Effect of hydride orientation on fracture toughness of Zircaloy-4 cladding

被引:35
|
作者
Hsu, Hsiao-Hung [1 ,2 ]
Tsay, Leu-Wen [2 ]
机构
[1] INER, Lungtan Township 325, Taoyuan County, Taiwan
[2] Natl Taiwan Ocean Univ, Inst Mat Engn, Chilung 202, Taiwan
关键词
STRESS ORIENTATION; HYDROGEN; ZIRCONIUM; SOLUBILITY;
D O I
10.1016/j.jnucmat.2010.10.068
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hydrogen embrittlement is one of the major degradation mechanisms for high burnup fuel cladding during reactor service and spent fuel dry storage, which is related to the hydrogen concentration, morphology and orientation of zirconium hydrides. In this work, the J-integral values for X-specimens with different hydride orientations are measured to evaluate the fracture toughness of Zircaloy-4 (Zry-4) cladding. The toughness values for Zry-4 cladding with various percentages of radial hydrides are much smaller than those with circumferential hydrides only in the same hydrogen content level at 25 degrees C. The fractograghic features reveal that the crack path is influenced by the orientation of zirconium hydride. Moreover, the fracture toughness measurements for X-specimens at 300 degrees C are not sensitive to a variation in hydride orientation but to hydrogen concentration. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:67 / 72
页数:6
相关论文
共 50 条
  • [1] The influence of hydride on fracture toughness of recrystallized Zircaloy-4 cladding
    Hsu, Hsiao-Hung
    Chiang, Ming-Feng
    Chen, Yen-Chen
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2014, 447 (1-3) : 56 - 62
  • [2] Fracture of Zircaloy-4 fuel cladding tubes with hydride blisters
    Macdonald, Vincent
    Le Boulch, David
    de Menibus, Arthur Hellouin
    Besson, Jacques
    Auzoux, Quentin
    Crepin, Jerome
    Le Jolu, Thomas
    [J]. 20TH EUROPEAN CONFERENCE ON FRACTURE, 2014, 3 : 233 - 238
  • [3] Hydride reorientation in Zircaloy-4 cladding
    Chu, H. C.
    Wu, S. K.
    Kuo, R. C.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2008, 373 (1-3) : 319 - 327
  • [4] Assessing the fracture toughness of Zircaloy-4 fuel rod cladding tubes: impact of delayed hydride cracking
    Francois, Pierrick
    Petit, Tom
    Auzoux, Quentin
    Le Boulch, David
    Nascimento, Isabela Zarpellon
    Besson, Jacques
    [J]. INTERNATIONAL JOURNAL OF FRACTURE, 2024, 247 (01) : 51 - 72
  • [5] Formation of hydride in zircaloy-4 cladding tube
    Choi, Y
    [J]. JOURNAL OF MATERIALS SCIENCE LETTERS, 1997, 16 (01) : 66 - 67
  • [6] Influence of the crack-tip hydride concentration on the fracture toughness of Zircaloy-4
    Bertolino, G
    Ipiña, JP
    Meyer, G
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2006, 348 (1-2) : 205 - 212
  • [7] Effects of hydride morphology on the embrittlement of Zircaloy-4 cladding
    Kim, Ju-Seong
    Kim, Tae-Hoon
    Kook, Dong-Hak
    Kim, Yong-Soo
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2015, 456 : 235 - 245
  • [8] Effects of hydride rim on the ductility of Zircaloy-4 cladding
    Kim, Ju-Seong
    Kim, Ho-A
    Kang, So-Young
    Kim, Yong-Soo
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2019, 523 : 383 - 390
  • [9] The influence of hydride blisters on the fracture of Zircaloy-4
    Pierron, ON
    Koss, DA
    Motta, AT
    Chan, KS
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2003, 322 (01) : 21 - 35
  • [10] Formation and characterization of hydride blisters in Zircaloy-4 cladding tubes
    de Menibus, Arthur Hellouin
    Auzoux, Quentin
    Dieye, Ousmane
    Berger, Pascal
    Bosonnet, Sophie
    Foy, Eddy
    Macdonald, Vincent
    Besson, Jacques
    Crepin, Jerome
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2014, 449 (1-3) : 132 - 147