Comparison of the biodegradability of various polyethylene films containing pro-oxidant additives

被引:120
|
作者
Fontanella, Stephane [2 ,3 ]
Bonhomme, Sylvie [2 ]
Koutny, Marek [4 ]
Husarova, Lucie [4 ]
Brusson, Jean-Michel [5 ]
Courdavault, Jean-Paul [9 ]
Pitteri, Silvio [6 ]
Samuel, Guy [7 ]
Pichon, Gerard [8 ]
Lemaire, Jacques [2 ]
Delort, Anne-Marie [1 ,3 ]
机构
[1] CNRS, UMR 6504, F-63177 Aubiere, France
[2] Univ Blaise Pascal, CNEP, F-63177 Aubiere, France
[3] Clermont Univ, UBP, Lab SEESIB, F-63000 Clermont Ferrand, France
[4] Tomas Bata Univ Zlin, Fac Technol, Dept Environm Engn, Zlin 76272, Czech Republic
[5] Total Petrochem Res Feluy, B-7181 Feluy, Belgium
[6] Basell Poliolefine Italia Srl, G Natta R&D Res Ctr, I-44100 Ferrara, Italy
[7] Assoc NEOSAC, F-43600 Ste Sigolene, France
[8] Grp Extrus Souflage Ste Sigolene E3S, F-43600 Ste Sigolene, France
[9] LyondellBasell, Lyon, France
关键词
Polyethylene; Biodegradation; Pro-oxidant; Photooxidation; Thermal oxidation; DEGRADATION;
D O I
10.1016/j.polymdegradstab.2010.03.009
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The biodegradability of high density polyethylene films (HDPE), low density polyethylene films (LDPE) and linear low density polyethylene films (LLDPE) with a balanced content of antioxidants and pro-oxidants (manganese + iron or manganese + iron + cobalt) was studied. Abiotic pre-treatment consisting of photooxidation and thermal oxidation corresponding to about three years of outdoor weathering (including 3-4 months of exposure to daylight) was monitored by FTIR and SEC measurements. The oxidized samples were then inoculated with the strain Rhodococcus rhodochrous in mineral medium, and incubated up to 180 days. The metabolic activity of the bacteria was assessed by measuring adenosine triphosphate content (ATP) and the viability of the cells. Complementary experiments were performed by H-1 NMR spectroscopy to monitor the biodegradation of soluble molecules excreted from the polymer in the incubation medium. Finally SEM was used to visualize the formation of a biofilm at the surface of the polymer. Three samples among the 12 tested were investigated in compost and soil environments. The results show that the main factor controlling the biodegradability of the polyethylene films is the nature of the pro-oxidant additive and to a lesser extent that of the matrix. Except for the samples containing very high content of cobalt additive, the various polymer films were used as substrates by the bacteria. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1011 / 1021
页数:11
相关论文
共 50 条
  • [21] Thermal degradation of high-impact polystyrene with pro-oxidant additives
    Francisco J. Arráez
    María Luisa Arnal
    Alejandro J. Müller
    Polymer Bulletin, 2019, 76 : 1489 - 1515
  • [22] Comparative effect of metal stearates as pro-oxidant additives on bacterial biodegradation of thermal- and photo-degraded low density polyethylene mulching films
    Abrusci, C.
    Pablos, J. L.
    Marín, I.
    Espí, E.
    Corrales, T.
    Catalina, F.
    INTERNATIONAL BIODETERIORATION & BIODEGRADATION, 2013, 83 : 25 - 32
  • [23] Bio-based Polyethylene-Lignin Composites Containing a Pro-oxidant/Pro-degradant Additive: Preparation and Characterization
    Samal, Sangram K.
    Fernandes, E. G.
    Corti, Andrea
    Chiellini, Emo
    JOURNAL OF POLYMERS AND THE ENVIRONMENT, 2014, 22 (01) : 58 - 68
  • [24] A study of the controlled degradation of polypropylene containing pro-oxidant agents
    de Carvalho, Celso Luis
    Silveira, Alexandre F.
    Rosa, Derval dos Santos
    SPRINGERPLUS, 2013, 2 : 1 - 11
  • [25] Biodegradation of photo-degraded mulching films based on polyethylenes and stearates of calcium and iron as pro-oxidant additives
    Abrusci, C.
    Pablos, J. L.
    Corrales, T.
    Lopez-Marin, J.
    Marin, I.
    Catalina, E.
    INTERNATIONAL BIODETERIORATION & BIODEGRADATION, 2011, 65 (03) : 451 - 459
  • [26] Comparison of the behaviour of pro-oxidant additive containing plastic degradation in the unmanaged natural environment and in the laboratory
    Sciscione, Fabiola
    Prout, Luba
    Jeffries, Jack W. E.
    Karam, Hajar J.
    Constantinou, Achilleas
    Peng, Fei
    Al-Salem, S. M.
    Hailes, Helen C.
    Miodownik, Mark
    ROYAL SOCIETY OPEN SCIENCE, 2025, 12 (03):
  • [27] PRO-OXIDANT AND ANTI-OXIDANT PROPERTIES OF SEVERAL THIOL-CONTAINING COMPOUNDS
    HAENEN, GRMM
    BAST, A
    PHARMACEUTISCH WEEKBLAD-SCIENTIFIC EDITION, 1984, 6 (06) : 260 - 260
  • [28] Comparison of the cytotoxic, pro-oxidant and pro-inflammatory characteristics of different oxysterols
    S. Lemaire-Ewing
    C. Prunet
    T. Montange
    A. Vejux
    A. Berthier
    G. Bessède
    L. Corcos
    P. Gambert
    D. Néel
    G. Lizard
    Cell Biology and Toxicology, 2005, 21 : 97 - 114
  • [29] Insights into the evaluation of the abiotic and biotic degradation rate of commercial pro-oxidant filled polyethylene (PE) thin films
    Al-Salem, S. M.
    Al-Hazza'a, A.
    Karam, H. J.
    Al-Wadi, M. H.
    Al-Dhafeeri, A. T.
    Al-Rowaih, A. A.
    JOURNAL OF ENVIRONMENTAL MANAGEMENT, 2019, 250
  • [30] Comparison of the cytotoxic, pro-oxidant and pro-inflammatory characteristics of different oxysterols
    Lemaire-Ewing, S
    Prunet, C
    Montange, T
    Vejux, A
    Berthier, A
    Bessède, G
    Corcos, L
    Gambert, P
    Néel, D
    Lizard, G
    CELL BIOLOGY AND TOXICOLOGY, 2005, 21 (02) : 97 - 114