Oxidation of alloys of the system Ni−Ta. I. Oxidation of the intermetallic Ni3Ta

被引:0
|
作者
V. G. Chuprina
机构
来源
Powder Metallurgy and Metal Ceramics | 1999年 / 38卷
关键词
Tantalum; Oxidation Kinetic; Scale Surface; Oxidation Rate Constant; Scale Boundary;
D O I
暂无
中图分类号
学科分类号
摘要
Oxidation kinetics for the intermetallic Ni3Ta in air at 600–1000°C are studied by a thermogravimetric method. The alloy has an ordered crystal structure (D132h-Pmmn) with rhombic lattice parameters a=0.512 nm, b=0.423 nm, and c=0.452 nm. The kinetic isotherms of Ni3Ta oxidation are described by a parabolic equation. With t≤800°C there is a periodic increase in the rate constant of parabolic oxidation, but with t>800°C there is a periodic decrease of it. In the range 850–875°C the alloy oxidation rate decreases as a result of scale sintering. Oxygen diffusion slows down in the compact scale. X-ray and metallographic analysis of the scale that forms on Ni3Ta indicates that it contains NiO, NiO·Ta2O5, Ta2O5 and also Ni and the solid solution Ni(Ta). These phase components are distributed in layers of the scale: NiO (first), NiO+NiO·Ta2O5 (second), NiO·Ta2O5+Ni+Ta2O5 (third), Ta2O5+Ni(Ta) (fourth). With a low temperature and short periods of heating there is no Nio·Ta2O5 or Ni(Ta) in the scale. Oxidation of Ni3Ta is controlled by oxygen diffusion in the scale over the direction towards the alloy. With t>850°C this mechanism changes. By analogy with oxidation of tantalum it is assumed that structural changes in the Ta2O5 lattice may be responsible for this.
引用
收藏
页码:179 / 185
页数:6
相关论文
共 50 条
  • [31] Ion Species/Energy Dependence of Irradiation-Induced Lattice Structure Transformation and Surface Hardness of Ni3Nb and Ni3Ta Intermetallic Compounds
    Kojima, H.
    Kaneno, Y.
    Ochi, M.
    Semboshi, S.
    Hori, F.
    Saitoh, Y.
    Ishikawa, N.
    Okamoto, Y.
    Iwase, A.
    MATERIALS TRANSACTIONS, 2017, 58 (05) : 739 - 748
  • [32] Anodic oxidation of Ta/Fe alloys
    Mato, S
    Alcala, G
    Thompson, GE
    Skeldon, P
    Shimizu, K
    Habazaki, H
    Quance, T
    Graham, MJ
    Masheder, D
    CORROSION SCIENCE, 2003, 45 (12) : 2881 - 2892
  • [33] OXIDATION OF HF-TA ALLOYS
    BERKOWIT.JB
    KAUFMAN, L
    CLOUGHERTY, EV
    HOPPER, R
    TRANSACTIONS OF THE METALLURGICAL SOCIETY OF AIME, 1967, 239 (05): : 750 - +
  • [34] High temperature oxidation behaviour of polycrystalline and single crystal Ta stabilized γ'-strengthened Co-Ni-Al-Ta-Cr alloys
    Xu, Wenguo
    Li, Yingju
    Qu, Shasha
    Lu, Bingyu
    Wang, Cuiping
    Yang, Yuansheng
    CORROSION SCIENCE, 2023, 225
  • [35] KINETICS OF MARTENSITE IN FE-NI-TA AND FE-NI-TA-CO ALLOYS
    RUSANENKO, VV
    PERKAS, MD
    SHAPOSHNIKOV, NG
    EDNERAL, AF
    METAL SCIENCE AND HEAT TREATMENT, 1979, 21 (9-10) : 696 - 700
  • [36] The effect of Ta on oxidation resistance of in-situ TiC/Ni composites
    Zhao, Ziyan
    Zheng, Kaiyue
    Yu, Xianghui
    Qi, Qian
    Wang, Lujie
    Liu, Yan
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2024, 118
  • [37] Oxidation at 1250°C of {Cr, Ta}-rich carbides-strengthened {Ni, Co}-based alloys
    Berthod, Patrice
    Gomis, Jean-Paul
    Aranda, Lionel
    Schweitzer, Thierry
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2022, 73 (07): : 1121 - 1131
  • [38] AN INVESTIGATION OF THE AGING OF MARTENSITE IN FE-NI-TA AND FE-NI-CO-TA ALLOYS
    EDNERAL, AF
    PERKAS, MD
    RUSANENKO, VV
    RUSSIAN METALLURGY, 1979, (03): : 118 - 123
  • [39] Investigation on the intermetallic compound Co3Ta and high-temperature phase equilibria in the Co-Ni-Ta system
    Zhou, Chenyang
    Guo, Cuiping
    Li, Changrong
    Du, Zhenmin
    INTERMETALLICS, 2019, 108 : 1 - 18
  • [40] RECRYSTALLIZATION TEXTURES IN NI-TA ALLOYS
    DETERT, K
    ZIEBS, J
    JOM-JOURNAL OF METALS, 1964, 16 (09): : 772 - &