摘要
Simulated loss of coolant accident (LOCA) tests on Zircaloy-4 cladding were carried out to evaluate the thermal shock property during the injection of emergency core coolant. A Zircaloy-4 specimen was oxidized in a steam environment between 1000 and 1250 degreesC followed by a flooding of the cooling water. After the test, the ductility of the thermally embrittled specimen was measured by a ring-compression test and a microstructural analysis was carried out. The results showed that the threshold equivalent cladding reacted (ECR) value to cause a failure was higher than the conventional 17% criterion calculated by the Baker-Just equation. A residual metal thickness under 0.3 mm as well as a ring-compression ductility below 0.2 mm for a fracture is effective to assess the thermal shock embrittlement of Zircaloy-4 in an axially unrestrained, or even in a restrained condition. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:67 / 75
页数:9
相关论文
共 50 条
  • [1] Failure behavior of Zircaloy-4 cladding after oxidation and water quench
    Kim, Jun Hwan
    Lee, Myoung Ho
    Choi, Byoung Kwon
    Jeong, Yong Hwan
    JOURNAL OF NUCLEAR MATERIALS, 2007, 362 (01) : 36 - 45
  • [2] The effect of oxidation-and-quenching process during a LOCA on the behavior of the oxidation and embrittlement of Zircaloy-4 cladding under reheating transients
    Miwa, Hideki
    Amaya, Masaki
    JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 2016, 53 (12) : 2090 - 2097
  • [3] Effects of hydride morphology on the embrittlement of Zircaloy-4 cladding
    Kim, Ju-Seong
    Kim, Tae-Hoon
    Kook, Dong-Hak
    Kim, Yong-Soo
    JOURNAL OF NUCLEAR MATERIALS, 2015, 456 : 235 - 245
  • [4] Analysis of the Secondary Cladding Hydrogenation During the Quench-LOCA Bundle Tests With Zircaloy-4 Claddings and its Influence on the Cladding Embrittlement
    Grosse, M.
    Stuckert, J.
    Roessger, C.
    Steinbrueck, M.
    Walter, M.
    Kaestner, A.
    ZIRCONIUM IN THE NUCLEAR INDUSTRY, 2015, 1543 : 1054 - 1073
  • [5] Investigation of the oxidation behavior of Zircaloy-4 cladding in a mixture of air and steam
    Nemoto, Yoshiyuki
    Ishijima, Yasuhiro
    Kondo, Keietsu
    Fujimura, Yuki
    Kaji, Yoshiyuki
    JOURNAL OF NUCLEAR MATERIALS, 2023, 575
  • [6] Effect of surface roughness on the texture and oxidation behavior of Zircaloy-4 cladding tube
    Akhiani, Hamed
    Szpunar, Jerzy A.
    APPLIED SURFACE SCIENCE, 2013, 285 : 832 - 839
  • [7] High-temperature oxidation and quench behaviour of Zircaloy-4 and E110 cladding alloys
    Steinbrueck, M.
    Birchley, J.
    Boldyrev, A. V.
    Goryachev, A. V.
    Grosse, M.
    Haste, T. J.
    Hozer, Z.
    Kisselev, A. E.
    Nalivaev, V. I.
    Semishkin, V. P.
    Sepold, L.
    Stuckert, J.
    Ver, N.
    Veshchunov, M. S.
    PROGRESS IN NUCLEAR ENERGY, 2010, 52 (01) : 19 - 36
  • [8] Contribution to the understanding of the effect of the water chemistry on the oxidation kinetics of Zircaloy-4 cladding
    Pêcheur, D
    Godlewski, J
    Peybernès, J
    Fayette, L
    Noé, M
    Frichet, A
    Kerrec, O
    Urbanic, VF
    Cheng, B
    Cox, B
    ZIRCONIUM IN THE NUCLEAR INDUSTRY: TWELFTH INTERNATIONAL SYMPOSIUM, 2000, 1354 : 793 - 811
  • [9] EMBRITTLEMENT OF ZIRCALOY-4 DUE TO OXIDATION IN ENVIRONMENT OF STAGNANT STEAM
    UETSUKA, H
    FURUTA, T
    KAWASAKI, S
    JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 1982, 19 (02) : 158 - 165
  • [10] ZIRCALOY-4 CLADDING EMBRITTLEMENT DUE TO INNER SURFACE OXIDATION UNDER SIMULATED LOSS-OF-COOLANT CONDITION
    UETSUKA, H
    FURUTA, T
    KAWASAKI, S
    JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 1981, 18 (09) : 705 - 717