HYDROGEN EMBRITTLEMENT IN PRE-DEFORMED NI3AL ALLOY

被引:3
|
作者
LI, HX
CHAKI, TK
机构
[1] Department of Mechanical Aerospace Engineering, State University of New York, Buffalo
基金
美国国家科学基金会;
关键词
HYDROGEN; BRITTLENESS; DEFORMATION; NICKEL; ALUMINUM; ALLOYS;
D O I
10.1016/0921-5093(94)03238-6
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Hydrogen embrittlement has been investigated in continuous cast sheet of a Ni3Al alloy (Ni77.82Al21.73Zr0.34B(0.1)) after imparting various amounts of pre-deformation. The specimens (25.4 mm long, 4.4 mm wide and 1 mm thick) were deformed in tension and then taken out of the testing rig for charging hydrogen cathodically for 120 min with a current density of 50 mA cm(-2). Upon testing again in tension, the specimens charged with hydrogen always failed after yielding, which occurred at the final pre-deformation stress. For instance, a specimen pre-deformed to 26% elongation and subsequently charged for 120 min failed (during tensile-testing at the strain rate of 5.8 x 10(-5) s(-1)) at a true stress of 1611 MPa, which is comparable to the true fracture stress (1753 MPa) of the uncharged specimen. However, the elongation at which the charged specimens failed decreased drastically from 5.4% to 1.3%, as the predeformation increased from zero to 2.0%. The fracture surface of the charged specimen consisted of regions of intergranular, quasi-cleavage and dimple fracture. The proportion of intergranular fracture decreased with the increasing pre-deformation, while that of dimple fracture increased. Our results suggest that grain boundaries in B-doped Ni3Al were not weakened by hydrogen, rather ductility-related voids and cracks were involved in hydrogen embrittlement of B-doped Ni3Al alloy.
引用
收藏
页码:387 / 393
页数:7
相关论文
共 50 条
  • [41] STUDY OF SLIDE CRYSTALLOGRAPHY IN NI3AL ALLOY
    POPOV, LE
    TERESHKO, IV
    KONEVA, NA
    KOZLOV, EV
    KORCHAGIN, MA
    IZVESTIYA VYSSHIKH UCHEBNYKH ZAVEDENII FIZIKA, 1971, (07): : 42 - +
  • [42] Oxidation behavior of a Ni3Al PM alloy
    P. Pérez
    J. L. González-Carrasco
    P. Adeva
    Oxidation of Metals, 1997, 48 : 143 - 170
  • [43] WELDING BEHAVIOR AND MICROSTRUCTURE OF A NI3AL ALLOY
    SANTELLA, ML
    HORTON, JA
    DAVID, SA
    WELDING JOURNAL, 1988, 67 (03) : S63 - S69
  • [44] SUPERPLASTICITY IN BORON DOPED NI3AL ALLOY
    MUKHOPADHYAY, J
    KASCHNER, G
    MUKHERJEE, AK
    SCRIPTA METALLURGICA ET MATERIALIA, 1990, 24 (05): : 857 - 862
  • [45] Phonon spectrum of alloy Ni3Al with impurities
    Kosevich, AM
    Feodosyev, SB
    Gospodarev, IA
    Grishaev, VI
    Syrkin, ES
    Grishaev, AV
    METALLOFIZIKA I NOVEISHIE TEKHNOLOGII, 1999, 21 (11): : 55 - 59
  • [46] Oxidation behavior of a Ni3Al PM alloy
    Perez, P
    GonzalezCarrasco, JL
    Adeva, P
    OXIDATION OF METALS, 1997, 48 (1-2): : 143 - 170
  • [47] The calculation of positron lifetime in Ni3Al alloy
    Chen Xiang-Lei
    Guo Wei-feng
    Du Huai-Jiang
    Weng Hui-Min
    Ye Bang-Jiao
    POSITRON AND POSITRONIUM CHEMISTRY, 2009, 607 : 146 - 148
  • [48] MORPHOLOGICAL STABILITY OF DISLOCATION LOOPS IN CYCLICALLY DEFORMED NI3AL
    KALLINGAL, CG
    SMITH, TR
    STOLOFF, NS
    RAJAN, K
    SCRIPTA METALLURGICA ET MATERIALIA, 1992, 27 (10): : 1407 - 1412
  • [49] The effect of Ce and pre-deformed process on aging transformation for Al-Li-Cu-Zr alloy
    Jia, LS
    Wei, YH
    Hu, LQ
    Xu, BS
    RARE METAL MATERIALS AND ENGINEERING, 2002, 31 (02) : 156 - 159
  • [50] The Effect of Ce and Pre-deformed Process on Aging Transformation for Al-Li-Cu-Zr Alloy
    Jia, Liansuo
    Wei, Yinghui
    Hu, Lanqing
    Xu, Bingshe
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2002, 31 (02): : 158 - 159