Valorization of Ceramic Waste Powder for Compressive Strength and Durability of Fly Ash Geopolymer Cement

被引:10
|
作者
Rashad, Alaa M. [1 ,2 ]
Essa, Ghada M. F. [1 ]
Mosleh, Youssef A. [1 ]
Morsi, W. M. [3 ]
机构
[1] Housing & Bldg Natl Res Ctr HBRC, Bldg Mat Res & Qual Control Inst, Cairo, Egypt
[2] Shaqra Univ, Coll Engn, Civil Engn Dept, Al Dawadmi, Riyadh, Saudi Arabia
[3] Housing & Bldg Natl Res Ctr HBRC, Bldg Phys Res Inst, Cairo, Egypt
关键词
Ceramic waste powder; Fly ash geopolymer; Workability; Compressive strength; Durability; ALKALI-ACTIVATED MORTARS; MECHANICAL-PROPERTIES; REACTION-PRODUCTS; METAKAOLIN; MICROSTRUCTURE; REPLACEMENT; CONCRETE; PASTES; CAO;
D O I
10.1007/s13369-023-08428-x
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Enormous amounts of ceramic and fly ash (FA) wastes are generated annually by ceramic industries/demolition/rejected units and thermal power plants. To preserve virgin natural resources, limit disposal amounts, and limit environmental pollution, these wastes can be applied in the construction field as a binder material after alkali activation. This work aims to get rid ceramic waste powder (CWP) by recycling it as a part of FA geopolymer cement activated with sodium silicate to get improved properties, especially those after exposed to severe conditions. For this purpose, the FA was partially replaced with CWP at levels ranging from 10 to 50% with a stride of 10 wt.%. The effect of CWP on the flowability, compressive strength, up to 240 days, and different durability aspects were investigated. After curing for 28 days, specimens were subjected to three different types of durability: accelerating aging, wetting/drying cycles in sodium sulfate solution, and simulated tidal zone. The identification of the different decomposition phases was accomplished through the utilization of X-ray diffraction (XRD), thermogravimetric analysis (TGA)/its derivative (TGA), and scanning electron microscopy (SEM). The results showed 27.5-55% reduction in the flowability with including 10-50% CWP. The compressive strength increased with including up to 40% CWP. The 28 days compressive strength was enhanced by 20.1-42.97% with including 10-40% CWP. All different types of properties were enhanced with the incorporation of up to 40% CWP. Contrarily, incorporating 50% CWP showed a negative effect on compressive strength and different types of durability. The XRD of the neat FA geopolymer sample before and after exposure to severe conditions showed the crystalline phases of quartz, hematite and mullite, whilst that containing CWP showed the crystalline phases of quartz, mullite, hematite and albite. The TGA analysis showed the formation of aluminosilicate (N-A-S-H) gel as the main hydration product in the samples with/without CWP, the amount of this gel decreased after exposure to severe conditions.
引用
收藏
页码:2767 / 2795
页数:29
相关论文
共 50 条
  • [41] Compressive strength of laterite soil stabilized with rice straw ash and fly ash based geopolymer
    Rangan, P. R.
    Irmawaty, R.
    Amiruddin, A. A.
    Bakri, B.
    3RD INTERNATIONAL CONFERENCE ON CIVIL AND ENVIRONMENTAL ENGINEERING (ICCEE 2019), 2020, 419
  • [42] Using Artificial Neural Networks for the Prediction of the Compressive Strength of Geopolymer Fly Ash
    Rusna, K. P.
    Kalpana, V. G.
    ENGINEERING TECHNOLOGY & APPLIED SCIENCE RESEARCH, 2022, 12 (05) : 9120 - 9125
  • [43] Modeling compressive strength of Moroccan fly ash-phosphogypsum geopolymer bricks
    Bebana, Mohamed Vadel
    Ziat, Khadija
    Semlal, Nawal
    Saidi, Mohamed
    SN APPLIED SCIENCES, 2019, 1 (12):
  • [44] Characteristics of the compressive strength on C – Type fly ash based geopolymer mortar
    Bachtiar, E.
    Lowland Technology International, 2020, 22 (02) : 178 - 191
  • [45] Optimum mix for fly ash geopolymer binder based on workability and compressive strength
    Arafa, S. A.
    Ali, A. Z. M.
    Awal, A. S. M. A.
    Loon, L. Y.
    4TH INTERNATIONAL CONFERENCE ON CIVIL AND ENVIRONMENTAL ENGINEERING FOR SUSTAINABILITY (ICONCEES 2017), 2018, 140
  • [46] Effect Of Crumb Rubber On Compressive Strength Of Fly Ash Based Geopolymer Concrete
    Azmi, Ahmad Azrem
    Abdullah, Mohd Mustafa Al Bakri
    Ghazali, Che Mohd Ruzaidi
    Sandu, Andrei Victor
    Hussin, Kamarudin
    2ND INTERNATIONAL CONFERENCE ON GREEN DESIGN AND MANUFACTURE 2016 (ICONGDM 2016), 2016, 78
  • [47] Compressive strength of fly-ash-based geopolymer concrete at elevated temperatures
    Shaikh, F. U. A.
    Vimonsatit, V.
    FIRE AND MATERIALS, 2015, 39 (02) : 174 - 188
  • [48] Compressive strength, flexural strength, and durability of high-volume fly ash concrete
    Rajput Babalu
    Agarwal Anil
    Kore Sudarshan
    Pawar Amol
    Innovative Infrastructure Solutions, 2023, 8
  • [49] Compressive strength, flexural strength, and durability of high-volume fly ash concrete
    Babalu, Rajput
    Anil, Agarwal
    Sudarshan, Kore
    Amol, Pawar
    INNOVATIVE INFRASTRUCTURE SOLUTIONS, 2023, 8 (05)
  • [50] Study on Strength and Durability of Cellular-Cement Fly Ash Blocks
    Baskaran, K.
    Jayakody, J. R. U. C.
    Sandaruwan, M. A. R.
    2019 MORATUWA ENGINEERING RESEARCH CONFERENCE (MERCON) / 5TH INTERNATIONAL MULTIDISCIPLINARY ENGINEERING RESEARCH CONFERENCE, 2019, : 31 - 35