ATMOSPHERE CONTROL DURING DEBINDING OF POWDER INJECTION-MOLDED PARTS

被引:5
|
作者
MOORE, JA
JARDING, BP
LOGRASSO, BK
ANDERSON, IE
机构
[1] Ames Laboratory, Metallurgy and Ceramics Div., Iowa State University, Ames, Iowa
关键词
DEBINDING; SINTERING; INJECTION MOLDING;
D O I
10.1007/BF02649064
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Atmosphere control during debinding of powder injection molded (PIM) parts is an important parameter to consider. Experimental results have shown that a stagnant atmosphere containing volatiles evolved during debinding can cause slumping of the green samples. Removal of volatiles from the sample zone aids debinding and can reduce cycle times and improve sample quality. Residual carbon and oxygen can be controlled during debinding by adjusting the atmosphere composition. This paper presents the results of PIM 70 vol% spherical copper powder and 30 vol% binder. Debinding atmospheres were altered to determine the effect of debinding on the green body and the sintered sample.
引用
收藏
页码:275 / 282
页数:8
相关论文
共 50 条
  • [21] Weldlines in injection-molded parts: a review
    Fellahi, S.
    Meddad, A.
    Fisa, B.
    Favis, B.D.
    Advances in Polymer Technology, 1600, 14 (03): : 169 - 195
  • [22] WELDLINES IN INJECTION-MOLDED PARTS - A REVIEW
    FELLAHI, S
    MEDDAD, A
    FISA, B
    FAVIS, BD
    ADVANCES IN POLYMER TECHNOLOGY, 1995, 14 (03) : 169 - 195
  • [23] Debugging of molds for injection-molded parts
    Hu, H.Q.
    Li, W.
    Liu, G.Y.
    Zhongguo Suliao/China Plastics, 2001, 15 (02):
  • [24] Research on thermal debinding of powder injection moulded SiC parts in air atmosphere
    Lu, Z.
    Zhang, K.
    Wang, C.
    MATERIALS RESEARCH INNOVATIONS, 2011, 15 : S263 - S265
  • [25] EXTRACTION DEBINDING OF INJECTION MOLDED PARTS BY CONDENSED SOLVENT
    LIN, ST
    GERMAN, RM
    POWDER METALLURGY INTERNATIONAL, 1989, 21 (05): : 19 - 24
  • [26] Wick debinding distortion of injection molded powder compacts
    Zhang, Haorong
    German, Randall M.
    Bose, Animesh
    International Journal of Powder Metallurgy (Princeton, New Jersey), 1990, 26 (03):
  • [27] Behavior of debinding and sintering in micron and submicron-sized copper powder injection molded parts
    Nishiyabu, Kazuaki
    Tanabe, Daiki
    Kanoko, Yasuhiro
    Tanaka, Shigeo
    1600, Japan Society of Mechanical Engineers (79): : 1593 - 1603
  • [28] MORE REALISTIC TESTING OF INJECTION-MOLDED PARTS
    HALL, WJ
    PLASTICS ENGINEERING, 1986, 42 (01) : 43 - 45
  • [29] Numerical simulation of warpage of injection-molded parts
    Guo, Zhiying
    Ruan, Xueyu
    Li, Dequn
    Zhongguo Jixie Gongcheng/China Mechanical Engineering, 2002, 13 (17):
  • [30] Shrinkage and warpage analysis of injection-molded parts
    Wang, TJ
    Yoon, CK
    ANTEC 2000: SOCIETY OF PLASTICS ENGINEERS TECHNICAL PAPERS, CONFERENCE PROCEEDINGS, VOLS I-III, 2000, : 687 - 692