HYDROGEN EMBRITTLEMENT IN PRE-DEFORMED NI3AL ALLOY

被引:3
|
作者
LI, HX
CHAKI, TK
机构
[1] Department of Mechanical Aerospace Engineering, State University of New York, Buffalo
基金
美国国家科学基金会;
关键词
HYDROGEN; BRITTLENESS; DEFORMATION; NICKEL; ALUMINUM; ALLOYS;
D O I
10.1016/0921-5093(94)03238-6
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Hydrogen embrittlement has been investigated in continuous cast sheet of a Ni3Al alloy (Ni77.82Al21.73Zr0.34B(0.1)) after imparting various amounts of pre-deformation. The specimens (25.4 mm long, 4.4 mm wide and 1 mm thick) were deformed in tension and then taken out of the testing rig for charging hydrogen cathodically for 120 min with a current density of 50 mA cm(-2). Upon testing again in tension, the specimens charged with hydrogen always failed after yielding, which occurred at the final pre-deformation stress. For instance, a specimen pre-deformed to 26% elongation and subsequently charged for 120 min failed (during tensile-testing at the strain rate of 5.8 x 10(-5) s(-1)) at a true stress of 1611 MPa, which is comparable to the true fracture stress (1753 MPa) of the uncharged specimen. However, the elongation at which the charged specimens failed decreased drastically from 5.4% to 1.3%, as the predeformation increased from zero to 2.0%. The fracture surface of the charged specimen consisted of regions of intergranular, quasi-cleavage and dimple fracture. The proportion of intergranular fracture decreased with the increasing pre-deformation, while that of dimple fracture increased. Our results suggest that grain boundaries in B-doped Ni3Al were not weakened by hydrogen, rather ductility-related voids and cracks were involved in hydrogen embrittlement of B-doped Ni3Al alloy.
引用
收藏
页码:387 / 393
页数:7
相关论文
共 50 条
  • [21] INTRINSIC STACKING FAULT IN DEFORMED NI3AL
    ENAMI, K
    NENNO, S
    JOURNAL OF THE PHYSICAL SOCIETY OF JAPAN, 1968, 25 (05) : 1517 - &
  • [22] The loss of magnetism in tetragonally deformed Ni3Al
    Legut, D
    Sob, M
    ACTA PHYSICA SLOVACA, 2006, 56 (02) : 149 - 152
  • [23] INTRINSIC DUCTILITY AND ENVIRONMENTAL EMBRITTLEMENT OF BINARY NI3AL
    GEORGE, EP
    LIU, CT
    POPE, DP
    SCRIPTA METALLURGICA ET MATERIALIA, 1993, 28 (07): : 857 - 862
  • [24] Multiple precipitation reactions and formation of θ′-phase in a pre-deformed Al-Cu alloy
    Liu, Chunhui
    Ma, Ziyao
    Ma, Peipei
    Zhan, Lihua
    Huang, Minghui
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 733 : 28 - 38
  • [25] The influence of thermal cycling on electrical properties of pre-deformed Ti-49.8% Ni alloy
    Babicheva, R. I.
    Mulyukov, Kh. Ya.
    LETTERS ON MATERIALS-PIS MA O MATERIALAKH, 2011, 1 (01): : 55 - 58
  • [26] STRUCTURAL ALLOY BASED ON NI3AL
    PORTNOI, KI
    BUNTUSHKIN, VP
    MELIMEVKER, OD
    METAL SCIENCE AND HEAT TREATMENT, 1981, 23 (5-6) : 396 - 399
  • [27] Hf dopants in γ′-Ni3Al alloy
    Ivanovski, V. N.
    Cekic, B.
    Umicevic, A.
    Belosevic-Cavor, J.
    Schumacher, G.
    Koteski, V.
    Barudzija, T.
    JOURNAL OF APPLIED PHYSICS, 2013, 114 (06)
  • [28] Twofold ordering in Ni3Al alloy
    Filus, F
    Hyspecka, L
    Fiala, J
    KOVOVE MATERIALY-METALLIC MATERIALS, 1997, 35 (04): : 285 - 290
  • [29] STRAIN HARDENING OF ALLOY NI3AL
    POPOV, LY
    KOZLOV, EV
    TERESHKO, IV
    PHYSICS OF METALS AND METALLOGRAPHY-USSR, 1968, 26 (04): : 129 - &
  • [30] ALLOY SOFTENING IN NI3AL POLYCRYSTALS
    QIAN, XR
    CHOU, YT
    JOURNAL OF MATERIALS SCIENCE, 1992, 27 (04) : 1036 - 1044