for National Defence on High–Strength Structural Materials
[2] Foshan University,School of Materials Science and Energy Engineering
关键词
intermetallic compound; low-temperature sintering behavior; mechanical properties; tin addition; tungsten heavy alloy;
D O I
暂无
中图分类号
学科分类号
摘要
In this work, we investigate low-temperature sintering behavior of the 90W-7Ni-3Fe alloy by introducing Sn. The 90W-7Ni-3Fe alloy with different Sn contents (0, 0.5, 1.0 and 1.5 wt.%) was fabricated via vacuum sintering at 1300 °C for 90 min. When 1 wt.% Sn was added, the liquidus temperature of the 90W-7Ni-3Fe alloy decreased from 1477 to 1265 °C, resulting in rapid densification (relative density increased from 77.77 to 98.59%) and an homogeneous liquid-phase sintered microstructure. Electron probe microanalysis (EPMA) and transmission electron microscopy (TEM) observations revealed that, apart from W and the γ-(Ni, Fe) phase, a new Ni3Sn2 phase appeared in the matrix phase. Furthermore, we discuss in detail the formation of the Ni3Sn2 phase based on element selection theory, which can be associated with the larger atomic radius of Sn and with the negative enthalpy of mixing Sn and Ni. Excessive Sn content (1.5 wt.%) led to the increase in Ni3Sn2 phase, and this deteriorated the relative density and tensile strength of the alloy. The 90W-7Ni-3Fe alloy with the addition of 1 wt.% Sn exhibited a maximum tensile strength value (710 MPa), which was much higher than that of the 90W-7Ni-3Fe alloy that was obtained at 1300 °C. Our findings shed light on further research directions and developed a 90W-6.3Ni-2.1Fe-1Sn alloy for low-temperature sintering.
引用
收藏
页码:5894 / 5901
页数:7
相关论文
共 50 条
  • [21] Densification, microstructural evolutions of 90W-7Ni-3Fe tungsten heavy alloys during laser melting deposition process
    Li, Chun
    Wang, Yingpei
    Ma, Shiyu
    Yang, Xiaoshan
    Li, Jinfeng
    Zhou, Yuzhao
    Liu, Xue
    Tang, Jingang
    Wang, Xiaoying
    Le, Guomin
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2020, 91 (91):
  • [22] Preparation of 90W-7Ni-3Fe Heavy Alloy Sheet by Tape-casting
    Li Bangyi
    Wu Fang
    Zhang Jing
    Feng Jian
    Shao Jiajun
    Zhu Yubin
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (08) : 2616 - 2622
  • [23] Effect of Strain Rate on the Plastic Deformation and Fracture of 90W-7Ni-3Fe Alloy Prepared by Liquid-Phase Sintering
    Yu, Yang
    Zu, Ming
    Ren, Chaoyuan
    Zhang, Wencong
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (12) : 6606 - 6615
  • [24] Effect of Strain Rate on the Plastic Deformation and Fracture of 90W-7Ni-3Fe Alloy Prepared by Liquid-Phase Sintering
    Yang Yu
    Ming Zu
    Chaoyuan Ren
    Wencong Zhang
    Journal of Materials Engineering and Performance, 2018, 27 : 6606 - 6615
  • [25] Effect of the Mechanical Activation Time on the Density of Fine-Grained 90W-7Ni-3Fe Alloy Synthesized by Spark Plasma Sintering
    Chuvil'deev, V. N.
    Nokhrin, A. V.
    Boldin, M. S.
    Lantsev, E. A.
    Sakharov, N. V.
    PHYSICS OF METALS AND METALLOGRAPHY, 2023, 124 (10): : 987 - 994
  • [26] 纳米级90W-7Ni-3Fe复合粉末的烧结特性
    马运柱
    黄伯云
    范景莲
    熊翔
    汪登龙
    中国有色金属学报, 2004, (08) : 1382 - 1388
  • [27] 纳米晶90W-7Ni-3Fe复合粉末的注射成形
    范景莲
    曲选辉
    黄伯云
    郭萍
    粉末冶金材料科学与工程, 2000, (02) : 146 - 150
  • [28] Effect of Cu addition on W-Ni-Fe alloys sintered at a low temperature
    Wang, CB
    Shen, Q
    Zhang, LM
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2002, 18 (03) : 234 - 236
  • [30] 液相烧结的90W-7Ni-3Fe合金的形变与断裂
    杜家驹
    时元龙
    金属学报, 1983, (04) : 102 - 107