Planar dislocation structure during creep-fatigue interactions of TP347H heat-resistant austenitic steel at 600 °C

被引:21
|
作者
Zhou, Hongwei [1 ,2 ]
Zhang, Hongyan [1 ,2 ]
Bai, Fengmei [3 ,4 ]
Song, Meng [1 ,4 ]
Chen, Yan [1 ,2 ]
Zhang, Liqiang [3 ]
Fang, Xudong [5 ]
He, Yizhu [1 ,2 ]
机构
[1] Anhui Univ Technol, Key Lab Green Fabricat & Surface Technol Adv Met, Minist Educ, Maanshan 243002, Peoples R China
[2] Anhui Univ Technol, Sch Mat Sci & Engn, Maanshan 243002, Anhui, Peoples R China
[3] Anhui Univ Technol, Sch Met Engn, Maanshan 243002, Anhui, Peoples R China
[4] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110189, Peoples R China
[5] Taiyuan Iron & Steel Grp Co Ltd, State Key Lab Adv Stainless Steel, Taiyuan 030003, Peoples R China
基金
中国国家自然科学基金;
关键词
Heat-resistant austenitic steel; Creep-fatigue; Low cycle fatigue; Fatigue fracture mode; Planar slip structure; LOW-CYCLE FATIGUE; GRAIN-BOUNDARY CARBIDES; 316L STAINLESS-STEEL; INTERACTION BEHAVIOR; PREDICTION METHODS; DAMAGE MECHANISM; LIFE PREDICTION; DEFORMATION; EVOLUTION; PRECIPITATION;
D O I
10.1016/j.msea.2020.139141
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The low-cycle fatigue (LCF) and creep-fatigue (CF) interaction tests of TP347H austenitic stainless steel are carried out in air under a fully-reversed strain amplitude of 1.0% at 600 degrees C. A 10 min tensile dwell is applied in CF interaction testing. The influences of dwell on dislocation structures and fracture behavior have been evaluated. It is found that CF interaction life is lower than LCF one. The fatigue fracture mode changes from transgranular crack under LCF to transgranular plus intergranular fracture with tensile dwell. A lot of dislocation planar slip bands (PSBs) were found under CF interaction condition. PSB interacts with PSB of another slip system, twins, grain boundary (GB), and triangular GB. Strongly PSB-GB interaction causes stress concentration at GB, creating cavities and crack initiation, causing intergranular fracture. The stress concentration within the PSBs will also cause cracks, resulting in transgranular fracture morphology with fatigue striation.
引用
收藏
页数:11
相关论文
共 48 条
  • [31] Twin Boundary Evolution Under Low-Cycle Fatigue of C-HRA-5 Austenitic Heat-Resistant Steel at High Temperature
    Zhou Hongwei
    Gao Jianbing
    Shen Jiaming
    Zhao Wei
    Bai Fengmei
    He Yizhu
    ACTA METALLURGICA SINICA, 2022, 58 (08) : 1013 - 1023
  • [32] Effect of rare earth alloying on creep rupture of economical 21Cr-11Ni-N heat-resistant austenitic steel at 650°C
    Chen Lei
    Long Hongjun
    Liu Xingang
    Jin Miao
    Ma Xiaocong
    JOURNAL OF RARE EARTHS, 2016, 34 (04) : 447 - 452
  • [33] Effect of boron addition on Nb(C, N) refinement and dissolution behavior in Super 304H austenitic heat-resistant steel
    Wang, Tong
    Ma, Jinyao
    Dong, Nan
    Zhang, Shucai
    Wang, Puli
    Cui, Peizhi
    Yang, Song
    Fang, Xudong
    Wang, Zhihua
    Han, Peide
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2025, 36 : 1705 - 1714
  • [34] Formation of Nb(C,N) Carbonitride in Cast Austenitic Heat-Resistant Steel during Directional Solidification under Different Withdraw Rates
    Zhang, Yinhui
    Yang, Jian
    MATERIALS, 2018, 11 (12)
  • [35] Study on Creep Rupture Strength and Fracture Behavior of Super304H/T92 Austenitic Heat-resistant Steel Friction Welding Joints
    Zhang J.
    Xue H.
    Lu Y.
    Cailiao Daobao/Materials Reports, 2019, 33 (06): : 2067 - 2070
  • [36] The Effect of Nb and Ti on Structure and Mechanical Properties of 12Ni-25Cr-0.4C Austenitic Heat-Resistant Steel after Aging at 900 A°C for 1000 h
    Javaheri, Vahid
    Shahri, Farzad
    Mohammadnezhad, Mahyar
    Tamizifar, Morteza
    Naseri, Masaab
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (10) : 3558 - 3566
  • [37] The Effect of Nb and Ti on Structure and Mechanical Properties of 12Ni-25Cr-0.4C Austenitic Heat-Resistant Steel after Aging at 900 °C for 1000 h
    Vahid Javaheri
    Farzad Shahri
    Mahyar Mohammadnezhad
    Morteza Tamizifar
    Masaab Naseri
    Journal of Materials Engineering and Performance, 2014, 23 : 3558 - 3566
  • [38] QUANTITATIVE-EVALUATION OF FINE-STRUCTURE PARAMETERS DURING CREEP AND AGING OF CR-MO-V HEAT-RESISTANT STEEL
    MINTS, II
    SHRON, RZ
    SHULGINA, NG
    FIZIKA METALLOV I METALLOVEDENIE, 1989, 67 (05): : 1011 - 1017
  • [39] Microstructural evolution of heat-resistant steel Super304H during 650°C long term aging
    Yu, Hong-Yao
    Chi, Cheng-Yu
    Dong, Jian-Xin
    Xie, Xi-Shan
    Cui, Zheng-Qiang
    Chen, Xiao-Fang
    Beijing Keji Daxue Xuebao/Journal of University of Science and Technology Beijing, 2010, 32 (07): : 877 - 882
  • [40] Microstructure of 10% Cr martensitic heat-resistant steel welded joints and type IV cracking behavior during creep rupture at 650 °C
    Zhang, Qunbing
    Zhang, Jianxun
    Zhao, Pengfei
    Huang, Yong
    Yang, Yong
    Zhao, Yale
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 638 : 30 - 37