共 50 条
- [42] Estimated and evaluated residual stress by Vickers indentation in several structural ceramics MATERIALS SCIENCE RESEARCH INTERNATIONAL, 2003, 9 (01): : 75 - 80
- [45] Successful 3-dimensional laser welding of ceramics LASER MATERIALS PROCESSING CONFERENCE, PTS 1 & 2: ICALEO '97, 1997, : A11 - A20
- [46] Estimation of Fracture Toughness for ε Zirconium Hydride by Vickers Microhardness Indentation Method JOM, 2021, 73 : 3468 - 3475
- [49] Measurement of fracture toughness in AISI 1018 borided steels by vickers indentation Diffus Defect Data Pt A Diffus Forum, 2008, (675-680): : 675 - 680
- [50] Measurement of Fracture Toughness in AISI 1018 Borided Steels by Vickers Indentation DIFFUSION IN SOLIDS AND LIQUIDS IV, 2009, 283-286 : 675 - +