Influence of various bonding techniques on the fracture strength of thin CAD/CAM-fabricated occlusal glass-ceramic veneers

被引:35
|
作者
Yazigi, Christine [1 ]
Kern, Matthias [1 ]
Chaar, Mohamed Sad [1 ]
机构
[1] Christian Albrechts Univ Kiel, Sch Dent, Dept Prosthodont Propaedeut & Dent Mat, Arnold Heller Str 16, D-24105 Kiel, Germany
关键词
Glass-ceramic veneers; Glass-ceramic tabletops; Occlusal veneers; Immediate dentin sealing; Total etch; Selective etch; Lithium disilicate restorations; Fracture resistance; Adhesive bonding to dentin; PARTIAL-COVERAGE RESTORATIONS; 3-YEAR CLINICAL EFFECTIVENESS; ARTIFICIAL ORAL ENVIRONMENT; SEVERE DENTAL EROSION; SELF-ETCH ADHESIVE; PREPARATION DESIGN; PORCELAIN VENEERS; CERVICAL LESIONS; POSTERIOR TEETH; COMPOSITE RESIN;
D O I
10.1016/j.jmbbm.2017.08.016
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Objectives: To evaluate the efficiency of immediate dentin sealing and the effects of different bonding protocols on the fracture strength of CAD/CAM occlusal veneers bonded to exposed dentin. Methods: Ninety-six extracted maxillary premolars were initially divided into three main groups with 32 specimens each: without immediate dentin sealing, immediate dentin sealing/total etching and immediate dentin sealing/selective etching. Teeth were identically prepared in the dentin to receive occlusal veneers of 0.8 mm thickness, milled from lithium disilicate ceramic blocks (IPS e.max CAD). Each main group was later subdivided, according to the pre-cementation surface etching protocol (total/selective), into two subgroups with 16 specimens each. All restorations were adhesively bonded using a resin cement (Variolink Esthetic). Half of the specimens of each subgroup were subjected to thermo-dynamic loading in a chewing simulator with 1,200,000 cycles at 10 kg load. The other half and the surviving specimens were subjected to quasi-static loading until failure. Statistical analysis was performed using three-way ANOVA and Tukey's post-hoc tests. Results: All specimens except one survived the artificial aging. A significantly higher fracture strength of restorations (p <= 0.001) was obtained when immediate dentin sealing was followed regardless of the etching method with values ranging from a minimum of 1122 +/- 336 N to a maximum of 1853 +/- 333 N. Neither the pre-cementation treatment nor the artificial aging had a statistical significant effect on the fracture strength. Significance: Immediate dentin sealing protocol is recommended whenever dentin is exposed during the preparation for thin glass-ceramic occlusal veneers.
引用
收藏
页码:504 / 511
页数:8
相关论文
共 50 条
  • [11] The Influence of a Novel, Crenelated Design of CAD-CAM Ceramic Veneers on the Debonding Strength
    Maroiu, Alexandra-Cristina
    Jivanescu, Anca
    Serban, Dan-Andrei
    Negru, Radu-Marcel
    Duma, Virgil-Florin
    Sinescu, Cosmin
    Rominu, Mihai
    MATERIALS, 2023, 16 (10)
  • [12] Effect of immediate dentin sealing on load-bearing capacity under accelerated fatigue of thin occlusal veneers made of CAD-CAM glass-ceramic and resin composite material
    Mueller, Bruna
    Pilecco, Rafaela Oliveira
    Valandro, Luiz Felipe
    Ruschel, Vanessa Carla
    Pereira, Gabriel Kalil Rocha
    Bernardon, Jussara Karina
    DENTAL MATERIALS, 2023, 39 (04) : 372 - 382
  • [13] Influence of conventional and digital intraoral impressions on the fit of CAD/CAM-fabricated all-ceramic crowns
    S. Berrendero
    M. P. Salido
    A. Valverde
    A. Ferreiroa
    G. Pradíes
    Clinical Oral Investigations, 2016, 20 : 2403 - 2410
  • [14] Influence of conventional and digital intraoral impressions on the fit of CAD/CAM-fabricated all-ceramic crowns
    Berrendero, S.
    Salido, M. P.
    Valverde, A.
    Ferreiroa, A.
    Pradies, G.
    Clinical Oral Investigations, 2016, 20 (09) : 2403 - 2410
  • [15] Fracture strength of CAD/CAM posterior ceramic crowns after manual enhancement of occlusal morphology
    Passos, L.
    Torrealba, Y.
    Linke, B.
    Street, A.
    Passos, S.
    INTERNATIONAL JOURNAL OF COMPUTERIZED DENTISTRY, 2018, 21 (03) : 191 - 200
  • [16] Resistance of CAD/CAM composite resin and ceramic occlusal veneers to fatigue and fracture in worn posterior teeth: A systematic review
    Maldonado, Karelys Del Cisne
    Espinoza, Juan Andres
    Astudillo, Daniela Andrea
    Delgado, Bolivar Andres
    Bravo, Wilson Daniel
    DENTAL AND MEDICAL PROBLEMS, 2024, 61 (03) : 417 - 426
  • [17] Fracture Resistance of CAD/CAM-Fabricated Lithium Disilicate MOD Inlays and Onlays with Various Cavity Preparation Designs
    Yoon, Hyung-In
    Sohn, Paul J.
    Jin, Sharon
    Elani, Hawazin
    Lee, Sang J.
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2019, 28 (02): : E524 - E529
  • [18] Influence of material thickness on fractural strength of CAD/CAM fabricated ceramic crowns
    Zimmermann, Moritz
    Egli, Gustav
    Zaruba, Markus
    Mehl, Albert
    DENTAL MATERIALS JOURNAL, 2017, 36 (06) : 778 - 783
  • [19] Ultrathin CAD-CAM glass-ceramic and composite resin occlusal veneers for the treatment of severe dental erosion: An up to 3-year randomized clinical trial
    Schlichting, Luis Henrique
    Resende, Tayane Holz
    Reis, Katia Rodrigues
    dos Santos, Aline Raybolt
    Correa, Ivo Carlos
    Magne, Pascal
    JOURNAL OF PROSTHETIC DENTISTRY, 2022, 128 (02): : 158.e1 - 158.e12
  • [20] EVALUATION OF THE OPTICAL PROPERTIES OF CAD-CAM GENERATED YTTRIA-STABILIZED ZIRCONIA AND GLASS-CERAMIC LAMINATE VENEERS
    Alghazzawi, Tariq F.
    Lemons, Jack
    Liu, Perng-Ru
    Essig, Milton E.
    Janowski, Gregg M.
    JOURNAL OF PROSTHETIC DENTISTRY, 2012, 107 (05): : 300 - 308