Characterization of as-deposited and annealed Cr-C alloy coatings produced from a trivalent chromium bath

被引:69
|
作者
Ghaziof, S. [1 ]
Golozar, M. A. [1 ]
Raeissi, K. [1 ]
机构
[1] Isfahan Univ Technol, Dept Mat Engn, Esfahan 8415683111, Iran
关键词
Cr-C alloy; Coating; Amorphous; Nanocrystalline; Annealing; Corrosion resistance; ELECTROCHEMICAL-BEHAVIOR; MECHANICAL-PROPERTIES; FORMIC-ACID; ELECTRODEPOSITION; LAYER;
D O I
10.1016/j.jallcom.2010.02.101
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Amorphous Cr-C alloy coatings were electrodeposited from a trivalent chromium bath containing formic acid. The effects of plating parameters such as pH and current density on composition, structure, morphology and corrosion behaviour of as-deposited coatings were investigated. Results showed that the suitable current density for Cr-C alloy electrodeposition is increased as the pH is decreased. Furthermore, by decreasing the pH, higher amount of carbon was introduced into the coatings. The Cr-C alloy coatings deposited at lower pH showed higher passive current density on Tafel plot. By annealing the amorphous Cr-C alloy coatings at 300 degrees C. a nanocrystalline structure having higher hardness was obtained. However, the corrosion resistance was seen to be impaired. Annealing at 600 degrees C led to the precipitation of Cr23C6 which resulted in a higher hardness. The formation of Cr23C6 enhanced the corrosion resistance of coatings due to an increase in corrosion potential. However, formation of micro-cells between the Cr23C6 precipitates and bulk chromium prevented the passive film formation. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:164 / 168
页数:5
相关论文
共 50 条
  • [21] Pulsed electrodeposition of microcrystalline chromium from trivalent Cr-DMF bath
    Saravanan, G.
    Mohan, S.
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 2009, 39 (08) : 1393 - 1397
  • [22] Pulsed electrodeposition of microcrystalline chromium from trivalent Cr-DMF bath
    G. Saravanan
    S. Mohan
    Journal of Applied Electrochemistry, 2009, 39 : 1393 - 1397
  • [23] Characterization of Cr-P-C/MoS2 composite plating electro-deposited from trivalent chromium
    Park, Jong-Kyu
    Seo, Sun-Kyo
    Byoun, Young-Min
    Lee, Chi-Hwan
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2018, 19 (06): : 445 - 449
  • [24] Electroplating and characterization of Cr-Al2O3 nanocomposite film from a trivalent chromium bath
    Doolabi, Mohsen Salehi
    Sadrnezhaad, Sayed Khatiboleslam
    Doolabi, Davood Salehi
    ANTI-CORROSION METHODS AND MATERIALS, 2014, 61 (04) : 205 - 214
  • [25] Anti-wear properties of Cr-C and Ni-Co alloy coatings as substitutes for conventional nanocrystalline Cr coatings
    Zeng, Zhixiang
    Zhang, Junyan
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2008, 41 (18)
  • [26] Influence of pulse parameters on electrocodeposition of Cr-Al2O3 nanocomposite coatings from trivalent chromium bath
    Sadrnezhaad, S. K. (sadrnezh@sharif.edu), 1600, Maney Publishing (06):
  • [27] Comparison of chromium coatings and electrochemical behaviour with direct current and pulse current deposition in trivalent chromium formate urea bath as alternative to conventional Cr coatings
    Mohan, S.
    Saravanan, G.
    Renganathan, N. G.
    SURFACE ENGINEERING, 2011, 27 (10) : 775 - 783
  • [28] Structure-property relations in Cr-C/a-C:H coatings deposited by reactive magnetron sputtering
    Gassner, G
    Mayrhofer, PH
    Mitterer, C
    Kiefer, J
    SURFACE & COATINGS TECHNOLOGY, 2005, 200 (1-4): : 1147 - 1150
  • [29] Effect of carbon content on resistance to cavitation erosion of Cr-C coatings deposited by Arc PVD method
    Safonov, V.
    Zykova, A.
    Steller, J.
    Tolmachova, G.
    Donkov, N.
    XXII INTERNATIONAL CONFERENCE AND SCHOOL ON QUANTUM ELECTRONICS, ICSQE 2022, 2023, 2487
  • [30] Alternating pulsed electrolysis for Fe-Cr alloy coatings using trivalent chromium solution
    Yagi, Shunsuke
    Murase, Kuniaki
    Hirato, Tetsuji
    Awakura, Yasuhiro
    SOHN INTERNATIONAL SYMPOSIUM ADVANCED PROCESSING OF METALS AND MATERIALS, VOL 7: INDUSTRIAL PRACTICE, 2006, : 479 - +