High Temperature Oxidation of the Austenitic (35Fe27Cr31Ni) Alloy Sanicro 28 in O2 + H2O Environment

被引:16
|
作者
Pettersson, C. [1 ]
Jonsson, T. [2 ]
Proff, C. [2 ]
Halvarsson, M. [2 ]
Svensson, J-E. [1 ]
Johansson, L-G. [1 ]
机构
[1] Chalmers Univ Technol, Dept Chem & Biol Engn, High Temp Corros Ctr, S-41296 Gothenburg, Sweden
[2] Chalmers Univ Technol, Dept Appl Phys, S-41296 Gothenburg, Sweden
来源
OXIDATION OF METALS | 2010年 / 74卷 / 1-2期
关键词
Oxidation; Sanicro; 28; Water vapor; Evaporation; WATER-VAPOR; CHROMIUM; OXIDES; 304L;
D O I
10.1007/s11085-010-9199-1
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The present study investigates the high temperature oxidation of alloy Sanicro 28 (35Fe27Cr31Ni) in 5% O-2 and in 5% O-2 + 40% H2O. Polished steel coupons were isothermally exposed in a tube furnace at 600, 700 and 800 A degrees C for up to 168 h. The samples were investigated by gravimetry, grazing angle X-ray diffraction (XRD), Auger electron spectroscopy (AES), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and scanning transmission electron microscopy/energy dispersive X-rays (STEM/EDX). The results show that the material forms a protective scale in both environments. The scale is duplex. The inner part of the scale consists of corundum type chromium-rich (Cr (x) Fe1-x )(2)O-3, and the outer layer consists of spinel type oxide. Chromia is lost from the protective oxide by vaporization of CrO2(OH)(2) in O-2 + H2O environment. The capacity of Sanicro 28 to suffer chromia vaporization without forming a rapidly growing iron-rich oxide is attributed to its high Cr/Fe ratio. The spinel formed at the oxide/gas interface could in addition be beneficial for oxidation behavior in wet oxygen because it may slow down chromia evaporation.
引用
收藏
页码:93 / 111
页数:19
相关论文
共 50 条
  • [41] KCl-Induced Corrosion of an FeCrAl Alloy at 600 A°C in O2 + H2O Environment: The Effect of Pre-oxidation
    Israelsson, N.
    Engkvist, J.
    Hellstrom, K.
    Halvarsson, M.
    Svensson, J. -E.
    Johansson, L. -G.
    OXIDATION OF METALS, 2015, 83 (1-2): : 29 - 53
  • [42] KCl-Induced Corrosion of an FeCrAl Alloy at 600 °C in O2 + H2O Environment: The Effect of Pre-oxidation
    N. Israelsson
    J. Engkvist
    K. Hellström
    M. Halvarsson
    J.-E. Svensson
    L.-G. Johansson
    Oxidation of Metals, 2015, 83 : 29 - 53
  • [43] OXIDATION OF PRIMARY BENZYLIC AMINES BY MO(O)(O2)2(H2O)(HMPA)
    TOLLARI, S
    BRUNI, S
    BIANCHI, CL
    RAINONI, M
    PORTA, F
    JOURNAL OF MOLECULAR CATALYSIS, 1993, 83 (03): : 311 - 322
  • [44] CALCULATED TABULATIONS OF H2O LINE BROADENING BY H2O,N2,O2, AND CO2 AT HIGH-TEMPERATURE
    DELAYE, C
    HARTMANN, JM
    TAINE, J
    APPLIED OPTICS, 1989, 28 (23): : 5080 - 5087
  • [45] HIGH-TEMPERATURE REACTION-RATE FOR H + O2 = OH + O AND OH + H2 = H2O + H
    FRANK, P
    JUST, T
    BERICHTE DER BUNSEN-GESELLSCHAFT-PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 1985, 89 (02): : 181 - 187
  • [46] KINETICS OF THERMAL-OXIDATION OF SILICON IN O2/H2O AND O2/CL2 MIXTURES
    DEAL, BE
    HESS, DW
    PLUMMER, JD
    HO, CP
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1978, 125 (02) : 339 - 346
  • [47] Chemical Effect of H2O on CH4 Oxidation during Combustion in O2/H2O Environments
    Hong, Dikun
    Liu, Liang
    Huang, Yu
    Zheng, Chuguang
    Guo, Xin
    ENERGY & FUELS, 2016, 30 (10) : 8491 - 8498
  • [48] Corrosion of SS310 and Alloy 740 in high temperature supercritical CO2 with impurities H2O and O2
    Li, Kaiyang
    Zeng, Yimin
    Luo, Jing-Li
    CORROSION SCIENCE, 2021, 184
  • [49] Analysis of Porphyrines as Catalysts for Electrochemical Reduction of O2 and Oxidation of H2O
    Baran, Jakub D.
    Gronbeck, Henrik
    Hellman, Anders
    JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2014, 136 (04) : 1320 - 1326
  • [50] Oxidation mechanisms in relation to high temperature crack propagation properties of alloy 718 in H2/H2O inert gas environment
    Browning, PF
    Henry, MF
    Rajan, K
    SUPERALLOYS 718, 625, 706 AND VARIOUS DERIVATIVES, 1996, : 665 - 678