OXYGEN INCORPORATION AND PRECIPITATION BEHAVIOR IN HEAVILY BORON-DOPED CZOCHRALSKI SILICON-CRYSTALS

被引:15
|
作者
CHOE, KS
机构
[1] Department of Electronic Materials Engineering, University of Suwon, Suwon, Kyoungki-Do 445-743
关键词
D O I
10.1016/0022-0248(94)00633-4
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
To understand the effect of heavy boron-doping, p(+)-type (100) silicon crystals doped with boron in the order of 1X10(19) atoms cm(-3) (0.006-0.01 Omega cm) and a p-type (100) silicon crystal doped with boron in the order of 1 X 10(15) atoms cm(-3) (12-16 Omega cm) were grown in a Czochralski puller and studied. The oxygen contents in the p(+)-type crystals were determined by gas fusion analysis and shown to be on the average about 23% higher than those in a comparable p-type crystal. Etch pit features of oxide precipitates after a high-low-high annealing were generally different between the two types of silicon, and three distinct regimes of behavior about the critical boron and oxygen concentrations were identified. Those are: with resistivity greater than or similar to 0.007 Omega cm or oxygen concentration less than or similar to 30 ppma (Old ASTM), the oxide precipitate density, in the order of 10(10) cm(-3), is basically unaffected by heavy boron-doping and dependent on oxygen concentration; with resistivity less than or similar to 0.007 Omega cm and oxygen concentration greater than or similar to 37 ppma, however, large platelets, which are 10-15 mu m in size and in the order of 10(7) cm(-3) in density, are formed instead and completely gettered oxide precipitates. In a medium-oxygen range of about 28-30 ppma, both p- and p(+)-type (100) silicon wafers formed an ideal internal gettering structure, consisting of a well-defined precipitate-free zone (PFZ) to a depth of about 15 mu m from the surface and dense bulk oxide precipitates in the order of 10(10) cm(-3) below the PFZ, after a high-low-high annealing.
引用
收藏
页码:55 / 63
页数:9
相关论文
共 50 条
  • [31] Precipitation of boron in highly boron-doped silicon
    Mizushima, I
    Mitani, Y
    Koike, M
    Yoshiki, M
    Tomita, M
    Kambayashi, S
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1998, 37 (3B): : 1171 - 1173
  • [32] INFRARED-ABSORPTION STUDY ON CARBON AND OXYGEN BEHAVIOR IN CZOCHRALSKI SILICON-CRYSTALS
    SHIMURA, F
    BAIARDO, JP
    FRAUNDORF, P
    APPLIED PHYSICS LETTERS, 1985, 46 (10) : 941 - 943
  • [33] Diffusion of gold into heavily boron-doped silicon
    Bracht, H
    Schachtrup, AR
    DEFECTS AND DIFFUSION IN SILICON PROCESSING, 1997, 469 : 25 - 36
  • [34] Activation and deactivation in heavily boron-doped silicon
    Yoo, SH
    Ro, JS
    JOURNAL OF THE KOREAN PHYSICAL SOCIETY, 2003, 43 (02) : 290 - 295
  • [35] Rapid-thermal-processing-based internal gettering for heavily boron-doped Czochralski silicon
    Fu, Liming
    Yang, Deren
    Ma, Xiangyang
    Tian, Daxi
    Que, Duanlin
    Journal of Applied Physics, 2006, 100 (10):
  • [36] Superconductivity in heavily boron-doped silicon carbide
    Kriener, Markus
    Muranaka, Takahiro
    Kato, Junya
    Ren, Zhi-An
    Akimitsu, Jun
    Maeno, Yoshiteru
    SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS, 2008, 9 (04)
  • [37] Rapid-thermal-processing-based internal gettering for heavily boron-doped Czochralski silicon
    Fu, Liming
    Yang, Deren
    Ma, Xiangyang
    Tian, Daxi
    Que, Duanlin
    JOURNAL OF APPLIED PHYSICS, 2006, 100 (10)
  • [38] DISLOCATION BEHAVIOR AND MECHANICAL STRENGTHS OF FLOAT-ZONE SILICON-CRYSTALS AND CZOCHRALSKI SILICON-CRYSTALS
    SUMINO, K
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1981, 128 (03) : C93 - C93
  • [39] Boron deactivation in heavily boron-doped Czochralski silicon during rapid thermal anneal: Atomic level understanding
    Gao, Chao
    Lu, Yunhao
    Dong, Peng
    Yi, Jun
    Ma, Xiangyang
    Yang, Deren
    APPLIED PHYSICS LETTERS, 2014, 104 (03)
  • [40] PARAMETERS AFFECTING OXYGEN INCORPORATION AT THE SEED-END OF CZOCHRALSKI-GROWN SILICON-CRYSTALS
    MURGAI, A
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1980, 127 (08) : C396 - C396