High Temperature Oxidation of the Austenitic (35Fe27Cr31Ni) Alloy Sanicro 28 in O2 + H2O Environment

被引:16
|
作者
Pettersson, C. [1 ]
Jonsson, T. [2 ]
Proff, C. [2 ]
Halvarsson, M. [2 ]
Svensson, J-E. [1 ]
Johansson, L-G. [1 ]
机构
[1] Chalmers Univ Technol, Dept Chem & Biol Engn, High Temp Corros Ctr, S-41296 Gothenburg, Sweden
[2] Chalmers Univ Technol, Dept Appl Phys, S-41296 Gothenburg, Sweden
来源
OXIDATION OF METALS | 2010年 / 74卷 / 1-2期
关键词
Oxidation; Sanicro; 28; Water vapor; Evaporation; WATER-VAPOR; CHROMIUM; OXIDES; 304L;
D O I
10.1007/s11085-010-9199-1
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The present study investigates the high temperature oxidation of alloy Sanicro 28 (35Fe27Cr31Ni) in 5% O-2 and in 5% O-2 + 40% H2O. Polished steel coupons were isothermally exposed in a tube furnace at 600, 700 and 800 A degrees C for up to 168 h. The samples were investigated by gravimetry, grazing angle X-ray diffraction (XRD), Auger electron spectroscopy (AES), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and scanning transmission electron microscopy/energy dispersive X-rays (STEM/EDX). The results show that the material forms a protective scale in both environments. The scale is duplex. The inner part of the scale consists of corundum type chromium-rich (Cr (x) Fe1-x )(2)O-3, and the outer layer consists of spinel type oxide. Chromia is lost from the protective oxide by vaporization of CrO2(OH)(2) in O-2 + H2O environment. The capacity of Sanicro 28 to suffer chromia vaporization without forming a rapidly growing iron-rich oxide is attributed to its high Cr/Fe ratio. The spinel formed at the oxide/gas interface could in addition be beneficial for oxidation behavior in wet oxygen because it may slow down chromia evaporation.
引用
收藏
页码:93 / 111
页数:19
相关论文
共 50 条
  • [11] Oxidation of Binary FeCr Alloys (Fe-2.25Cr, Fe-10Cr, Fe-18Cr and Fe-25Cr) in O2 and in O2 + H2O Environment at 600 °C
    Pujilaksono, B.
    Jonsson, T.
    Heidari, H.
    Halvarsson, M.
    Svensson, J. -E.
    Johansson, L. -G.
    OXIDATION OF METALS, 2011, 75 (3-4): : 183 - 207
  • [12] Oxidation of Binary FeCr Alloys (Fe–2.25Cr, Fe–10Cr, Fe–18Cr and Fe–25Cr) in O2 and in O2 + H2O Environment at 600 °C
    B. Pujilaksono
    T. Jonsson
    H. Heidari
    M. Halvarsson
    J.-E. Svensson
    L.-G. Johansson
    Oxidation of Metals, 2011, 75 : 183 - 207
  • [13] Initial oxidation mechanisms of stainless steel Sanicro 28 (35Fe27Cr31Ni) exposed to KCl, NaCl, and K2CO3 under dry and humid conditions at 535 °C
    Sui, Jingxin
    Lehmusto, Juho
    Bergelin, Mikael
    Hupa, Leena
    CORROSION SCIENCE, 2019, 155 : 29 - 45
  • [14] High temperature oxidation of Fe-Cr alloy in O2-H2-H2O atmospheres;: microstructure and kinetics
    Mikkelsen, L
    Linderoth, S
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 361 (1-2): : 198 - 212
  • [15] HIGH-TEMPERATURE OXIDATION OF FE-18CR-6A1 ALLOY IN A H2/H2O/H2S GASEOUS ENVIRONMENT
    HUANG, TT
    RICHTER, R
    PFENDER, E
    JOURNAL OF METALS, 1984, 36 (07): : 29 - 30
  • [16] Passivation of iron by oxidation in H2O and O2/H2O mixtures
    Roosendaal, SJ
    Bakker, JPR
    Vredenberg, AM
    Habraken, FHPM
    SURFACE SCIENCE, 2001, 494 (03) : 197 - 205
  • [17] KCl-Induced Corrosion of a 304-type Austenitic Stainless Steel in O2 and in O2 + H2O Environment: The Influence of Temperature
    J. Pettersson
    J.-E. Svensson
    L.-G. Johansson
    Oxidation of Metals, 2009, 72 : 159 - 177
  • [18] KCl-Induced Corrosion of a 304-type Austenitic Stainless Steel in O2 and in O2 + H2O Environment: The Influence of Temperature
    Pettersson, J.
    Svensson, J. -E.
    Johansson, L. -G.
    OXIDATION OF METALS, 2009, 72 (3-4): : 159 - 177
  • [19] ADSORPTION OF H2O ON OXIDIZED FE(100) SURFACES - COMPARISON BETWEEN THE OXIDATION OF IRON BY H2O AND O2
    HUNG, WH
    SCHWARTZ, J
    BERNASEK, SL
    SURFACE SCIENCE, 1993, 294 (1-2) : 21 - 32
  • [20] Oxidation of Fe-10Cr in O2 and in O2+H2O environment at 600 °C: A microstructural investigation
    Jonsson, T.
    Pujilaksono, B.
    Heidari, H.
    Liu, F.
    Svensson, J. -E.
    Halvarsson, M.
    Johansson, L-G.
    CORROSION SCIENCE, 2013, 75 : 326 - 336