Effects of hydrothermal aging on glass–fiber/polyetherimide (PEI) composites

被引:1
|
作者
Taner Yilmaz
Tamer Sinmazcelik
机构
[1] Kocaeli University,Civil Aviation College
[2] Kocaeli University,Mechanical Engineering Department
来源
关键词
Thermal Cycle; Dynamic Mechanical Thermal Analysis; Fiber Protrusion; Flexural Modulus; Dynamic Mechanical Thermal Analysis;
D O I
暂无
中图分类号
学科分类号
摘要
The moisture absorption behavior and the influence of moisture on thermal and mechanical properties of glass–fiber/polyetherimide (PEI) laminates have been investigated. The laminates were exposed to hydrothermal aging at two different temperatures and high moisture rates. The properties of as-received and hydrothermally aged samples were compared. The hydrothermally aged laminates contained a large amount of moisture which caused decrease in the glass transition temperature and deterioration in mechanical properties (interlaminar shear strength, flexural modulus, bearing strength, etc.). Fractographic analysis revealed interfacial debonding as the dominant failure mechanism, indicating a strong influence of water degradation on fracture toughness results. Alterations in visco-elastic properties of glass/PEI composite which was exposed to hydrothermal aging were analyzed with the dynamic mechanical thermal analysis (DMTA) method. DMTA tests give evidence of plasticization of the PEI matrix.
引用
收藏
页码:399 / 404
页数:5
相关论文
共 50 条
  • [21] Modeling of hydrothermal aging of short flax fiber reinforced composites
    Regazzi, Arnaud
    Leger, Romain
    Corn, Stephane
    Ienny, Patrick
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2016, 90 : 559 - 566
  • [22] Electrospinning of Polyetherimide (PEI) Solution Effect of nozzle sizes on the diameter of the fiber
    Manea, Liliana Rozemarie
    Nechita, Elena
    Sandu, Ion
    REVISTA DE CHIMIE, 2015, 66 (11): : 1841 - 1845
  • [23] Improved hydrothermal aging performance of glass fiber-reinforced polymer composites via silica nanoparticle coating
    Zhang, Yongchao
    Mi, Changwen
    JOURNAL OF APPLIED POLYMER SCIENCE, 2020, 137 (19)
  • [24] Effects of MAPP Compatibilization and Acetylation Treatment Followed by Hydrothermal Aging on Polypropylene Alfa Fiber Composites
    Hamour, Noura
    Boukerrou, Amar
    Djidjelli, Hocine
    Maigret, Jean-Eudes
    Beaugrand, Johnny
    INTERNATIONAL JOURNAL OF POLYMER SCIENCE, 2015, 2015
  • [25] Effect of Low-Cycle Fatigue and Hydrothermal Aging on Tensile Properties of Open-Hole Glass Fiber/Polycarbonate and Glass Fiber/Polyamide 6 Composites
    Shao, Yuanyi
    Dong, Yuying
    Yang, Yuqiu
    FIBERS AND POLYMERS, 2021, 22 (09) : 2527 - 2534
  • [26] Effect of Low-Cycle Fatigue and Hydrothermal Aging on Tensile Properties of Open-Hole Glass Fiber/Polycarbonate and Glass Fiber/Polyamide 6 Composites
    Yuanyi Shao
    Yuying Dong
    Yuqiu Yang
    Fibers and Polymers, 2021, 22 : 2527 - 2534
  • [27] Effects of thickness and environmental temperature on fracture behaviour of polyetherimide (PEI)
    Ki-Young Kim
    Lin Ye
    Journal of Materials Science, 2004, 39 : 1267 - 1276
  • [28] Effects of thickness and environmental temperature on fracture behaviour of polyetherimide (PEI)
    Kim, KY
    Ye, L
    JOURNAL OF MATERIALS SCIENCE, 2004, 39 (04) : 1267 - 1276
  • [29] Environmental Effects on Thermal Properties of PEI/Glass Fiber Composite Materials
    Botelho, Edson Cocchieri
    Bravim Junior, Jose Carlos
    Costa, Michelle Leali
    Magalhaes de Faria, Maria Candida
    JOURNAL OF AEROSPACE TECHNOLOGY AND MANAGEMENT, 2013, 5 (02) : 241 - 254
  • [30] Impact–fatigue behaviour of unidirectional carbon fibre reinforced polyetherimide (PEI) composites
    Tamer Sınmazçelik
    A. Armağan Arıcı
    Volkan Günay