Oxidation of alloys of the system Ni−Ta. I. Oxidation of the intermetallic Ni3Ta

被引:0
|
作者
V. G. Chuprina
机构
来源
Powder Metallurgy and Metal Ceramics | 1999年 / 38卷
关键词
Tantalum; Oxidation Kinetic; Scale Surface; Oxidation Rate Constant; Scale Boundary;
D O I
暂无
中图分类号
学科分类号
摘要
Oxidation kinetics for the intermetallic Ni3Ta in air at 600–1000°C are studied by a thermogravimetric method. The alloy has an ordered crystal structure (D132h-Pmmn) with rhombic lattice parameters a=0.512 nm, b=0.423 nm, and c=0.452 nm. The kinetic isotherms of Ni3Ta oxidation are described by a parabolic equation. With t≤800°C there is a periodic increase in the rate constant of parabolic oxidation, but with t>800°C there is a periodic decrease of it. In the range 850–875°C the alloy oxidation rate decreases as a result of scale sintering. Oxygen diffusion slows down in the compact scale. X-ray and metallographic analysis of the scale that forms on Ni3Ta indicates that it contains NiO, NiO·Ta2O5, Ta2O5 and also Ni and the solid solution Ni(Ta). These phase components are distributed in layers of the scale: NiO (first), NiO+NiO·Ta2O5 (second), NiO·Ta2O5+Ni+Ta2O5 (third), Ta2O5+Ni(Ta) (fourth). With a low temperature and short periods of heating there is no Nio·Ta2O5 or Ni(Ta) in the scale. Oxidation of Ni3Ta is controlled by oxygen diffusion in the scale over the direction towards the alloy. With t>850°C this mechanism changes. By analogy with oxidation of tantalum it is assumed that structural changes in the Ta2O5 lattice may be responsible for this.
引用
收藏
页码:179 / 185
页数:6
相关论文
共 50 条
  • [41] Nitrogen Solubility in Liquid Ni-V, Ni-Ta, Ni-Cr-V, and Ni-Cr-Ta Alloys
    Qian, Kun
    Chen, Bo
    Shu, Lei
    Liu, Kui
    METALS, 2019, 9 (11)
  • [42] INVESTIGATION OF THE PHASE DIAGRAM OF THE TERNARY SYSTEM NI-NI3NB-NI3TA
    KORNILOV, II
    PYLAEVA, EN
    JOURNAL OF INORGANIC CHEMISTRY-USSR, 1956, 1 (02): : 123 - 132
  • [43] KINETICS OF OXIDATION OF TA-TI ALLOYS
    PROKOSHKIN, DA
    VORONOVA, TA
    GORBOVA, AS
    RUSSIAN METALLURGY, 1984, (05): : 186 - 189
  • [44] Aging effect on microstructure and hardness of two-phase Ni3Al-Ni3V intermetallic alloys containing Ta and Re
    Moronaga, Taku
    Ishii, Seiya
    Kaneno, Yasuyuki
    Tsuda, Hiroshi
    Takasugi, Takayuki
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 539 : 30 - 37
  • [45] NITROGEN SOLUBILITY IN LIQUID FE-TA, FE-CR-TA, FE-NI-TA, AND FE-CR-NI-TA ALLOYS
    WADA, H
    PEHLKE, RD
    METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1980, 11 (01): : 51 - 56
  • [46] Effects of Al and Ta on the high temperature oxidation of Ni-based superalloys
    Park, Si-Jun
    Seo, Seong-Moon
    Yoo, Young-Soo
    Jeong, Hi-Won
    Jang, HeeJin
    CORROSION SCIENCE, 2015, 90 : 305 - 312
  • [47] Microstructure, mechanical property and oxidation property in Ni3Si-Ni3Ti-Ni3Nb multi-phase intermetallic alloys
    Ohira, K
    Kaneno, Y
    Takasugi, T
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 399 (1-2): : 332 - 343
  • [48] VYDELENIE TANTALIDA NIKELYA NI3TA IZ SPLAVOV DVOINOI SISTEMY NIKEL-TANTAL
    KORNILOV, II
    PYLAEVA, EN
    DOKLADY AKADEMII NAUK SSSR, 1953, 91 (04): : 841 - 843
  • [49] STUDY OF OXIDATION OF NI3NB INTERMETALLIC COMPOUND
    CHUPRINA, VG
    DOPOVIDI AKADEMII NAUK UKRAINSKOI RSR SERIYA A-FIZIKO-MATEMATICHNI TA TECHNICHNI NAUKI, 1977, (02): : 169 - 172
  • [50] Indentation size effect and strain rate sensitivity of Ni3Ta high temperature shape memory alloy
    Shuitcev, A. V.
    Tong, Y. X.
    Li, L.
    VACUUM, 2019, 160 : 25 - 30