Development of solidification microstructure and tensile mechanical properties of Sn-0.7Cu and Sn-0.7Cu-2.0Ag solders

被引:0
|
作者
José Eduardo Spinelli
Amauri Garcia
机构
[1] Federal University of São Carlos,Department of Materials Engineering
[2] University of Campinas,Department of Materials Engineering
关键词
Solder Alloy; Dendritic Spacing; Primary Dendritic Spacing; Large Ag3Sn; Casting Length;
D O I
暂无
中图分类号
学科分类号
摘要
Non modified and Ag-modified eutectic Sn-0.7Cu solder alloys were directionally solidified under transient heat flow conditions. The microstructure of the Sn-0.7Cu alloy has been characterized and the present experimental results include the cell/primary dendrite arm spacing (λ1) and its correlation with: the tip cooling rate (T∙\documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$$\mathop T\limits^{ \bullet }$$\end{document}) during solidification, ultimate tensile strength (σu) and elongation to fracture (δ). Distinct morphologies of intermetallic compounds have been associated with the solidification cooling rate for both alloys examined. For the Sn-0.7Cu alloy, cellular regions were observed to occur for cooling rates lower than 0.9 K/s, being characterized by aligned eutectic colonies. On the other hand, the alloy containing 2.0 wt %Ag enabled the launch of tertiary branches within the dendritic arrangement. The comparison of results allows stating that finer solder microstructures are shown to be associated with higher ultimate tensile strengths (σu) for both alloys although a more complex microstructure was found for the SAC alloy. In contrast the elongation (δ) exhibited opposite tendencies. The growth of coarse Ag3Sn fibers and platelets within interdendritic regions seems to contribute for the reduction on ductility observed for the SAC alloy.
引用
收藏
页码:478 / 486
页数:8
相关论文
共 50 条
  • [32] Comparison of spreading behaviour and interfacial microstructure in Sn-0.7Cu, Sn-0.3Ag-0.7Cu and Sn-2.5Ag-0.5Cu lead free solder alloys on Fe-42Ni substrate
    Narayan, S.
    Prabhu, K. N.
    MATERIALS SCIENCE AND TECHNOLOGY, 2013, 29 (04) : 464 - 473
  • [33] Effect of Type of Reinforcement at Nanolength Scale on the Tensile Properties of Sn-0.7Cu Solder Alloy
    Zhong, X. L.
    Gupta, M.
    EPTC: 2008 10TH ELECTRONICS PACKAGING TECHNOLOGY CONFERENCE, VOLS 1-3, 2008, : 669 - 674
  • [34] Microstructure and mechanical properties of Sn-0.7Cu flip chip solder bumps using stencil printing method
    Kim, DG
    Jung, SB
    MATERIALS TRANSACTIONS, 2005, 46 (11) : 2366 - 2371
  • [35] Influence of Cu Nanoparticles on Microstructure and Mechanical Properties of Sn0.7Ag0.5Cu-BiNi/Cu Solder Joint
    G. F. Ban
    F. L. Sun
    J. J. Fan
    Y. Liu
    S. N. Cong
    Journal of Materials Engineering and Performance, 2017, 26 : 1069 - 1075
  • [36] Influence of Cu Nanoparticles on Microstructure and Mechanical Properties of Sn0.7Ag0.5Cu-BiNi/Cu Solder Joint
    Ban, G. F.
    Sun, F. L.
    Fan, J. J.
    Liu, Y.
    Cong, S. N.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (03) : 1069 - 1075
  • [37] The Effect of Copper Addition on the Properties of Sn-0.7Cu Solder Paste
    Said, R. M.
    Johari, F. H. Mohamad
    Salleh, M. A. A. Mohd
    Sandu, A. V.
    MALAYSIAN TECHNICAL UNIVERSITIES CONFERENCE ON ENGINEERING AND TECHNOLOGY 2017 (MUCET 2017), 2018, 318
  • [39] Effects of nano-sized Ag reinforcing particulates on the microstructure of Sn-0.7Cu solder joints
    Tai, Feng
    Guo, Fu
    Xia, Zhi-dong
    Lei, Yong-ping
    Shi, Yao-wu
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2009, 16 (06) : 677 - 684
  • [40] A rheological assessment of the effect of trace level Ni additions on the solidification of Sn-0.7Cu
    Gourlay, CM
    Nogita, K
    McDonald, SD
    Nishimura, T
    Sweatman, K
    Dahle, AK
    SCRIPTA MATERIALIA, 2006, 54 (09) : 1557 - 1562