摘要
Biomedical implants are useful to replace missing organ of a diseased person. Stainless steel (SS) of 316L grade is commonly used as resource material to make implants. Once fixed in the human body, implants undergo some changes including corrosion. Corroded implant may induce inflammation leading to implant rejection by the body. It is important to prevent the corrosion of implant to increase chances of acceptance in body. The objective of this study was to evaluate the corrosion inhibition properties of Ficus benghalensis synthesized Iron oxide nanoparticles (IONPs) in Ringer’s solution for SS-316L. The synthesized green NPs were spherical in shape, 30–50 nm in size and have − 12 mV surface charge. Further, the IONPs have a tendency to agglomerate. Gravimetric test and electrochemical tests were carried out to estimate the corrosion inhibition efficiency. The adsorption of IONPs over SS-316L surface followed Langmuir adsorption isotherm. Maximum 82.20% potentiodynamic polarization corrosion inhibition efficiency (IE) was obtained using 100 ppm of IONPs. The electrochemical study showed mixed type of corrosion inhibition (anodic and cathodic). The corrosion inhibition efficiency was found to increase with increase in the concentration of IONPs in the Ringer’s solution. Thus, IONPs can be explored as efficient corrosion inhibitor for SS-316L in an aggressive environment. © 2022, The Author(s), under exclusive licence to Springer Nature Switzerland AG.
引用
收藏
相关论文
共 50 条
  • [31] Crystallographic effects in corrosion of austenitic stainless steel 316L
    Lindell, D.
    Pettersson, R.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2015, 66 (08): : 727 - 732
  • [32] Corrosion Resistance of Welds in Type 316L Stainless Steel
    Esmailian, Mohammad
    MATERIALS PERFORMANCE, 2017, 56 (03) : 58 - 61
  • [33] Corrosion performance of the plasma nitrided 316L stainless steel
    Gil, Linda
    Bruhl, Sonia
    Jimenez, Lorena
    Leon, Ovidio
    Guevara, Rafael
    Staia, Maniana H.
    SURFACE & COATINGS TECHNOLOGY, 2006, 201 (07): : 4424 - 4429
  • [34] Study of 316L stainless steel corrosion in cvasibiological conditions
    Tutunaru, Bogdan
    Samide, Adriana Patru
    Preda, Mircea
    REVISTA DE CHIMIE, 2007, 58 (10): : 923 - 926
  • [35] Effects of formulation components on the corrosion of 316L stainless steel
    Lam, P
    Keck, R
    Lo, S
    Wong, R
    Hsu, C
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2003, 225 : U184 - U184
  • [36] Effect of Ringer's Solution on Wear and Friction of Stainless Steel 316L after Plasma Electrolytic Nitrocarburising at Low Voltages
    N.Afsar Kazerooni
    M.E.Bahrololoom
    M.H.Shariat
    F.Mahzoon
    T.Jozaghi
    JournalofMaterialsScience&Technology, 2011, 27 (10) : 906 - 912
  • [37] Effect of Ringer's Solution on Wear and Friction of Stainless Steel 316L after Plasma Electrolytic Nitrocarburising at Low Voltages
    Kazerooni, N. Afsar
    Bahrololoom, M. E.
    Shariat, M. H.
    Mahzoon, F.
    Jozaghi, T.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2011, 27 (10) : 906 - 912
  • [38] Corrosion Resistance and Hemocompatibility of Passivated 316L Stainless Steel
    Wang J.
    Liu Y.
    Liu, Ying (lying@ncu.edu.cn), 2018, Shanghai Jiaotong University (52): : 593 - 598
  • [39] Corrosion behavior of nitrogen stainless steel in Ringer's solution
    Ilieva, G. P.
    Loukaycheva, M. H.
    Tzaneva, B. R.
    Gekova, L. T.
    Fachikov, L. B.
    BULGARIAN CHEMICAL COMMUNICATIONS, 2016, 48 : 66 - 72
  • [40] Formation of chromium oxide on 316L austenitic stainless steel
    Ohmi, T
    Nakagawa, Y
    Nakamura, M
    Ohki, A
    Koyama, T
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1996, 14 (04): : 2505 - 2510