Cryogenic machining of hard-to-cut materials

被引:251
|
作者
Wang, ZY [1 ]
Rajurkar, KP
机构
[1] Univ Nevada, Dept Mech Engn, Las Vegas, NV 89154 USA
[2] Univ Nebraska, Dept Ind & Management Syst Engn, Lincoln, NE 68588 USA
关键词
cryogenic turning; ceramics; titanium; inconel; tantalum;
D O I
10.1016/S0043-1648(99)00361-0
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This paper presents a technique for machining of advanced ceramics with liquid nitrogen (LN2) cooled polycrystalline cubic boron nitride (PCBN) tool, titanium alloys, Inconel alloys, and tantalum with cemented carbide tools. With LN2 cooling, the temperature in the cutting zone is reduced to a lower range, therefore, the hot-strength and hot-hardness of the tool remain high, and the temperature-dependent tool wear reduces significantly under all machining conditions. The surface roughness of all materials machined with LN2 cooling were found to be much better than the surface roughness of materials machined without LN2 cooling after the same length of cutting. (C) 2000 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:168 / 175
页数:8
相关论文
共 50 条
  • [31] Design and performance of AlTiN and TiAlCrN PVD coatings for machining of hard to cut materials
    Fox-Rabinovich, G. S.
    Kovalev, A. I.
    Aguirre, M. H.
    Beake, B. D.
    Yamamoto, K.
    Veldhuis, S. C.
    Endrino, J. L.
    Wainstein, D. L.
    Rashkovskiy, A. Y.
    SURFACE & COATINGS TECHNOLOGY, 2009, 204 (04): : 489 - 496
  • [32] Heating Current Control in Electric Hot Minipore drilling hard-to-cut material
    Xu, L. Y.
    Wu, Q.
    Ye, B. Y.
    Hu, X. F.
    Li, Y. Z. H.
    Qu, X. I.
    MECHANICAL ENGINEERING AND GREEN MANUFACTURING, PTS 1 AND 2, 2010, : 1605 - +
  • [33] INVESTIGATING TURNING OF HARD-TO-CUT MATERIAL USING SELF-PROPELLED ROTARY TOOL
    El-Mounayri, H.
    Razak, A. Latif
    Kessler, M.
    PROCEEDINGS OF THE ASME INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE 2011, VOL 2, 2011, : 331 - 338
  • [34] CONSERVE DIAMOND BORT AND CUT HARD-TO-MACHINE MATERIALS WITH NEW MACHINING PROCESSES
    不详
    JOURNAL OF METALS, 1952, 4 (04): : 378 - 380
  • [35] Investigation of a green nanofluid added with graphene and Al 2 O 3 nano-additives for grinding hard-to-cut materials
    Li, Wei
    Zeng, Zhixiong
    Le, Shajiu
    Zhu, Keyi
    Huang, Xiangming
    Hegab, Hussien
    Ibrahim, Ahmed Mohamed Mahmoud
    TRIBOLOGY INTERNATIONAL, 2024, 195
  • [36] The effects of Cryogenic Cooling on Surface Integrity in Hard Machining
    Umbrello, D.
    Pu, Z.
    Caruso, S.
    Outeiro, J. C.
    Jayal, A. D.
    Dillon, O. W., Jr.
    Jawahir, I. S.
    1ST CIRP CONFERENCE ON SURFACE INTEGRITY (CSI), 2011, 19
  • [37] Modelling the dynamic behaviour of hard-to-cut alloys under conditions of vibro-impact cutting
    Muhammad, R.
    Demiral, M.
    Roy, A.
    Silberschmidt, V. V.
    INTERNATIONAL SYMPOSIUM ON DYNAMIC DEFORMATION AND FRACTURE OF ADVANCED MATERIALS (D2FAM 2013), 2013, 451
  • [38] The effects of cryogenic cooling on surface integrity in hard machining: A comparison with dry machining
    Umbrello, Domenico
    Micari, Fabrizio
    Jawahir, I. S.
    CIRP ANNALS-MANUFACTURING TECHNOLOGY, 2012, 61 (01) : 103 - 106
  • [39] The influence of depth of cut on cryogenic machining performance of hardened steel
    Gharibi, Armin
    Kaynak, Yusuf
    JOURNAL OF THE FACULTY OF ENGINEERING AND ARCHITECTURE OF GAZI UNIVERSITY, 2019, 34 (02): : 582 - 596
  • [40] The Diagnostics of Abrasive Tools After Internal Cylindrical Grinding of Hard-to-Cut Materials by Means of a Laser Technique Using Imaging and Analysis of Scattered Light
    W. Kapłonek
    K. Nadolny
    Arabian Journal for Science and Engineering, 2013, 38 : 953 - 970