Surface morphology and helium retention on tungsten exposed to low energy and high flux helium plasma

被引:42
|
作者
Tokunaga, K
Doerner, RP
Seraydarian, R
Noda, N
Kubota, Y
Yoshida, N
Sogabe, T
Kato, T
Schedler, B
机构
[1] Kyushu Univ, Appl Mech Res Inst, Kasuga, Fukuoka 8168580, Japan
[2] Univ Calif San Diego, Fus Energy Res Program, La Jolla, CA 92093 USA
[3] Natl Inst Fus Sci, Gifu 5095292, Japan
[4] Toyo Tanso Co Ltd, Kagawa 7691614, Japan
[5] Nippon Plansee KK, Chiyoda Ku, Tokyo 1020083, Japan
[6] Plansee Aktiengesell, A-6600 Reutte, Austria
关键词
tungsten; tungsten coated carbon; helium; radiation effects; low energy; high flux;
D O I
10.1016/S0022-3115(02)01362-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Surface modification and helium retention on powder metallurgy tungsten and plasma sprayed tungsten coated CFC exposed by low energy (100 eV) high flux (3.83 x 10(21)-1.20 x 10(22) m(-2) s(-1)) helium plasma have been investigated. Fluence is about 10(26) He m(-2). It is found that fine surface morphology change occurs by the helium exposure. There is little difference of the surface modification between the powder metallurgy tungsten and the plasma sprayed tungsten. In the case that the surface morphology do not changed, two helium desorption peak appeared. The amount of desorption of helium is larger than that of deuterium from tungsten under the same exposure condition by heating up to 1273 K by TDS. In the case that fine surface morphology change occurs, desorption peak at high temperature newly appears. Surface modification such as blister is not formed on the surface exposed to helium under the same exposure condition which the blister is formed by deuterium exposure. (C) 2003 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:92 / 96
页数:5
相关论文
共 50 条
  • [21] Temperature dependence of surface topography and deuterium retention in tungsten exposed to low-energy, high-flux D plasma
    Alimov, V. Kh
    Shu, W. M.
    Roth, J.
    Lindig, S.
    Balden, M.
    Isobe, K.
    Yamanishi, T.
    JOURNAL OF NUCLEAR MATERIALS, 2011, 417 (1-3) : 572 - 575
  • [22] Temperature dependence of surface morphology and deuterium retention in polycrystalline ITER-grade tungsten exposed to low-energy, high-flux D plasma
    Alimov, V. Kh.
    Tyburska-Pueschel, B.
    Lindig, S.
    Hatano, Y.
    Balden, M.
    Roth, J.
    Isobe, K.
    Matsuyama, M.
    Yamanishi, T.
    JOURNAL OF NUCLEAR MATERIALS, 2012, 420 (1-3) : 519 - 524
  • [23] Helium retention and early stages of helium-vacancy complexes formation in low energy helium-implanted tungsten
    Lhuillier, P. E.
    Belhabib, T.
    Desgardin, P.
    Courtois, B.
    Sauvage, T.
    Barthe, M. F.
    Thomann, A. L.
    Brault, P.
    Tessier, Y.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 433 (1-3) : 305 - 313
  • [24] Surface morphology changes of tungsten exposed to high heat loading with mixed hydrogen/helium beams
    Greuner, H.
    Maier, H.
    Balden, M.
    Boeswirth, B.
    Elgeti, S.
    Schmid, K.
    Schwarz-Selinger, T.
    JOURNAL OF NUCLEAR MATERIALS, 2014, 455 (1-3) : 681 - 684
  • [25] Nanostructure evolution and surface modification of tungsten exposed to low energy, high flux deuterium plasma
    Guo, Wangguo
    Cheng, Long
    Wang, Jun
    Fu, Qingwei
    Qin, Shaoyang
    Yuan, Yue
    Lu, Guang-Hong
    FUSION ENGINEERING AND DESIGN, 2017, 125 : 473 - 478
  • [26] Deuterium retention in tungsten exposed to low-energy pure and helium-seeded deuterium plasmas
    Ogorodnikova, O. V.
    Schwarz-Selinger, T.
    Sugiyama, K.
    Alimov, V. Kh.
    JOURNAL OF APPLIED PHYSICS, 2011, 109 (01)
  • [27] Surface morphology of tungsten exposed to helium plasma at temperatures below fuzz formation threshold 1073 K
    Sakamoto, Ryuichi
    Bernard, Elodie
    Kreter, Arkadi
    Yoshida, Naoaki
    NUCLEAR FUSION, 2017, 57 (01)
  • [28] Helium self-trapping and diffusion behaviors in deformed 316L stainless steel exposed to high flux and low energy helium plasma
    Gong, Yihao
    Jin, Shuoxue
    Zhu, Te
    Cheng, Long
    Cao, Xingzhong
    You, Li
    Lu, Guanghong
    Guo, Liping
    Wang, Baoyi
    NUCLEAR FUSION, 2018, 58 (04)
  • [29] Nanostructuring of iron thin films by high flux low energy helium plasma
    Bieberle-Hutter, A.
    Tanyeli, I.
    Lavrijsen, R.
    Koopmans, B.
    Sinha, R.
    van de Sanden, M. C. M.
    THIN SOLID FILMS, 2017, 631 : 50 - 56
  • [30] Microscopic evolution of pre-damaged and undamaged tungsten exposed to low-energy and high-flux helium ions
    Yang, Qi
    Liu, Dongping
    Fan, Hongyu
    Li, Xin
    Niu, Jinhai
    Wang, Younian
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2014, 325 : 73 - 78