Evolution of micro-arc oxidation behaviors of the hot-dipping aluminum coatings on Q235 steel substrate

被引:31
|
作者
Lu Lihong [1 ,2 ]
Shen Dejiu [2 ]
Zhang Jingwu [2 ]
Song Jian [3 ]
Li Liang [3 ]
机构
[1] Chinese Peoples Armed Police Acad, Res Dept, Langfang 065000, Peoples R China
[2] Yanshan Univ, Coll Mat Sci & Engn, State Key Lab Metastable Mat Sci & Technol, Qinhuangdao 066004, Peoples R China
[3] Tsinghua Univ, State Key Lab Automot Safety & Energy, Beijing 100084, Peoples R China
关键词
Evolution; Q235; steel; Hot-dipping aluminum; Micro-arc oxidation; Ceramic coatings; PLASMA ELECTROLYTIC OXIDATION; CERAMIC COATINGS; WEAR-RESISTANCE; GROWTH; ALLOY;
D O I
10.1016/j.apsusc.2010.11.187
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Micro-arc oxidation (MAO) is not applicable to prepare ceramic coatings on the surface of steel directly. In this work, hybrid method of MAO and hot-dipping aluminum (HDA) were employed to fabricate composite ceramic coatings on the surface of Q235 steel. The evolution of MAO coatings, such as growth rate, thickness of the total coatings, ingrown and outgrown coatings, cross section and surface morphologies and phase composition of the ceramic coatings were studied. The results indicate that both the current density and the processing time can affect the total thickness, the growth rate and the ratio of ingrown and outgrown thickness of the ceramic coatings. The total thickness, outgrown thickness and growth rate have maximum values with the processing time prolonged. The time when the maximum value appears decreases and the ingrown dominant turns to outgrown dominant little by little with the current density increasing. The composite coatings obtained by this hybrid method consists of three layers from inside to outside, i.e. Fe-Al alloy layer next to the substrate, aluminum layer between the Fe-Al layer and the ceramic coatings which is as the top exterior layer. Metallurgical bonding was observed between every of the two layers. There are many micro-pores and micro-cracks, which act as discharge channels and result of quick and non-uniform cooling of melted sections in the MAO coatings. The phase composition of the ceramic coatings is mainly composed of amorphous phase and crystal Al2O3 oxides. The crystal Al2O3 phase includes kappa-Al2O3, 0-Al2O3 and beta-Al2O3. Compared with the others, the beta-Al2O3 content is the least. The MAO process can be divided into three periods, namely the common anodic oxidation stage, the stable MAO stage and the ceramic coatings destroyed stage. The exterior loose part of the ceramic coatings was destroyed badly in the last period which should be avoided during the MAO process. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:4144 / 4150
页数:7
相关论文
共 50 条
  • [41] Effects of electrolyte parameters on black ceramic coatings prepared by micro-arc oxidation of aluminum alloy
    Liang, Ge
    Zhao, Ren-Bing
    Jiang, Bai-Ling
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2006, 27 (05): : 91 - 94
  • [42] The effect of surface roughness of the substrate on fatigue life of coated aluminum alloy by micro-arc oxidation
    Dai, Wei Bing
    Yuan, Long Xiang
    Li, Chang You
    He, David
    Jia, Da Wei
    Zhang, Yi Min
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 765 : 1018 - 1025
  • [43] Effect of high temperature oxidation prefab film on formation of micro-arc oxidation coatings on 6061 aluminum alloy
    Shen Dejiu
    Zou Jie
    Wu Lailei
    Liu Fangfei
    Li Guolong
    Cai Jingrui
    He Donglei
    Ma Haojie
    Jiang Guirong
    APPLIED SURFACE SCIENCE, 2013, 265 : 431 - 437
  • [44] Corrosion resistance of micro-arc oxidation composite coatings on S355 offshore steel
    He X.
    Kong D.-J.
    Song R.-G.
    Gongcheng Kexue Xuebao/Chinese Journal of Engineering, 2019, 41 (09): : 1152 - 1161
  • [45] Morphology of composite coatings formed on Mo1 substrate using hot-dip aluminising and micro-arc oxidation techniques
    Wang, Shao-Peng
    Zhou, Lian
    Li, Chang-Jiu
    Li, Zheng-Xian
    Li, Hong-Zhan
    Yang, Li-Jing
    APPLIED SURFACE SCIENCE, 2020, 508 (508)
  • [46] Effects of rare earth (RE) additives on performances of micro-arc oxidation coatings formed on aluminum alloy
    Huang, Dan
    Zhang, Xiaoyan
    Wu, Defeng
    Zhou, Xiaosong
    ADVANCES IN APPLIED SCIENCES AND MANUFACTURING, PTS 1 AND 2, 2014, 850-851 : 140 - 143
  • [47] ON THE MICRO-ARC OXIDATION AND ITS EFFECT ON THE CORROSION-MECHANICAL BEHAVIOR OF ALUMINUM-ALLOYS AND COATINGS
    SAAKIYAN, LS
    EFREMOV, AP
    SOBOLEVA, IA
    PROTECTION OF METALS, 1994, 30 (01): : 85 - 88
  • [48] Formation of bioceramic coatings containing hydroxyapatite on the titanium substrate by micro-arc oxidation coupled with electrophoretic deposition
    Bai, Yu
    Park, Il Song
    Park, Hyeoung Ho
    Bae, Tae Sung
    Lee, Min Ho
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2010, 95B (02) : 365 - 373
  • [49] Growth of Ceramic Coatings on LY12 Aluminum Alloys by Micro-Arc Oxidation and Microstructure Properties of Ceramic Coatings
    Gao, Jinglong
    Shao, Zhongcai
    Li, Tongzhen
    MEASUREMENT AND CONTROL OF GRANULAR MATERIALS, 2012, 508 : 246 - 249
  • [50] Effect of ultrasonic on microstructure and growth characteristics of micro-arc oxidation ceramic coatings on 6061 aluminum alloy
    Shen Dejiu
    Cai Jingrui
    Li Guolong
    He Donglei
    Wu Lailei
    Ma Haojie
    Xia Yonghong
    Chen He
    Yang Yaqian
    VACUUM, 2014, 99 : 143 - 148