High temperature oxidation behaviour of Ag-36.35 wt.% Zn and Ag-38.50 wt.% Zn-0.60 wt.% Al

被引:5
|
作者
Chandra-ambhorn, S. [1 ]
Chumpanya, P. [1 ]
机构
[1] King Mongkuts Univ Technol North Bangkok, High Temp Corros Res Ctr, Dept Mat & Prod Technol Engn, Fac Engn, 1518,Pracharat 1 Rd, Bangkok 10800, Thailand
关键词
Ag-Zn; Ag-Zn-Al; High temperature corrosion; Oxidation; AZ91D MAGNESIUM ALLOY; DEGREES-C; SOLUBILITY LIMIT; AG; KINETICS; MICROSTRUCTURE; ADHESION; STEELS; STEAM; O-2;
D O I
10.1016/j.corsci.2017.11.007
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ag-36.35 wt.% Zn and Ag-38.50 wt.% Zn-0.60 wt.% Al were oxidised in air at 450-650 degrees C up to 48 h. The oxidation kinetics of both alloys were parabolic with the lower rate constant for the latter alloy. After oxidation for 48 h, thermal oxide scale on Ag-36.35 wt.% Zn was ZnO at all studied temperatures. When 0.60 wt.% Al was added to Ag-38.50 wt.% Zn, ZnO and ZnAl2O4 were formed at all studied temperatures. Al2O3 was evidently observed at 550 and 650 degrees C. The formation of Al-containing oxides helped reduce the oxidation rate of Ag-38.50 wt.% Zn-0.60 wt.% Al.
引用
收藏
页码:38 / 44
页数:7
相关论文
共 50 条
  • [31] Rare earth microalloying in as-cast and homogenized alloys Cu-6 wt.% Ag and Cu-24 wt.% Ag
    Liu, J.B.
    Meng, L.
    Zhang, L.
    Journal of Alloys and Compounds, 2006, 425 (1-2): : 185 - 190
  • [32] Microstructure nanocrystallization of a Mg-3 wt.%Al-1 wt.%Zn alloy by mechanically assisted hydriding-dehydriding
    Hu, Lianxi
    Wu, Yang
    Yuan, Yuan
    Wang, Heng
    MATERIALS LETTERS, 2008, 62 (17-18) : 2984 - 2987
  • [33] Microstructure and Creep Resistance of Mg-(8-12 Wt.%) Zn-(2-6 Wt.%) Al Alloys
    Wan, Xiao Feng
    Ni, Hong Jun
    Huang, Ming Yu
    MANUFACTURING ENGINEERING AND AUTOMATION II, PTS 1-3, 2012, 591-593 : 1034 - 1037
  • [34] Grain refining of Zn-22 wt.% Al superplastic alloy
    Central and Metallurgical Research, and Development Inst , Cairo, Egypt
    J Mater Process Technol, 1-3 (73-78):
  • [35] Solidification, solution treatment and age hardening of a Mg-1.6 wt.% Ca-3.2 wt.% Zn alloy
    Levi, G
    Avraham, S
    Zilberov, A
    Bamberger, M
    ACTA MATERIALIA, 2006, 54 (02) : 523 - 530
  • [36] Morphology and Mechanical, Corrosive, and Antibacterial Behaviors of Indirectly Extruded Zn-0.05 wt.%Mg-(0.5, 1 wt.%)Ag Alloys (pg 1, 2019)
    Xiao, C.
    Zhao, D. W.
    Sun, Q.
    Su, Y.
    Cui, D. P.
    Zhang, X. Z.
    Dong, X. L.
    Wang, H. X.
    Wang, F.
    Ren, Y. P.
    Qin, G. W.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (11) : 6873 - 6873
  • [37] Electromigration in a Sn-3 wt.%Ag-0.5 wt.%Cu-3 wt.%Bi Solder Stripe Between Two Cu Electrodes Under Current Stressing
    Lee, Shang-Hua
    Chen, Chih-Ming
    JOURNAL OF ELECTRONIC MATERIALS, 2011, 40 (09) : 1943 - 1949
  • [38] High temperature oxidation behaviour of Fe-15.7 wt.% Cr-8.5 wt.% Mn in oxygen without and with water vapour at 700 °C
    Chandra-ambhorn, S.
    Saranyachot, P.
    Thublaor, T.
    CORROSION SCIENCE, 2019, 148 : 39 - 47
  • [39] Investigation on microstructure characterizations and phase compositions of rapidly solidification/powder metallurgy Mg-6 wt.% Zn-5 wt.% Ce-1.5 wt.% Ca alloy
    Zhou, Tao
    Xia, Hua
    Yang, Mingbo
    Zhou, Zhiming
    Chen, Kang
    Hu, Jianjun
    Chen, Zhenhua
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (09) : L145 - L149
  • [40] Improvement of room-temperature superplasticity in Zn-22 wt.%Al alloy
    Xia, Shao Hua
    Wang, Jia
    Wang, Jing Tao
    Liu, Jin Qiang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 493 (1-2): : 111 - 115