NEUTRON DAMAGE OF CHEMICAL-VAPOR-DEPOSITION DIAMOND

被引:23
|
作者
MAINWOOD, A
ALLERS, L
COLLINS, AT
HASSARD, JF
HOWARD, AS
MAHON, AR
PARSONS, HL
SUMNER, T
COLLINS, JL
SCARSBROOK, GA
SUSSMANN, RS
WHITEHEAD, AJ
机构
[1] UNIV LONDON IMPERIAL COLL SCI TECHNOL & MED,BLACKETT LAB,DEPT PHYS,LONDON SW7 2BZ,ENGLAND
[2] DE BEERS IND DIAMOND DIV UK LTD,ASCOT SL5 9PX,BERKS,ENGLAND
关键词
D O I
10.1088/0022-3727/28/6/035
中图分类号
O59 [应用物理学];
学科分类号
摘要
Many of the components of particle detectors for the next generation of high energy experiments need to be extremely radiation-hard ii they are to continue to function for more than a few months. For example, in the first few year's operation of the large hadron collider, we expect about 10(13) neutrons cm(-2) year(-1) 1 cm from the beam pipe, with other particles causing about ten times as much additional damage. Diamond is being considered as both a detector material and perhaps as a structural component. We report on tests of chemical vapour deposition diamond films irradiated by 6 x 10(14) neutrons cm(-2) of energy below 10 keV, plus (2.0 +/- 0.5) x 10(14) neutrons cm(-2) of energy above 10 keV peaking at about 1 MeV. The diamonds were metallized with titanium-gold contacts-strips on the front and a continuous electrode on the back. The leakage current (already extremely small) decreased by factors of about 50 as a result of the irradiation, both measured between adjacent strips and through the thickness of the samples. The detection efficiency of charged particles improved by 30-40% after irradiation. In addition, natural diamonds irradiated by 4 x 10(14) neutrons cm(-2) showed very little optical absorption in the GR1 and ND1 bands (neutral and negative vacancy) corresponding to a concentration of vacancies of 4(+/-2) x 10(14) cm(-3).
引用
收藏
页码:1279 / 1283
页数:5
相关论文
共 50 条
  • [31] Simulation of band diagram for chemical-vapor-deposition diamond surface conductivity
    Kono, S
    Koide, Y
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2005, 44 (12): : 8378 - 8382
  • [32] FORMATION OF DIAMOND FILMS BY INTERMITTENT DISCHARGE PLASMA CHEMICAL-VAPOR-DEPOSITION
    NODA, M
    KUSAKABE, H
    TANIGUCHI, K
    MARUNO, S
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1994, 33 (7B): : 4400 - 4403
  • [33] FABRICATION OF DIAMOND TIPS BY THE MICROWAVE PLASMA CHEMICAL-VAPOR-DEPOSITION TECHNIQUE
    LIU, N
    MA, Z
    CHU, X
    HU, T
    XUE, Z
    JIANG, X
    PANG, S
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 1994, 12 (03): : 1712 - 1715
  • [34] CHEMICAL-VAPOR-DEPOSITION OF SILVER
    YUAN, Z
    DRYDEN, NH
    VITTAL, JJ
    PUDDEPHATT, RJ
    CHEMISTRY OF MATERIALS, 1995, 7 (09) : 1696 - 1702
  • [35] EXTENSIVE DIAMOND FILM DEPOSITION BY DC PLASMA-JET CHEMICAL-VAPOR-DEPOSITION
    LUGSCHEIDER, E
    SCHLUMP, W
    DEUERLER, F
    REMER, P
    DIAMOND AND RELATED MATERIALS, 1994, 3 (4-6) : 325 - 327
  • [36] PROGRESS IN CHEMICAL-VAPOR-DEPOSITION
    CARLSSON, JO
    JANSSON, U
    PROGRESS IN SOLID STATE CHEMISTRY, 1993, 22 (04) : 237 - 292
  • [37] DIAMOND DEPOSITION ON CHROMIUM, COBALT AND NICKEL SUBSTRATES BY MICROWAVE PLASMA CHEMICAL-VAPOR-DEPOSITION
    HAUBNER, R
    LINDLBAUER, A
    LUX, B
    DIAMOND AND RELATED MATERIALS, 1993, 2 (12) : 1505 - 1515
  • [38] CHEMICAL-VAPOR-DEPOSITION AND PLASMA-ENHANCED CHEMICAL-VAPOR-DEPOSITION CARBONIZATION OF SILICON MICROTIPS
    ZHIRNOV, VV
    GIVARGIZOV, EI
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 1994, 12 (02): : 633 - 637
  • [39] EFFECT OF THE CHEMICAL NATURE OF TRANSITION-METAL SUBSTRATES ON CHEMICAL-VAPOR-DEPOSITION OF DIAMOND
    CHEN, X
    NARAYAN, J
    JOURNAL OF APPLIED PHYSICS, 1993, 74 (06) : 4168 - 4173
  • [40] SCALING LAWS FOR DIAMOND CHEMICAL-VAPOR-DEPOSITION .1. DIAMOND SURFACE-CHEMISTRY
    GOODWIN, DG
    JOURNAL OF APPLIED PHYSICS, 1993, 74 (11) : 6888 - 6894