Comparison of the biodegradability of various polyethylene films containing pro-oxidant additives

被引:120
|
作者
Fontanella, Stephane [2 ,3 ]
Bonhomme, Sylvie [2 ]
Koutny, Marek [4 ]
Husarova, Lucie [4 ]
Brusson, Jean-Michel [5 ]
Courdavault, Jean-Paul [9 ]
Pitteri, Silvio [6 ]
Samuel, Guy [7 ]
Pichon, Gerard [8 ]
Lemaire, Jacques [2 ]
Delort, Anne-Marie [1 ,3 ]
机构
[1] CNRS, UMR 6504, F-63177 Aubiere, France
[2] Univ Blaise Pascal, CNEP, F-63177 Aubiere, France
[3] Clermont Univ, UBP, Lab SEESIB, F-63000 Clermont Ferrand, France
[4] Tomas Bata Univ Zlin, Fac Technol, Dept Environm Engn, Zlin 76272, Czech Republic
[5] Total Petrochem Res Feluy, B-7181 Feluy, Belgium
[6] Basell Poliolefine Italia Srl, G Natta R&D Res Ctr, I-44100 Ferrara, Italy
[7] Assoc NEOSAC, F-43600 Ste Sigolene, France
[8] Grp Extrus Souflage Ste Sigolene E3S, F-43600 Ste Sigolene, France
[9] LyondellBasell, Lyon, France
关键词
Polyethylene; Biodegradation; Pro-oxidant; Photooxidation; Thermal oxidation; DEGRADATION;
D O I
10.1016/j.polymdegradstab.2010.03.009
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The biodegradability of high density polyethylene films (HDPE), low density polyethylene films (LDPE) and linear low density polyethylene films (LLDPE) with a balanced content of antioxidants and pro-oxidants (manganese + iron or manganese + iron + cobalt) was studied. Abiotic pre-treatment consisting of photooxidation and thermal oxidation corresponding to about three years of outdoor weathering (including 3-4 months of exposure to daylight) was monitored by FTIR and SEC measurements. The oxidized samples were then inoculated with the strain Rhodococcus rhodochrous in mineral medium, and incubated up to 180 days. The metabolic activity of the bacteria was assessed by measuring adenosine triphosphate content (ATP) and the viability of the cells. Complementary experiments were performed by H-1 NMR spectroscopy to monitor the biodegradation of soluble molecules excreted from the polymer in the incubation medium. Finally SEM was used to visualize the formation of a biofilm at the surface of the polymer. Three samples among the 12 tested were investigated in compost and soil environments. The results show that the main factor controlling the biodegradability of the polyethylene films is the nature of the pro-oxidant additive and to a lesser extent that of the matrix. Except for the samples containing very high content of cobalt additive, the various polymer films were used as substrates by the bacteria. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1011 / 1021
页数:11
相关论文
共 50 条
  • [41] An organic bioactive pro-oxidant behavior in thermal degradation kinetics of polypropylene films
    Tavares, Lara B.
    Rocha, Rafaela G.
    Rosa, Derval S.
    IRANIAN POLYMER JOURNAL, 2017, 26 (04) : 273 - 280
  • [42] Thermal characterization of the oxo-degradation of polypropylene containing a pro-oxidant/pro-degradant additive
    Contat-Rodrigo, L.
    POLYMER DEGRADATION AND STABILITY, 2013, 98 (11) : 2117 - 2124
  • [43] Preparation and Characterization of Oxo-degradable Polypropylene Composites Containing a Modified Pro-oxidant
    Sunil Sable
    Sanjeev Ahuja
    Haripada Bhunia
    Journal of Polymers and the Environment, 2021, 29 : 721 - 733
  • [44] Efficient enhancement in polyethylene biodegradation as a consequence of oxidative fragmentation promoted by pro-oxidant/pro-degradant metal stearate
    Kerouani, Samira
    Djerboua, Ferhat
    Sadoun, Tahar
    JOURNAL OF POLYMER ENGINEERING, 2018, 38 (07) : 625 - 634
  • [45] Preparation and Characterization of Oxo-degradable Polypropylene Composites Containing a Modified Pro-oxidant
    Sable, Sunil
    Ahuja, Sanjeev
    Bhunia, Haripada
    JOURNAL OF POLYMERS AND THE ENVIRONMENT, 2021, 29 (03) : 721 - 733
  • [46] Effect of pro-oxidant concentration on characteristics of packaging films of cobalt stearate filled polypropylene
    Sable, Sunil
    Ahuja, Sanjeev
    Bhunia, Haripada
    JOURNAL OF POLYMER ENGINEERING, 2020, 40 (08) : 637 - 646
  • [47] Defining the ascorbic acid crossover from anti-oxidant to pro-oxidant in a model wine matrix containing (+)-catechin
    Bradshaw, MP
    Cheynier, V
    Scollary, GR
    Prenzler, PD
    JOURNAL OF AGRICULTURAL AND FOOD CHEMISTRY, 2003, 51 (14) : 4126 - 4132
  • [48] Weathering Effects on Degradation of Low-Density Polyethylene-Nanosilica Composite with Added Pro-oxidant
    Zepp, Richard G. G.
    Acrey, Brad
    Davis, Mary J. B.
    Andrady, Anthony L. L.
    Locklin, Jason
    Arnold, Rachelle
    Okungbowa, Osadolor
    Commodore, Adwoa
    JOURNAL OF POLYMERS AND THE ENVIRONMENT, 2023, 31 (10) : 4184 - 4192
  • [49] Weathering Effects on Degradation of Low-Density Polyethylene-Nanosilica Composite with Added Pro-oxidant
    Richard G. Zepp
    Brad Acrey
    Mary J. B. Davis
    Anthony L. Andrady
    Jason Locklin
    Rachelle Arnold
    Osadolor Okungbowa
    Adwoa Commodore
    Journal of Polymers and the Environment, 2023, 31 : 4184 - 4192
  • [50] A study on the effect of pro-oxidant on the thermo-oxidative degradation behaviour of sago starch filled polyethylene
    Sharma, N
    Chang, LP
    Chu, YL
    Ismail, H
    Ishiaku, US
    Ishak, ZAM