Comparison of the biodegradability of various polyethylene films containing pro-oxidant additives

被引:120
|
作者
Fontanella, Stephane [2 ,3 ]
Bonhomme, Sylvie [2 ]
Koutny, Marek [4 ]
Husarova, Lucie [4 ]
Brusson, Jean-Michel [5 ]
Courdavault, Jean-Paul [9 ]
Pitteri, Silvio [6 ]
Samuel, Guy [7 ]
Pichon, Gerard [8 ]
Lemaire, Jacques [2 ]
Delort, Anne-Marie [1 ,3 ]
机构
[1] CNRS, UMR 6504, F-63177 Aubiere, France
[2] Univ Blaise Pascal, CNEP, F-63177 Aubiere, France
[3] Clermont Univ, UBP, Lab SEESIB, F-63000 Clermont Ferrand, France
[4] Tomas Bata Univ Zlin, Fac Technol, Dept Environm Engn, Zlin 76272, Czech Republic
[5] Total Petrochem Res Feluy, B-7181 Feluy, Belgium
[6] Basell Poliolefine Italia Srl, G Natta R&D Res Ctr, I-44100 Ferrara, Italy
[7] Assoc NEOSAC, F-43600 Ste Sigolene, France
[8] Grp Extrus Souflage Ste Sigolene E3S, F-43600 Ste Sigolene, France
[9] LyondellBasell, Lyon, France
关键词
Polyethylene; Biodegradation; Pro-oxidant; Photooxidation; Thermal oxidation; DEGRADATION;
D O I
10.1016/j.polymdegradstab.2010.03.009
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The biodegradability of high density polyethylene films (HDPE), low density polyethylene films (LDPE) and linear low density polyethylene films (LLDPE) with a balanced content of antioxidants and pro-oxidants (manganese + iron or manganese + iron + cobalt) was studied. Abiotic pre-treatment consisting of photooxidation and thermal oxidation corresponding to about three years of outdoor weathering (including 3-4 months of exposure to daylight) was monitored by FTIR and SEC measurements. The oxidized samples were then inoculated with the strain Rhodococcus rhodochrous in mineral medium, and incubated up to 180 days. The metabolic activity of the bacteria was assessed by measuring adenosine triphosphate content (ATP) and the viability of the cells. Complementary experiments were performed by H-1 NMR spectroscopy to monitor the biodegradation of soluble molecules excreted from the polymer in the incubation medium. Finally SEM was used to visualize the formation of a biofilm at the surface of the polymer. Three samples among the 12 tested were investigated in compost and soil environments. The results show that the main factor controlling the biodegradability of the polyethylene films is the nature of the pro-oxidant additive and to a lesser extent that of the matrix. Except for the samples containing very high content of cobalt additive, the various polymer films were used as substrates by the bacteria. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1011 / 1021
页数:11
相关论文
共 50 条
  • [31] Comparison of the effects of dehydroepiandrosterone and analogs on arrhythmia and pro-oxidant damage
    Peng, XD
    Xu, DH
    Mei, XT
    Ma, QD
    Lv, JY
    Xu, SB
    DRUG DEVELOPMENT RESEARCH, 2005, 66 (03) : 227 - 227
  • [32] Thermal degradation studies of LDPE containing cobalt stearate as pro-oxidant
    Roy, P. K.
    Surekha, P.
    Rajagopal, C.
    Choudhary, V.
    EXPRESS POLYMER LETTERS, 2007, 1 (04): : 208 - 216
  • [33] Photodegradation and biodegradation by bacteria of mulching films based on ethylene-vinyl acetate copolymer: Effect of pro-oxidant additives
    Abrusci, C.
    Pablos, J. L.
    Marin, I.
    Espi, E.
    Corrales, T.
    Catalina, F.
    JOURNAL OF APPLIED POLYMER SCIENCE, 2012, 126 (05) : 1664 - 1675
  • [34] Biodegradation of Pro-oxidant Filled Polypropylene Films and Evaluation of the Ecotoxicological Impact
    Mandal, Dev K.
    Bhunia, Haripada
    Bajpai, Pramod K.
    Kumar, Anil
    Madhu, Gaurav
    Nando, Golok B.
    JOURNAL OF POLYMERS AND THE ENVIRONMENT, 2018, 26 (03) : 1061 - 1071
  • [35] Biodegradation of Pro-oxidant Filled Polypropylene Films and Evaluation of the Ecotoxicological Impact
    Dev K. Mandal
    Haripada Bhunia
    Pramod K. Bajpai
    Anil Kumar
    Gaurav Madhu
    Golok B. Nando
    Journal of Polymers and the Environment, 2018, 26 : 1061 - 1071
  • [36] Thermo-oxidative aging of low density polyethylene blown films in presence of cellulose nanocrystals and a pro-oxidant additive
    Moo-Tun, Nora M.
    Valadez-Gonzalez, Alex
    Uribe-Calderon, Jorge A.
    POLYMER BULLETIN, 2018, 75 (07) : 3149 - 3169
  • [37] Effect of colorant, thickness, and pro-oxidant loading on degradation of low-density polyethylene films during thermal aging
    Maalihan, Reymark D.
    Pajarito, Bryan B.
    JOURNAL OF PLASTIC FILM & SHEETING, 2016, 32 (02) : 124 - 139
  • [38] Thermo-oxidative aging of low density polyethylene blown films in presence of cellulose nanocrystals and a pro-oxidant additive
    Nora M. Moo-Tun
    Alex Valadez-González
    Jorge A. Uribe-Calderon
    Polymer Bulletin, 2018, 75 : 3149 - 3169
  • [39] Photodegradation of polyethylenes: Comparative effect of Fe and Ca-stearates as pro-oxidant additives
    Pablos, J. L.
    Abrusci, C.
    Marin, I.
    Lopez-Marin, J.
    Catalina, F.
    Espi, E.
    Corrales, T.
    POLYMER DEGRADATION AND STABILITY, 2010, 95 (10) : 2057 - 2064
  • [40] An organic bioactive pro-oxidant behavior in thermal degradation kinetics of polypropylene films
    Lara B. Tavares
    Rafaela G. Rocha
    Derval S. Rosa
    Iranian Polymer Journal, 2017, 26 : 273 - 280