Valorization of Ceramic Waste Powder for Compressive Strength and Durability of Fly Ash Geopolymer Cement

被引:10
|
作者
Rashad, Alaa M. [1 ,2 ]
Essa, Ghada M. F. [1 ]
Mosleh, Youssef A. [1 ]
Morsi, W. M. [3 ]
机构
[1] Housing & Bldg Natl Res Ctr HBRC, Bldg Mat Res & Qual Control Inst, Cairo, Egypt
[2] Shaqra Univ, Coll Engn, Civil Engn Dept, Al Dawadmi, Riyadh, Saudi Arabia
[3] Housing & Bldg Natl Res Ctr HBRC, Bldg Phys Res Inst, Cairo, Egypt
关键词
Ceramic waste powder; Fly ash geopolymer; Workability; Compressive strength; Durability; ALKALI-ACTIVATED MORTARS; MECHANICAL-PROPERTIES; REACTION-PRODUCTS; METAKAOLIN; MICROSTRUCTURE; REPLACEMENT; CONCRETE; PASTES; CAO;
D O I
10.1007/s13369-023-08428-x
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Enormous amounts of ceramic and fly ash (FA) wastes are generated annually by ceramic industries/demolition/rejected units and thermal power plants. To preserve virgin natural resources, limit disposal amounts, and limit environmental pollution, these wastes can be applied in the construction field as a binder material after alkali activation. This work aims to get rid ceramic waste powder (CWP) by recycling it as a part of FA geopolymer cement activated with sodium silicate to get improved properties, especially those after exposed to severe conditions. For this purpose, the FA was partially replaced with CWP at levels ranging from 10 to 50% with a stride of 10 wt.%. The effect of CWP on the flowability, compressive strength, up to 240 days, and different durability aspects were investigated. After curing for 28 days, specimens were subjected to three different types of durability: accelerating aging, wetting/drying cycles in sodium sulfate solution, and simulated tidal zone. The identification of the different decomposition phases was accomplished through the utilization of X-ray diffraction (XRD), thermogravimetric analysis (TGA)/its derivative (TGA), and scanning electron microscopy (SEM). The results showed 27.5-55% reduction in the flowability with including 10-50% CWP. The compressive strength increased with including up to 40% CWP. The 28 days compressive strength was enhanced by 20.1-42.97% with including 10-40% CWP. All different types of properties were enhanced with the incorporation of up to 40% CWP. Contrarily, incorporating 50% CWP showed a negative effect on compressive strength and different types of durability. The XRD of the neat FA geopolymer sample before and after exposure to severe conditions showed the crystalline phases of quartz, hematite and mullite, whilst that containing CWP showed the crystalline phases of quartz, mullite, hematite and albite. The TGA analysis showed the formation of aluminosilicate (N-A-S-H) gel as the main hydration product in the samples with/without CWP, the amount of this gel decreased after exposure to severe conditions.
引用
收藏
页码:2767 / 2795
页数:29
相关论文
共 50 条
  • [31] Comparison of strength and durability characteristics of a geopolymer produced from fly ash, ground glass fiber and glass powder
    Rashidian-Dezfouli, H.
    Rangaraju, P. R.
    MATERIALES DE CONSTRUCCION, 2017, 67 (328)
  • [32] Phosphate-based geopolymer: Influence of municipal solid waste fly ash introduction on structure and compressive strength
    Bernasconi, Davide
    Viani, Alberto
    Zarybnicka, Lucie
    Macova, Petra
    Bordignon, Simone
    Caviglia, Caterina
    Destefanis, Enrico
    Gobetto, Roberto
    Pavese, Alessandro
    CERAMICS INTERNATIONAL, 2023, 49 (13) : 22149 - 22159
  • [33] Experimental Investigation on Strength and Durability of Fly Ash and GGBS Based Geopolymer Concrete
    Asha, G.
    Antony, Jiji
    PROCEEDINGS OF STRUCTURAL ENGINEERING AND CONSTRUCTION MANAGEMENT, SECON'19, 2020, 46 : 53 - 64
  • [34] Optimization of Alkaline Activator/fly ASH Ratio on The Compressive Strength of Manufacturing Fly ASH-BASED Geopolymer
    Al Bakri, A. M. Mustafa
    Kamarudin, H.
    Karem, Omar A. K. A.
    Ruzaidi, C. M.
    Rafiza, A. R.
    Norazian, M. N.
    MECHANICAL AND AEROSPACE ENGINEERING, PTS 1-7, 2012, 110-116 : 734 - +
  • [35] COMPRESSIVE STRENGTH AND DURABILITY OF CONCRETE WITH COCONUT SHELL ASH AS CEMENT REPLACEMENT
    Adajar, Mary Ann
    Galupino, Joenel
    Frianeza, Cielo
    Faye Aguilon, Jilliane
    Sy, Jan Brayden
    Tan, Paul Adrian
    INTERNATIONAL JOURNAL OF GEOMATE, 2020, 18 (70): : 183 - 190
  • [36] THE INFLUENCE OF MODIFIED FLY ASH PARTICLES BY HEATING ON THE COMPRESSIVE STRENGTH OF GEOPOLYMER MORTAR
    Xiem Nguyen Thang
    Louda, Petr
    Kroisova, Dora
    Trung Nguyen Duc
    Thien Nguyen
    CHEMICKE LISTY, 2012, 106 : S557 - S559
  • [37] Investigation of early compressive strength of fly ash-based geopolymer concrete
    Assi, Lateef N.
    Deaver, Edward
    ElBatanouny, Mohamed K.
    Ziehld, Paul
    CONSTRUCTION AND BUILDING MATERIALS, 2016, 112 : 807 - 815
  • [38] Influence of slag as additive on compressive strength of fly ash-based geopolymer
    Li, Zongjin
    Liu, Sifeng
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2007, 19 (06) : 470 - 474
  • [39] Compressive Strength and Microstructural Properties of Fly Ash-Based Geopolymer Concrete
    Nagalia, Gaurav
    Park, Yeonho
    Abolmaali, Ali
    Aswath, Pranesh
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2016, 28 (12)
  • [40] The Synergetic Compressive Strength and Microstructure of Fly Ash and Metakaolin Blend Geopolymer Pastes
    Zulkifly, K.
    Heah, C. Y.
    Liew, Y. M.
    Abdullah, M. M. A. B.
    Abdullah, S. F. A.
    4TH ELECTRONIC AND GREEN MATERIALS INTERNATIONAL CONFERENCE 2018 (EGM 2018), 2018, 2045