Static and Fatigue Characteristics of Heat-Treated Ti–6Al–3Mo–2Zr–2Sn–2Nb–1.5Cr–0.1Si Alloy

被引:0
|
作者
Ramadan N. Elshaer
M. Abdelhameed
Khaled M. Ibrahim
M. El-Shennawy
A. Sobh
机构
[1] Tabbin Institute for Metallurgical Studies,Faculty of Engineering
[2] Petrojet Co.,undefined
[3] Central Metallurgical R&D Institute,undefined
[4] Helwan University,undefined
关键词
TC21 Ti-alloy; Solution treatment; Aging; Microstructure; Tensile; Fatigue;
D O I
暂无
中图分类号
学科分类号
摘要
Static and fatigue characteristics of Ti–6Al–3Mo–2Zr–2Sn–2Nb–1.5Cr–0.1Si (TC21 Ti-alloy) in as-received and heat-treated conditions were investigated at ambient temperature. Two solution treatment cycles were applied on as-received TC21 samples. The first treatment was done below β-transus temperature (Tβ) at 920 °C/15 min and the second one above β-transus temperature (Tβ) at 1020 °C/15 min followed by water quenching. Both groups of samples were aged at 600 °C for 4 h before being air-cooled. The treated samples at 920 °C showed an equiaxed α + β structure. However, a complete martensitic structure was obtained in the treated samples at 1020 °C. In addition, secondary α-platelets (αs) precipitated inside retained β-phase (βr) due to aging process. The treated samples at 920 °C revealed the best tensile properties (tensile strength, 1447 MPa, and elongation, 8%). Theoretical study using Solidworks simulation program showed a fatigue limit of 709 MPa for as-received smooth samples. The treated samples at 920 °C obtained the highest fatigue limit of 866.5 MPa. However, the treated samples at 1020 °C revealed the lowest fatigue limit of 598.5 MPa. The as-received notched samples recorded a fatigue limit of 392 MPa by a decrease in the fatigue limit of about 45% compared with the as-received smooth samples. The experimental study using rotary bending fatigue machine recorded the best fatigue limit of 782.5 MPa for treated samples at 920 °C. As-received and treated samples at 1020 °C achieved fatigue limits of 651 and 546 MPa, respectively. The as-received notched samples showed a reduction in fatigue limit by approximately 43% from 625 to 359 MPa. Hence, the treated samples at 920 °C showed the best fatigue properties. The difference between theoretical and experimental fatigue values was less than 10% in four studied conditions.
引用
收藏
页码:443 / 453
页数:10
相关论文
共 50 条
  • [41] Microstructural effects on fatigue and dwell-fatigue crack growth in α/β Ti-6Al-2Sn-4Zr-2Mo-0.1Si
    W. Shen
    W. O. Soboyejo
    A. B. O. Soboyejo
    Metallurgical and Materials Transactions A, 2004, 35 : 163 - 187
  • [42] Microstructural effects on fatigue and dwell-fatigue crack growth in α/β Ti-6Al-2Sn-4Zr-2Mo-0.1 Si
    Shen, W
    Soboyejo, ABO
    Syejo, WO
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2004, 35A (01): : 163 - 187
  • [43] Fatigue and dwell-fatigue crack growth in Ti-6Al-2Sn-4Zr-2Mo-0.1Si with elongated α/β microstructure
    Shen, W
    Soboyejo, ABO
    Soboyejo, WO
    FATIGUE - DAVID L. DAVIDSON SYMPOSIUM, 2002, : 227 - 245
  • [44] Modelling Predication of Flow Stress and Grain Size in the High Temperature Deformation of Ti-6Al-2Zr-2Sn-2Mo- 1.5Cr-2Nb Alloy
    高温变形过程中Ti-6Al-2Zr-2Sn-2Mo-1.5Cr-2Nb合金的流动应力和晶粒尺寸的模型预测
    Luo, Jiao (luojiao@nwpu.edu.cn), 1716, Science Press (47):
  • [45] HYDROGEN-ENHANCED FATIGUE CRACK-GROWTH IN TI-6AL-2SN-4ZR-2MO-0.1SI
    PAO, PS
    JOURNAL OF METALS, 1982, 34 (08): : 59 - 59
  • [46] Effect of heat treatment and silicon addition on the microstructure development of Ti-6Al-2Cr-2Mo-2Sn-2Zr alloy
    Zhang, XD
    Bonniwell, P
    Fraser, HL
    Baeslack, WA
    Evans, DJ
    Ginter, T
    Bayha, T
    Cornell, B
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 343 (1-2): : 210 - 226
  • [47] Experimental studies on the dynamic tensile behavior of Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb-Si alloy with Widmanstatten microstructure at elevated temperatures
    Gong, Xuhui
    Wang, Yu
    Xia, Yuanming
    Ge, Peng
    Zhao, Yongqing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 523 (1-2): : 53 - 59
  • [48] Influence of Optimization Techniques on Wire Electrical Discharge Machining of Ti–6Al–2Sn–4Zr–2Mo Alloy using Modeling Approach
    A. Perumal
    A. Azhagurajan
    S. Suresh Kumar
    R. Prithivirajan
    S. Baskaran
    P. R. Rajkumar
    C. Kailasanathan
    G. Venkatesan
    Journal of Inorganic and Organometallic Polymers and Materials, 2021, 31 : 3272 - 3289
  • [49] Effects of microstructure on short crack growth behavior of Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy
    Jin, O
    Mall, S
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 359 (1-2): : 356 - 367
  • [50] PROCESSING-MICROSTRUCTURE RELATIONSHIPS FOR TI-6AL-2SN-4ZR-2MO-0.1SI
    SEMIATIN, SL
    THOMAS, JF
    DADRAS, P
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1983, 14 (11): : 2363 - 2374