Effect of carbon fiber volume fraction on 6H to 4H-SiC polytype transformation

被引:4
|
作者
Moslemi, Mahboubeh [1 ]
Razavi, Mansour [1 ]
Zakeri, Mohammad [1 ]
Rahimipour, Mohammad Reza [1 ]
Schreiner, Marcus [2 ]
机构
[1] Mat & Energy Res Ctr, Dept Ceram, Karaj, Iran
[2] TU Bergakad Freiberg, Inst Energy Proc Engn & Chem Engn, Freiberg, Germany
关键词
alpha-SiC; spark plasma sintering; polytype transformation; Rietveld; SILICON-CARBIDE CERAMICS; REINFORCED SIC COMPOSITES; MECHANICAL-PROPERTIES; INFILTRATION; MICROSTRUCTURE; FABRICATION; ADDITIVES; POWDERS;
D O I
10.1080/01411594.2018.1481214
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
In this study, polycrystalline -SiC composed of 55.7wt.% 6H-SiC, 35.1wt.% 4H-SiC with different volume fractions of carbon fibers (0-5-10-15-20%) was successfully sintered by spark plasma sintering technique at 2000 degrees C and 35MPa of applied pressure. The micrographs obtained from scanning electron microscopy revealed that the sintered samples were composed of equiaxed SiC grains. Results indicated that the presence of carbon fibers retarded the SiC densification process, decreased their relative densities and increased their porosity. Additionally, according to quantitative phase analysis by the Rietveld method during the sintering step, it was found that the 6H to 4H transformation has taken place. Increasing the carbon fibers content accelerated this trend as the sample containing 20vol.% carbon fiber was consisted of 85.5wt.% 4H-SiC.
引用
收藏
页码:733 / 741
页数:9
相关论文
共 50 条
  • [41] Nano 6H diamond polytype polycrystalline powder
    Ownby, PD
    NSTI NANOTECH 2004, VOL 3, TECHNICAL PROCEEDINGS, 2004, : 210 - 213
  • [42] Photoluminescence and Zeeman effect in chromium-doped 4H and 6H SiC
    Son, NT
    Ellison, A
    Magnusson, B
    MacMillan, MF
    Chen, WM
    Monemar, B
    Janzén, E
    JOURNAL OF APPLIED PHYSICS, 1999, 86 (08) : 4348 - 4353
  • [43] Annealing effect on surfaces of 4H(6H)-SiC(0001)Si face
    Tsukamoto, T
    Hirai, M
    Kusaka, M
    Iwami, M
    Ozawa, T
    Nagamura, T
    Nakata, T
    APPLIED SURFACE SCIENCE, 1997, 113 : 467 - 471
  • [44] Role of carbon in the formation of ohmic contact in Ni/4H-SiC and Ni/Ti/4H-SiC
    Siad, M.
    Abdesslam, M.
    Chami, A. C.
    APPLIED SURFACE SCIENCE, 2012, 258 (18) : 6819 - 6822
  • [45] Optical investigation of residual doping species in 6H and 4H-SIC layers grown by chemical vapor deposition
    Neyret, E
    Ferro, G
    Juillaguet, S
    Bluet, JM
    Jaussaud, C
    Camassel, J
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 1999, 61-2 : 253 - 257
  • [46] Solution growth of single crystalline 6H, 4H-SiC using Si-Ti-C melt
    Kamei, Kazuhito
    Kusunoki, Kazuhiko
    Yashiro, Nobuyoshi
    Okada, Nobuhiro
    Tanaka, Tsutomu
    Yauchi, Akihiro
    JOURNAL OF CRYSTAL GROWTH, 2009, 311 (03) : 855 - 858
  • [47] MECHANISM OF 2H-]6H SOLID-STATE TRANSFORMATION IN SIC
    PANDEY, D
    LELE, S
    KRISHNA, P
    JOURNAL OF CRYSTAL GROWTH, 1977, 42 (DEC) : 644 - 650
  • [48] Interface properties of metal-oxide-semiconductor structures on n-type 6H and 4H-SiC
    Friedrichs, P
    Burte, EP
    Schomer, R
    JOURNAL OF APPLIED PHYSICS, 1996, 79 (10) : 7814 - 7819
  • [49] Effect of cerium impurity on the stable growth of the 4H-SiC polytype by the physical vapour transport method
    Racka-Szmidt K.
    Tymicki E.
    Raczkiewicz M.
    Sar J.
    Wejrzanowski T.
    Grasza K.
    Journal of Crystal Growth, 2022, 586
  • [50] ELECTRON-PARAMAGNETIC-RES OF (TIN)0 IMPURITY PAIRS IN 6H POLYTYPE OF SIC
    VAINER, VS
    ILIN, VA
    KARACHINOV, VA
    TAIROV, YM
    FIZIKA TVERDOGO TELA, 1986, 28 (02): : 363 - 368