HYDROGEN EMBRITTLEMENT IN PRE-DEFORMED NI3AL ALLOY

被引:3
|
作者
LI, HX
CHAKI, TK
机构
[1] Department of Mechanical Aerospace Engineering, State University of New York, Buffalo
基金
美国国家科学基金会;
关键词
HYDROGEN; BRITTLENESS; DEFORMATION; NICKEL; ALUMINUM; ALLOYS;
D O I
10.1016/0921-5093(94)03238-6
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Hydrogen embrittlement has been investigated in continuous cast sheet of a Ni3Al alloy (Ni77.82Al21.73Zr0.34B(0.1)) after imparting various amounts of pre-deformation. The specimens (25.4 mm long, 4.4 mm wide and 1 mm thick) were deformed in tension and then taken out of the testing rig for charging hydrogen cathodically for 120 min with a current density of 50 mA cm(-2). Upon testing again in tension, the specimens charged with hydrogen always failed after yielding, which occurred at the final pre-deformation stress. For instance, a specimen pre-deformed to 26% elongation and subsequently charged for 120 min failed (during tensile-testing at the strain rate of 5.8 x 10(-5) s(-1)) at a true stress of 1611 MPa, which is comparable to the true fracture stress (1753 MPa) of the uncharged specimen. However, the elongation at which the charged specimens failed decreased drastically from 5.4% to 1.3%, as the predeformation increased from zero to 2.0%. The fracture surface of the charged specimen consisted of regions of intergranular, quasi-cleavage and dimple fracture. The proportion of intergranular fracture decreased with the increasing pre-deformation, while that of dimple fracture increased. Our results suggest that grain boundaries in B-doped Ni3Al were not weakened by hydrogen, rather ductility-related voids and cracks were involved in hydrogen embrittlement of B-doped Ni3Al alloy.
引用
收藏
页码:387 / 393
页数:7
相关论文
共 50 条
  • [2] EFFECT OF AN OXIDE DISPERSION ON THE HYDROGEN EMBRITTLEMENT OF A NI3AL BASE ALLOY
    CAMUS, GM
    DUQUETTE, DJ
    STOLOFF, NS
    JOURNAL OF MATERIALS RESEARCH, 1990, 5 (05) : 950 - 954
  • [3] ON THE MECHANISMS OF HYDROGEN EMBRITTLEMENT OF NI3AL ALLOYS
    BOND, GM
    ROBERTSON, IM
    BIRNBAUM, HK
    ACTA METALLURGICA, 1989, 37 (05): : 1407 - 1413
  • [4] A study on the creep cavitation in an Ni3Al alloy using the hydrogen embrittlement technique
    Kim, HK
    Kim, SH
    Hyun, CY
    PRAKTISCHE METALLOGRAPHIE-PRACTICAL METALLOGRAPHY, 2005, 42 (11): : 533 - 545
  • [5] The effects of boron and hydrogen on the embrittlement of polycrystalline Ni3AL
    Wang, FH
    Shang, JX
    Li, JM
    Wang, CY
    INTERMETALLICS, 2000, 8 (5-6) : 589 - 593
  • [6] HYDROGEN EMBRITTLEMENT OF Ni3Al plus B.
    Kuruvilla, A.K.
    Stoloff, N.S.
    1986, : 711 - 715
  • [7] Effect of recrystallization on environmental embrittlement of a Ni3Al(Zr) alloy
    Li, YF
    Guo, GT
    Zhou, LZ
    Ye, HQ
    ACTA METALLURGICA SINICA, 2004, 40 (05) : 499 - 503
  • [8] Environmental embrittlement of Ni3Al(Zr) alloy at high temperatures
    College of Material Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016, China
    不详
    Nanjing Hangkong Hangtian Daxue Xuebao, 2008, 3 (380-384):
  • [9] Mechanism of boron-induced embrittlement of Ni3Al in hydrogen
    Painter, GS
    SCRIPTA MATERIALIA, 1997, 37 (07) : 1023 - 1029
  • [10] Shape memory behavior of a Ni3Ta alloy pre-deformed in compression
    Rudajevova, A.
    Pospisil, J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (12): : 2900 - 2905