摘要
Non modified and Ag-modified eutectic Sn-0.7Cu solder alloys were directionally solidified under transient heat flow conditions. The microstructure of the Sn-0.7Cu alloy has been characterized and the present experimental results include the cell/primary dendrite arm spacing (λ1) and its correlation with: the tip cooling rate (T∙\documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$$\mathop T\limits^{ \bullet }$$\end{document}) during solidification, ultimate tensile strength (σu) and elongation to fracture (δ). Distinct morphologies of intermetallic compounds have been associated with the solidification cooling rate for both alloys examined. For the Sn-0.7Cu alloy, cellular regions were observed to occur for cooling rates lower than 0.9 K/s, being characterized by aligned eutectic colonies. On the other hand, the alloy containing 2.0 wt %Ag enabled the launch of tertiary branches within the dendritic arrangement. The comparison of results allows stating that finer solder microstructures are shown to be associated with higher ultimate tensile strengths (σu) for both alloys although a more complex microstructure was found for the SAC alloy. In contrast the elongation (δ) exhibited opposite tendencies. The growth of coarse Ag3Sn fibers and platelets within interdendritic regions seems to contribute for the reduction on ductility observed for the SAC alloy.
引用
收藏
页码:478 / 486
页数:8
相关论文
共 50 条
  • [41] Interfacial reaction and mechanical reliability of eutectic Sn-0.7Cu/immersion Ag-plated Cu solder joint
    Yoon, J-W.
    Jung, S-B.
    MATERIALS SCIENCE AND TECHNOLOGY, 2009, 25 (12) : 1478 - 1484
  • [42] In Situ TEM Observations of Cu6Sn5 Polymorphic Transformations in Reaction Layers Between Sn-0.7Cu Solders and Cu Substrates
    Nogita, K.
    Salleh, M. A. A. Mohd
    Tanaka, E.
    Zeng, G.
    Mcdonald, S. D.
    Matsumura, S.
    JOM, 2016, 68 (11) : 2871 - 2878
  • [43] Modeling and Experimental Verification of Intermetallic Compounds Grown by Electromigration and Thermomigration for Sn-0.7Cu Solders
    Sung-Min Baek
    Yujin Park
    Cheolmin Oh
    Eun-Joon Chun
    Namhyun Kang
    Journal of Electronic Materials, 2019, 48 : 142 - 151
  • [44] In Situ TEM Observations of Cu6Sn5 Polymorphic Transformations in Reaction Layers Between Sn-0.7Cu Solders and Cu Substrates
    K. Nogita
    M. A. A. Mohd Salleh
    E. Tanaka
    G. Zeng
    S. D. McDonald
    S. Matsumura
    JOM, 2016, 68 : 2871 - 2878
  • [45] Effect of Ni-MOF Derivatives on the Electrochemical Corrosion Behavior of Sn-0.7Cu Solders
    Lu, Guoge
    Lin, Bo
    Gao, Zhan
    Li, Yingxin
    Wei, Fuxiang
    METALS, 2022, 12 (07)
  • [46] Modeling and Experimental Verification of Intermetallic Compounds Grown by Electromigration and Thermomigration for Sn-0.7Cu Solders
    Baek, Sung-Min
    Park, Yujin
    Oh, Cheolmin
    Chun, Eun-Joon
    Kang, Namhyun
    JOURNAL OF ELECTRONIC MATERIALS, 2019, 48 (01) : 142 - 151
  • [47] Effects of Cu, Bi, and In on microstructure and tensile properties of Sn-Ag-X(Cu, Bi, In) solders
    Huang, ML
    Wang, L
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2005, 36A (06): : 1439 - 1446
  • [48] Effects of Cu, Bi, and In on microstructure and tensile properties of Sn-Ag-X(Cu, Bi, In) solders
    M. L. Huang
    L. Wang
    Metallurgical and Materials Transactions A, 2005, 36 : 1439 - 1446
  • [49] Nanocomposite SAC solders: morphology, electrical and mechanical properties of Sn-3.8Ag-0.7Cu solders by adding Co nanoparticles
    Yakymovych, A.
    Plevachuk, Yu.
    Svec, P., Sr.
    Janickovic, D.
    Sebo, P.
    Beronska, N.
    Nosko, M.
    Orovcik, L.
    Roshanghias, A.
    Ipser, H.
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2017, 28 (15) : 10965 - 10973
  • [50] Mechanical shock behavior of Sn-3.9Ag-0.7Cu and Sn-3.9Ag-0.7Cu-0.5Ce solder joints
    Xie, H. X.
    Chawla, N.
    MICROELECTRONICS RELIABILITY, 2013, 53 (05) : 733 - 740