Static and Fatigue Characteristics of Heat-Treated Ti–6Al–3Mo–2Zr–2Sn–2Nb–1.5Cr–0.1Si Alloy

被引:0
|
作者
Ramadan N. Elshaer
M. Abdelhameed
Khaled M. Ibrahim
M. El-Shennawy
A. Sobh
机构
[1] Tabbin Institute for Metallurgical Studies,Faculty of Engineering
[2] Petrojet Co.,undefined
[3] Central Metallurgical R&D Institute,undefined
[4] Helwan University,undefined
关键词
TC21 Ti-alloy; Solution treatment; Aging; Microstructure; Tensile; Fatigue;
D O I
暂无
中图分类号
学科分类号
摘要
Static and fatigue characteristics of Ti–6Al–3Mo–2Zr–2Sn–2Nb–1.5Cr–0.1Si (TC21 Ti-alloy) in as-received and heat-treated conditions were investigated at ambient temperature. Two solution treatment cycles were applied on as-received TC21 samples. The first treatment was done below β-transus temperature (Tβ) at 920 °C/15 min and the second one above β-transus temperature (Tβ) at 1020 °C/15 min followed by water quenching. Both groups of samples were aged at 600 °C for 4 h before being air-cooled. The treated samples at 920 °C showed an equiaxed α + β structure. However, a complete martensitic structure was obtained in the treated samples at 1020 °C. In addition, secondary α-platelets (αs) precipitated inside retained β-phase (βr) due to aging process. The treated samples at 920 °C revealed the best tensile properties (tensile strength, 1447 MPa, and elongation, 8%). Theoretical study using Solidworks simulation program showed a fatigue limit of 709 MPa for as-received smooth samples. The treated samples at 920 °C obtained the highest fatigue limit of 866.5 MPa. However, the treated samples at 1020 °C revealed the lowest fatigue limit of 598.5 MPa. The as-received notched samples recorded a fatigue limit of 392 MPa by a decrease in the fatigue limit of about 45% compared with the as-received smooth samples. The experimental study using rotary bending fatigue machine recorded the best fatigue limit of 782.5 MPa for treated samples at 920 °C. As-received and treated samples at 1020 °C achieved fatigue limits of 651 and 546 MPa, respectively. The as-received notched samples showed a reduction in fatigue limit by approximately 43% from 625 to 359 MPa. Hence, the treated samples at 920 °C showed the best fatigue properties. The difference between theoretical and experimental fatigue values was less than 10% in four studied conditions.
引用
收藏
页码:443 / 453
页数:10
相关论文
共 50 条
  • [31] An investigation on fatigue and dwell-fatigue crack growth in Ti-6Al-2Sn-4Zr-2Mo-0.1Si
    Shen, W
    Soboyejo, WO
    Soboyejo, ABO
    MECHANICS OF MATERIALS, 2004, 36 (1-2) : 117 - 140
  • [32] Impact of thermal oxidation parameters on micro-hardness and hot corrosion of Ti-6Al-3Mo-2Nb-2Sn-2Zr-1.5Cr alloy
    Fathy S. Ahmed
    Mohamed A. El-Zomor
    Magdy S. Abo Ghazala
    Ramadan N. Elshaer
    Scientific Reports, 13
  • [33] Impact of thermal oxidation parameters on micro-hardness and hot corrosion of Ti-6Al-3Mo-2Nb-2Sn-2Zr-1.5Cr alloy
    Ahmed, Fathy. S. S.
    El-Zomor, Mohamed. A. A.
    Ghazala, Magdy S. Abo
    Elshaer, Ramadan. N. N.
    SCIENTIFIC REPORTS, 2023, 13 (01)
  • [34] Grain morphology control and texture characterization of laser solid formed Ti6Al2Sn2Zr3Mo1.5Cr2Nb titanium alloy
    Zhang, Q.
    Chen, J.
    Lin, X.
    Tan, H.
    Huang, W. D.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2016, 238 : 202 - 211
  • [35] Wear and Electrochemical Corrosion Behavior of Biomedical Ti–25Nb–3Mo–3Zr–2Sn Alloy in Simulated Physiological Solutions
    Huang W.
    Wang Z.
    Liu C.
    Yu Y.
    Journal of Bio- and Tribo-Corrosion, 2015, 1 (1)
  • [36] Influence of microstructure on fatigue crack growth behavior of Ti–6Al–3Nb–2Zr–1Mo alloy: Bimodal vs. lamellar structures
    Ren, Junqiang
    Wang, Qi
    Zhang, Binbin
    Yang, Dan
    Lu, Xuefeng
    Zhang, Xiaobo
    Zhang, Xudong
    Hu, Jingyu
    Intermetallics, 2021, 130
  • [37] Modelling Predication of Flow Stress and Grain Size in the High Temperature Deformation of Ti-6Al-2Zr-2Sn-2Mo-1.5Cr-2Nb Alloy
    Luo Jiao
    Gao Jun
    Li Miaoquan
    RARE METAL MATERIALS AND ENGINEERING, 2018, 47 (06) : 1716 - 1722
  • [38] Thermomechanical processing and heat treatment of Ti-6Al-2Sn-2Zr-2Cr-2Mo-Si for structural applications
    Wood, JR
    Russo, PA
    Welter, MF
    Crist, EM
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 243 (1-2): : 109 - 118
  • [39] Tuning the number density of αs precipitates in Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb-0.1Si alloys for achieving high strength
    Wang, Shu
    Liang, Yilong
    Sun, Hao
    Feng, Xin
    Huang, Chaowen
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 882
  • [40] Influence of Isothermal Forging Temperature on Microstructure and Mechanical Properties of Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb-Si Titanium Alloy
    Shi Zhifeng
    Guo Hongzhen
    Peng Xiaona
    Wang Tao
    Yao Zekun
    TI-2011: PROCEEDINGS OF THE 12TH WORLD CONFERENCE ON TITANIUM, VOL I, 2012, : 252 - 255