摘要
Hydrogen ingress into zirconium alloy fuel cladding during operation in nuclear reactors can degrade cladding performance, both during operation and under dry storage, due to formation of brittle hydrides. At temperature and under stress, hydrogen redistribution and reorientation can occur, reducing cladding resistance to failure. Thus, it is crucial to understand the kinetics of hydride dissolution and re-orientation under stress and at temperature. High-energy and micro-beam synchrotron diffraction are used to study the kinetics of hydride reorientation and hydride distribution near a crack tip in previously hydrided Zircaloy sheet. Reorientation of hydrides in bulk samples is studied in situ (at temperature and under applied tensile stress). In-situ transmission diffraction data provides unique strain and orientation information on the hydrides. Micro-beam diffraction has been performed on previously cracked compact tension specimens under load. Measurement of the hydride distribution and associated strains can be performed with the micro-beam to determine hydrogen response to an applied strain field.
引用
收藏
页码:683 / 688
页数:6
相关论文
共 50 条
  • [31] Effect of hydride orientation on fracture toughness of Zircaloy-4 cladding
    Hsu, Hsiao-Hung
    Tsay, Leu-Wen
    JOURNAL OF NUCLEAR MATERIALS, 2011, 408 (01) : 67 - 72
  • [32] Hydrogen in Zircaloy-4: effects of the neutron irradiation on the hydride formation
    Pablo Vizcaíno
    Abraham D. Banchik
    José P. Abriata
    Journal of Materials Science, 2007, 42 : 6633 - 6637
  • [33] Hydrogen in Zircaloy-4:: effects of the neutron irradiation on the hydride formation
    Vizcaino, Pablo
    Banchik, Abraham D.
    Abriata, Jose P.
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (16) : 6633 - 6637
  • [34] Fracture of Zircaloy-4 fuel cladding tubes with hydride blisters
    Macdonald, Vincent
    Le Boulch, David
    de Menibus, Arthur Hellouin
    Besson, Jacques
    Auzoux, Quentin
    Crepin, Jerome
    Le Jolu, Thomas
    20TH EUROPEAN CONFERENCE ON FRACTURE, 2014, 3 : 233 - 238
  • [36] Hydride phase dissolution enthalpy in neutron irradiated Zircaloy-4
    Vizcaíno, P
    Banchik, AD
    Abriata, JP
    JOURNAL OF NUCLEAR MATERIALS, 2005, 336 (01) : 54 - 64
  • [37] Formation and characterization of hydride blisters in Zircaloy-4 cladding tubes
    de Menibus, Arthur Hellouin
    Auzoux, Quentin
    Dieye, Ousmane
    Berger, Pascal
    Bosonnet, Sophie
    Foy, Eddy
    Macdonald, Vincent
    Besson, Jacques
    Crepin, Jerome
    JOURNAL OF NUCLEAR MATERIALS, 2014, 449 (1-3) : 132 - 147
  • [38] Embrittlement behavior of zircaloy-4 cladding during oxidation and water quench
    Kim, JH
    Lee, MH
    Choi, BK
    Jeong, YH
    NUCLEAR ENGINEERING AND DESIGN, 2005, 235 (01) : 67 - 75
  • [39] Effects of Hydrogenation on the Corrosion Behavior of Zircaloy-4
    Yue, Huifang
    Zhou, Mingyang
    Zhao, Yanli
    Han, Yinjie
    Liu, Shichao
    Geng, Laiyao
    Xu, Shitong
    Xin, Yong
    Yao, Meiyi
    MATERIALS, 2024, 17 (05)
  • [40] Electrochemical behavior of hydrogen precipitated Zircaloy-4
    Rafique, Mohsin
    Afzal, Naveed
    Deen, K. M.
    Kim, Yong-Soo
    MODERN PHYSICS LETTERS B, 2015, 29 (32):