Influence of various bonding techniques on the fracture strength of thin CAD/CAM-fabricated occlusal glass-ceramic veneers

被引:35
|
作者
Yazigi, Christine [1 ]
Kern, Matthias [1 ]
Chaar, Mohamed Sad [1 ]
机构
[1] Christian Albrechts Univ Kiel, Sch Dent, Dept Prosthodont Propaedeut & Dent Mat, Arnold Heller Str 16, D-24105 Kiel, Germany
关键词
Glass-ceramic veneers; Glass-ceramic tabletops; Occlusal veneers; Immediate dentin sealing; Total etch; Selective etch; Lithium disilicate restorations; Fracture resistance; Adhesive bonding to dentin; PARTIAL-COVERAGE RESTORATIONS; 3-YEAR CLINICAL EFFECTIVENESS; ARTIFICIAL ORAL ENVIRONMENT; SEVERE DENTAL EROSION; SELF-ETCH ADHESIVE; PREPARATION DESIGN; PORCELAIN VENEERS; CERVICAL LESIONS; POSTERIOR TEETH; COMPOSITE RESIN;
D O I
10.1016/j.jmbbm.2017.08.016
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Objectives: To evaluate the efficiency of immediate dentin sealing and the effects of different bonding protocols on the fracture strength of CAD/CAM occlusal veneers bonded to exposed dentin. Methods: Ninety-six extracted maxillary premolars were initially divided into three main groups with 32 specimens each: without immediate dentin sealing, immediate dentin sealing/total etching and immediate dentin sealing/selective etching. Teeth were identically prepared in the dentin to receive occlusal veneers of 0.8 mm thickness, milled from lithium disilicate ceramic blocks (IPS e.max CAD). Each main group was later subdivided, according to the pre-cementation surface etching protocol (total/selective), into two subgroups with 16 specimens each. All restorations were adhesively bonded using a resin cement (Variolink Esthetic). Half of the specimens of each subgroup were subjected to thermo-dynamic loading in a chewing simulator with 1,200,000 cycles at 10 kg load. The other half and the surviving specimens were subjected to quasi-static loading until failure. Statistical analysis was performed using three-way ANOVA and Tukey's post-hoc tests. Results: All specimens except one survived the artificial aging. A significantly higher fracture strength of restorations (p <= 0.001) was obtained when immediate dentin sealing was followed regardless of the etching method with values ranging from a minimum of 1122 +/- 336 N to a maximum of 1853 +/- 333 N. Neither the pre-cementation treatment nor the artificial aging had a statistical significant effect on the fracture strength. Significance: Immediate dentin sealing protocol is recommended whenever dentin is exposed during the preparation for thin glass-ceramic occlusal veneers.
引用
收藏
页码:504 / 511
页数:8
相关论文
共 50 条
  • [31] NOVEL-DESIGN ULTRA-THIN CAD/CAM COMPOSITE RESIN AND CERAMIC OCCLUSAL VENEERS FOR THE TREATMENT OF SEVERE DENTAL EROSION
    Schlichting, Luis Henrique
    Maia, Hamilton Pires
    Baratieri, Luiz Narciso
    Magne, Pascal
    JOURNAL OF PROSTHETIC DENTISTRY, 2011, 105 (04): : 217 - 226
  • [32] Influence of Material Selection on the Marginal Accuracy of CAD/CAM-Fabricated Metal- and All-Ceramic Single Crown Copings
    Roediger, Matthias
    Schneider, Lea
    Rinke, Sven
    BIOMED RESEARCH INTERNATIONAL, 2018, 2018
  • [33] Influence of the Crystallization Firing Process on Marginal and Internal Adaptation of Silicate-based Glass-ceramic Inlays Fabricated With a CAD/CAM Chairside System
    Kobayashi, M.
    Niizuma, Y.
    Sugai, R.
    Manabe, A.
    OPERATIVE DENTISTRY, 2023, 48 (06) : 657 - 665
  • [34] Correction: Compressive strength evaluation of thin occlusal veneers from different CAD/CAM materials, before and after acidic saliva exposure
    Codruța Ille
    Elena-Alina Moacă
    Daniel Pop
    Luciana Goguță
    Carmen Opriș
    Ioana Ligia Pîrvulescu
    Liane Avram
    Andrei Faur
    Anca Jivănescu
    Odontology, 2023, 111 : 375 - 375
  • [35] Discoloration of manually fabricated resins and industrially fabricated CAD/CAM blocks versus glass-ceramic: Effect of storage media, duration, and subsequent polishing
    Stawarczyk, Bogna
    Sener, Beatrice
    Trottmann, Albert
    Roos, Malgorzata
    Oezcan, Mutlu
    Haemmerle, Christoph H. F.
    DENTAL MATERIALS JOURNAL, 2012, 31 (03) : 377 - 383
  • [36] High-strength CAD/CAM-fabricated veneering material sintered to zirconia copings - A new fabrication mode for all-ceramic restorations
    Beuer, Florian
    Schweiger, Josef
    Eichberger, Marlis
    Kappert, Heinrich F.
    Gernet, Wolfgang
    Edelhoff, Daniel
    DENTAL MATERIALS, 2009, 25 (01) : 121 - 128
  • [37] Retentive Strength of CAD/CAM-Fabricated All-Ceramic Crowns Luted on Titanium Implant Abutments Using Different Ceramic Materials and Luting Agents: An In Vitro Study
    Bjelopavlovic, Monika
    Weyhrauch, Michael
    Scheller, Herbert
    Wentaschek, Stefan
    Lehmann, Karl Martin
    MATERIALS, 2022, 15 (19)
  • [38] Influence of ageing on glass and resin bonding of dental glass-ceramic veneer adhesion to zirconia: A fracture mechanics analysis and interpretation
    Swain, M., V
    Gee, C.
    Li, K. C.
    ACTA BIOMATERIALIA, 2018, 74 : 454 - 463
  • [39] Fracture strength of CAD/CAM fabricated lithium disilicate and resin nano ceramic restorations used for endodontically treated teeth
    Gungor, Merve Bankoglu
    Bal, Bilge Turhan
    Yilmaz, Handan
    Aydin, Cemal
    Nemli, Secil Karakoca
    DENTAL MATERIALS JOURNAL, 2017, 36 (02) : 135 - 141
  • [40] Fracture-free surfaces of CAD/CAM lithium metasilicate glass-ceramic using micro-slurry jet erosion
    Yin, Ling
    Baba, Takashi
    Nakanishi, Yoshitaka
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2018, 80 : 59 - 67