Microhardness of resin composites polymerized by plasma arc or conventional visible light curing

被引:0
|
作者
Park, SH [1 ]
Krejci, I [1 ]
Lutz, F [1 ]
机构
[1] NHIC, Ilsan Hosp, Dept Conservat Dent, Iksan Gu, Seoul, South Korea
关键词
D O I
暂无
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
This study evaluated the effectiveness of the plasma are curing (PAC) unit for composite curing. To compare its effectiveness with conventional quartz tungsten halogen (QTH) light curing units, the microhardness of two composites (Z100 and Tetric Ceram) that had been light cured by the PAC or QTH units, were compared according to the depth from, the composite surface. In addition, linear polymerization shrinkage was compared using a custom-made linometer between composites which were light cured by PAC or QTH units. Measuring polymerization shrinkage for two resin composites Z100 and Tetric Ceram) was performed after polymerization with either QTH or PAC units. In the case of curing with the PAC unit, the composite was light cured with Apollo 95E for two (Group 1), three (Group 2), six (Group 3) or 2 x 6 (Group 4) seconds. For light curing with the QTH unit, the composite was light cured for 60 seconds with Optilux 500 (Group 5). The linear polymerization shrinkage of composites was determined in the linometer. Two resin composites were used to measure microhardness. Two-mm. thick samples were light cured for three seconds (Group 1), six seconds (Group 2) or 12 (2 x 6) seconds (Group 3) with Apollo 95E or they were conventionally light cured with Optilux 500 for 30 seconds (Group 4) or 60 seconds (Group 5). For 3 mm thick samples, the composites were light cured for six seconds (Group 1), 12 (2 x 6) seconds (Group 2) or 18 (3 x 6) seconds (Group 3) with Apollo 95E or they were conventionally light cured with Optilux 500 for 30 seconds (Group 4) or 60 seconds (Group 5). Twenty samples were assigned to each group. The microhardness of the upper and lower surfaces was measured with a Vickers hardness-measuring instrument under load. The difference in microhardness between the upper and lower surfaces in each group was analyzed by paired t-test. For the upper or lower surfaces, one-way ANOVA with Tukey was used. For Tetric Ceram, the amount of polymerization shrinkage was lower when cured with the Apollo 95E for two or three seconds than when cured for six and 12 (2 x 6) seconds, or for 60 seconds with Optilux 500 (p<0.05). For Z100, the amount of linear polymerization shrinkage was lower when cured with the Apollo 95E for two, three and six seconds than for 12 (2 x 6) seconds with Apollo 95E or for 60 seconds with the Optilux 500 (p<0.05). The results of the microhardness test indicated that there was no statistically significant difference in microhardness between groups for the upper surface. However, for the lower surface, when the composites were light cured with Apollo 95E for three seconds as recommended by the manufacturer, microhardness of the lower surface was usually lower than that of the upper surface and did not cure sufficiently. Conclusively, when compared with conventional QTH unit, the PAC unit, Apollo 95E did not properly cure the lower composite surface when the layer thickness exceeded 2 mm. In addition, three seconds of curing time, which the manufacturer recommended, was insufficient for optimal curing of composites.
引用
收藏
页码:30 / 37
页数:8
相关论文
共 50 条
  • [1] Material characteristics of resin composites polymerized with plasma arc and conventional halogen curing units.
    Davids, H.
    Danesh, G.
    Reinhardt, K. -J.
    Ott, K. H. R.
    Schaefer, E.
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : B199 - B199
  • [2] Wear of resin composites polymerized by conventional halogen light curing and light emitting diodes curing units
    Kim, H
    Park, SH
    Jung, IY
    Jeon, SB
    Lee, KY
    ASBM6: ADVANCED BIOMATERIALS VI, 2005, 288-289 : 645 - 648
  • [3] Characterization of resin composites polymerized with plasma are curing units
    Peutzfeldt, A
    Sahafi, A
    Asmussen, E
    DENTAL MATERIALS, 2000, 16 (05) : 330 - 336
  • [4] Microhardness evaluation of resin composites polymerized by three different light sources
    Hubbezoglu, Ihsan
    Bolayir, Giray
    Dogan, Orhan Murat
    Dogan, Arife
    Ozer, Ali
    Bek, Buelent
    DENTAL MATERIALS JOURNAL, 2007, 26 (06) : 845 - 853
  • [5] The comparison of visible light curing unit and plasma ARC curing unit with the degree of conversion of composite resin
    Park, JH
    Choi, NK
    Yang, KH
    JOURNAL OF DENTAL RESEARCH, 2001, 80 (04) : 1352 - 1352
  • [6] Microhardness of resin composites with high-intensity light curing.
    El-Mowafy, O
    El-Badrawy, W
    Ghandi, D
    Deniz, B
    Rosca, G
    Karastathis, D
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : A499 - A499
  • [7] Assessment of Microhardness of Conventional and Bulk-Fill Resin Composites Using Different Light-Curing Intensity
    Jakupovic, Selma
    Pervan, Nedim
    Mesic, Elmedin
    Gavranovic-Glamoc, Alma
    Bajsman, Anita
    Muratovic, Enis
    Kazazic, Lejla
    Kantardzic-Kovacevic, Alma
    POLYMERS, 2023, 15 (10)
  • [8] Microhardness of flowable resin composites with high-intensity light curing.
    El-Badrawy, W.
    Encioiu, A.
    El-Mowafy, O.
    Karastathis, D.
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : B330 - B330
  • [9] Effect of Light Curing Distance on Microhardness Profiles of Bulk-Fill Resin Composites
    Hasanain, Fatin A.
    Nassar, Hani M.
    Ajaj, Reem A.
    POLYMERS, 2022, 14 (03)
  • [10] In vitro microleakage of a fissure sealant polymerized by either a quartz tungsten halogen curing light or a plasma arc curing light
    Shah, Sarah
    Roebuck, Elizabeth M.
    Nugent, Zoann
    Deery, Chris
    INTERNATIONAL JOURNAL OF PAEDIATRIC DENTISTRY, 2007, 17 (05) : 371 - 377