High-temperature oxidation and quench behaviour of Zircaloy-4 and E110 cladding alloys

被引:52
|
作者
Steinbrueck, M. [1 ]
Birchley, J. [2 ]
Boldyrev, A. V. [3 ]
Goryachev, A. V. [4 ]
Grosse, M. [1 ]
Haste, T. J. [2 ]
Hozer, Z. [5 ]
Kisselev, A. E. [3 ]
Nalivaev, V. I. [6 ]
Semishkin, V. P. [7 ]
Sepold, L. [1 ]
Stuckert, J. [1 ]
Ver, N. [5 ]
Veshchunov, M. S. [3 ]
机构
[1] KIT, D-76021 Karlsruhe, Germany
[2] Paul Scherrer Inst, NES LTH, OVGA 312, CH-5232 Villigen, Switzerland
[3] Russian Acad Sci, Nucl Safety Inst IBRAE, Moscow 115191, Russia
[4] RIAR, Dimitrovgrad 433510 10, Russia
[5] KFKI Atom Energy Res Inst AEKI, H-1525 Budapest, Hungary
[6] NPO Luch, Podolsk 142100, Russia
[7] OKB GIDROPRESS, Podolsk 142103, Russia
关键词
Severe accidents; Safety; Zircaloy; Cladding; Oxidation; ACCIDENT CODE CALCULATIONS; ZIRCONIUM ALLOYS; KINETICS; STEAM;
D O I
10.1016/j.pnucene.2009.07.012
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
This paper gives an overview on the status of knowledge of high-temperature oxidation of the two zirconium alloys Zircaloy-4 and E110 with special emphasis on results obtained during the SARNET period. The tin-bearing alloy Zircaloy-4 and the niobium-bearing alloy E110 are the materials for cladding and structures used in pressurised water reactors of the Western-type and VVERs and RBMKs, respectively. Results of separate-effects tests, single-rod tests, and large-scale bundle experiments are summarised. Focus is directed to oxidation kinetics at high temperature, hydrogen release and absorption by the remaining metal, and behaviour during quenching. Both materials behave very similarly as long as the superficial oxide scales formed during oxidation are dense and protective. Main differences are seen in connection with breakaway oxidation which leads to enhanced oxidation and hydrogen uptake and thus embrittlement and possibly earlier failure of the cladding. The temperature range at which pronounced breakaway is observed is different for the two alloys. The status of modelling of oxidation kinetics, thermo-mechanical behaviour during cooldown and the influence of irradiation are discussed at the end of the paper. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:19 / 36
页数:18
相关论文
共 50 条
  • [1] OXIDATION OF ZIRCALOY-4 WITH HIGH-TEMPERATURE AIR
    SULISTIJONO
    BOUDEN, A
    CHERFAOUI, M
    BERANGER, G
    LAMBERTIN, M
    [J]. JOURNAL DE PHYSIQUE IV, 1993, 3 (C9): : 439 - 445
  • [2] High-temperature oxidation kinetics of sponge-based E110 cladding alloy
    Yan, Yong
    Garrison, Benton E.
    Howell, Mike
    Bell, Gary L.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2018, 499 : 595 - 612
  • [3] Embrittlement behavior of zircaloy-4 cladding during oxidation and water quench
    Kim, JH
    Lee, MH
    Choi, BK
    Jeong, YH
    [J]. NUCLEAR ENGINEERING AND DESIGN, 2005, 235 (01) : 67 - 75
  • [4] HIGH-TEMPERATURE OXIDATION OF ZIRCALOY-2 AND ZIRCALOY-4 IN STEAM
    URBANIC, VF
    HEIDRICK, TR
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1978, 75 (02) : 251 - 261
  • [5] HIGH-TEMPERATURE OXIDATION OF ZIRCALOY-4 IN DILUTED STEAM
    UETSUKA, H
    OTOMO, T
    [J]. JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 1989, 26 (02) : 240 - 248
  • [6] Failure behavior of Zircaloy-4 cladding after oxidation and water quench
    Kim, Jun Hwan
    Lee, Myoung Ho
    Choi, Byoung Kwon
    Jeong, Yong Hwan
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2007, 362 (01) : 36 - 45
  • [7] High-Temperature Secondary Hydriding Experiments with E110 and E110G Cladding
    Hozer, Zoltan
    Nagy, Imre
    Vimi, Andras
    Kunstar, Mihaly
    Szabo, Peter
    Novotny, Tamas
    Perez-Fero, Erzsebet
    Kis, Zoltan
    Szentmiklosi, Laszlo
    Horvath, Marta
    Csordas, Anna Pinter
    Barsy, Eszter
    Kulacsy, Katalin
    Grosse, Mirco
    [J]. ZIRCONIUM IN THE NUCLEAR INDUSTRY: 18TH INTERNATIONAL SYMPOSIUM, 2018, 1597 : 1093 - 1113
  • [8] EFFECT OF THE INTERMEDIATE COOLING PROCESS ON THE BEHAVIOR OF ZIRCALOY-4 CLADDING AFTER A HIGH-TEMPERATURE OXIDATION
    Kim, Jun Hwan
    Choi, Byoung Kwon
    Jeong, Yong Hwan
    Oh, Seung Jin
    [J]. NUCLEAR TECHNOLOGY, 2009, 165 (02) : 241 - 248
  • [9] OXIDATION OF ZIRCALOY-4 UNDER HIGH-TEMPERATURE STEAM ATMOSPHERE AND ITS EFFECT ON DUCTILITY OF CLADDING
    KAWASAKI, S
    FURUTA, T
    SUZUKI, M
    [J]. JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 1978, 15 (08) : 589 - 596
  • [10] High-Temperature Oxidation of Zircaloy-4 in Oxygen–Nitrogen Mixtures
    Martin Steinbrück
    Steffi Schaffer
    [J]. Oxidation of Metals, 2016, 85 : 245 - 262