Evolution of micro-arc oxidation behaviors of the hot-dipping aluminum coatings on Q235 steel substrate

被引:31
|
作者
Lu Lihong [1 ,2 ]
Shen Dejiu [2 ]
Zhang Jingwu [2 ]
Song Jian [3 ]
Li Liang [3 ]
机构
[1] Chinese Peoples Armed Police Acad, Res Dept, Langfang 065000, Peoples R China
[2] Yanshan Univ, Coll Mat Sci & Engn, State Key Lab Metastable Mat Sci & Technol, Qinhuangdao 066004, Peoples R China
[3] Tsinghua Univ, State Key Lab Automot Safety & Energy, Beijing 100084, Peoples R China
关键词
Evolution; Q235; steel; Hot-dipping aluminum; Micro-arc oxidation; Ceramic coatings; PLASMA ELECTROLYTIC OXIDATION; CERAMIC COATINGS; WEAR-RESISTANCE; GROWTH; ALLOY;
D O I
10.1016/j.apsusc.2010.11.187
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Micro-arc oxidation (MAO) is not applicable to prepare ceramic coatings on the surface of steel directly. In this work, hybrid method of MAO and hot-dipping aluminum (HDA) were employed to fabricate composite ceramic coatings on the surface of Q235 steel. The evolution of MAO coatings, such as growth rate, thickness of the total coatings, ingrown and outgrown coatings, cross section and surface morphologies and phase composition of the ceramic coatings were studied. The results indicate that both the current density and the processing time can affect the total thickness, the growth rate and the ratio of ingrown and outgrown thickness of the ceramic coatings. The total thickness, outgrown thickness and growth rate have maximum values with the processing time prolonged. The time when the maximum value appears decreases and the ingrown dominant turns to outgrown dominant little by little with the current density increasing. The composite coatings obtained by this hybrid method consists of three layers from inside to outside, i.e. Fe-Al alloy layer next to the substrate, aluminum layer between the Fe-Al layer and the ceramic coatings which is as the top exterior layer. Metallurgical bonding was observed between every of the two layers. There are many micro-pores and micro-cracks, which act as discharge channels and result of quick and non-uniform cooling of melted sections in the MAO coatings. The phase composition of the ceramic coatings is mainly composed of amorphous phase and crystal Al2O3 oxides. The crystal Al2O3 phase includes kappa-Al2O3, 0-Al2O3 and beta-Al2O3. Compared with the others, the beta-Al2O3 content is the least. The MAO process can be divided into three periods, namely the common anodic oxidation stage, the stable MAO stage and the ceramic coatings destroyed stage. The exterior loose part of the ceramic coatings was destroyed badly in the last period which should be avoided during the MAO process. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:4144 / 4150
页数:7
相关论文
共 50 条
  • [11] Characterization of micro-arc oxidation coatings on aluminum drillpipes at different current density
    Wang, Ping
    Wu, Ting
    Xiao, You Tao
    Zhang, Luo
    Pu, Jun
    Cao, Wen Jie
    Zhong, Xue Mei
    VACUUM, 2017, 142 : 21 - 28
  • [12] The Investigation of Hot-dip Aluminum and Micro-arc Oxidation Multilayer Coating on 080A15 Steel
    Zhao, Zhilong
    Wang, Jianlong
    Liu, Yan
    MANUFACTURING ENGINEERING AND AUTOMATION I, PTS 1-3, 2011, 139-141 : 406 - 409
  • [13] Wetting of liquid Zinc-aluminum-magnesium alloy on steel substrate during hot-dipping: Understanding the role of the flux
    Xu, Minyun
    Zheng, Zhaoyang
    Han, Dong
    Ma, Ruina
    Du, An
    Fan, Yongzhe
    Zhao, Xue
    Cao, Xiaoming
    SURFACE TOPOGRAPHY-METROLOGY AND PROPERTIES, 2022, 10 (03):
  • [14] Preparation of ceramic coatings on inner surface of steel tubes using a combined technique of hot-dipping and plasma electrolytic oxidation
    Gu, Wei-Chao
    Lv, Guo-Hua
    Chen, Huan
    Chen, Guang-Liang
    Feng, Wen-Ran
    Zhang, Gu-Ling
    Yang, Si-Ze
    JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 430 (1-2) : 308 - 312
  • [15] Microstructure and corrosion resistance of ceramic coatings formed on aluminum alloy by micro-arc oxidation
    Du, Jun
    Chen, Dong-Chu
    Li, Wen-Fang
    Zhang, Yong-Jun
    Peng, Ji-Hua
    Huanan Ligong Daxue Xuebao/Journal of South China University of Technology (Natural Science), 2007, 35 (03): : 6 - 10
  • [16] Design of Scanning Micro-Arc Oxidation Forming Ceramic Coatings on 2024 Aluminum Alloy
    Lv, Peng Xiang
    Chi, Guan Xin
    Wei, Dong Bo
    Di, Shi Chun
    MANUFACTURING PROCESS TECHNOLOGY, PTS 1-5, 2011, 189-193 : 1296 - 1300
  • [17] Study of Microhardness of Ceramic Coatings Formed on 6061 Aluminum Alloy by Micro-arc Oxidation
    Wang, X. -D.
    Wu, X. -H.
    Wang, Rui
    2011 INTERNATIONAL CONFERENCE ON FUZZY SYSTEMS AND NEURAL COMPUTING (FSNC 2011), VOL VII, 2011, : 388 - 391
  • [18] Effects of Process Parameters on Content of Serpentine in Micro-arc Oxidation Coatings on Aluminum Alloy
    Zheng Shi-bin
    Cheng Dong
    Yu Guang-yu
    Yan Zhi-jun
    Zhu Xin-he
    Ma Chun-sheng
    CHINA SURFACE ENGINEERING, 2018, 31 (01) : 96 - 105
  • [19] Microstructure and properties of ceramic coatings prepared by micro-arc oxidation on 7075 aluminum alloy
    Cao, G. P.
    Song, R. G.
    MATERIALS RESEARCH EXPRESS, 2018, 5 (02):
  • [20] Study of Microhardness of Ceramic Coatings Formed on 6061 Aluminum Alloy by Micro-arc Oxidation
    Wang, X. -D.
    Wu, X. -H.
    Wang, Rui
    2011 AASRI CONFERENCE ON ARTIFICIAL INTELLIGENCE AND INDUSTRY APPLICATION (AASRI-AIIA 2011), VOL 4, 2011, : 399 - 402