Effects of hydride morphology on the embrittlement of Zircaloy-4 cladding

被引:61
|
作者
Kim, Ju-Seong [1 ]
Kim, Tae-Hoon [2 ]
Kook, Dong-Hak [1 ]
Kim, Yong-Soo [2 ]
机构
[1] Korea Atom Energy Res Inst, Taejon 305353, South Korea
[2] Hanyang Univ, Seoul 133791, South Korea
关键词
MECHANICAL-PROPERTIES; LATERAL COMPRESSION; FRACTURE-TOUGHNESS; RADIAL HYDRIDES; HYDROGEN; STRESS; BEHAVIOR; TUBES; REORIENTATION; TEMPERATURE;
D O I
10.1016/j.jnucmat.2014.09.025
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Spent nuclear fuel claddings discharged from water reactors contain hydrogen up to 800 wppm depending on the burn-up and power history. During long-term dry storage, the cladding temperature slowly decreases with diminishing decay heat and absorbed hydrogen atoms are precipitated in Zr-matrix according to the terminal solid solubility of hydrogen. Under these conditions, hydrides can significantly reduce cladding ductility and impact resistance, especially when the radial hydrides are massively present in the material. In this study, the effects of hydride morphology on the embrittlement of Zircaloy-4 cladding were investigated using a ring compression test. The results show that circumferentially hydrided Zircaloy-4 cladding is brittle at room temperature but its ductility is regained substantially as the temperature goes above 150 degrees C. On the other hand, radially hydrided cladding remains brittle at 150 degrees C and micro-cracks developed in the radial hydrides can act as crack propagation paths. Fracture energy analysis shows that ductile to brittle transition temperature is low in between 25 degrees C and 100 degrees C in the former case, whereas it lies in between 200 degrees C and 250 degrees C in the latter case. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:235 / 245
页数:11
相关论文
共 50 条
  • [1] Effects of hydride rim on the ductility of Zircaloy-4 cladding
    Kim, Ju-Seong
    Kim, Ho-A
    Kang, So-Young
    Kim, Yong-Soo
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2019, 523 : 383 - 390
  • [2] Hydride reorientation in Zircaloy-4 cladding
    Chu, H. C.
    Wu, S. K.
    Kuo, R. C.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2008, 373 (1-3) : 319 - 327
  • [3] Radial-hydride embrittlement of high-burnup Zircaloy-4 fuel cladding
    Daum, Robert S.
    Majumdar, Saurin
    Liu, Yung
    Billone, Michael C.
    [J]. JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 2006, 43 (09) : 1054 - 1067
  • [4] Formation of hydride in zircaloy-4 cladding tube
    Choi, Y
    [J]. JOURNAL OF MATERIALS SCIENCE LETTERS, 1997, 16 (01) : 66 - 67
  • [5] INFLUENCE OF AN OXIDE LAYER ON THE HYDRIDE EMBRITTLEMENT IN ZIRCALOY-4
    BAI, JB
    [J]. SCRIPTA METALLURGICA ET MATERIALIA, 1993, 29 (05): : 617 - 622
  • [6] HYDRIDE EMBRITTLEMENT IN ZIRCALOY-4 PLATE .2. INTERACTION BETWEEN THE TENSILE-STRESS AND THE HYDRIDE MORPHOLOGY
    BAI, JB
    JI, N
    GILBON, D
    PRIOUL, C
    FRANCOIS, D
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1994, 25 (06): : 1199 - 1208
  • [7] The influence of hydride on fracture toughness of recrystallized Zircaloy-4 cladding
    Hsu, Hsiao-Hung
    Chiang, Ming-Feng
    Chen, Yen-Chen
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2014, 447 (1-3) : 56 - 62
  • [8] Effect of hydride orientation on fracture toughness of Zircaloy-4 cladding
    Hsu, Hsiao-Hung
    Tsay, Leu-Wen
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2011, 408 (01) : 67 - 72
  • [9] Fracture of Zircaloy-4 fuel cladding tubes with hydride blisters
    Macdonald, Vincent
    Le Boulch, David
    de Menibus, Arthur Hellouin
    Besson, Jacques
    Auzoux, Quentin
    Crepin, Jerome
    Le Jolu, Thomas
    [J]. 20TH EUROPEAN CONFERENCE ON FRACTURE, 2014, 3 : 233 - 238
  • [10] Formation and characterization of hydride blisters in Zircaloy-4 cladding tubes
    de Menibus, Arthur Hellouin
    Auzoux, Quentin
    Dieye, Ousmane
    Berger, Pascal
    Bosonnet, Sophie
    Foy, Eddy
    Macdonald, Vincent
    Besson, Jacques
    Crepin, Jerome
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2014, 449 (1-3) : 132 - 147