Surface morphology and helium retention on tungsten exposed to low energy and high flux helium plasma
被引:42
|作者:
Tokunaga, K
Doerner, RP
Seraydarian, R
Noda, N
Kubota, Y
Yoshida, N
Sogabe, T
Kato, T
Schedler, B
机构:
[1] Kyushu Univ, Appl Mech Res Inst, Kasuga, Fukuoka 8168580, Japan
[2] Univ Calif San Diego, Fus Energy Res Program, La Jolla, CA 92093 USA
[3] Natl Inst Fus Sci, Gifu 5095292, Japan
[4] Toyo Tanso Co Ltd, Kagawa 7691614, Japan
[5] Nippon Plansee KK, Chiyoda Ku, Tokyo 1020083, Japan
[6] Plansee Aktiengesell, A-6600 Reutte, Austria
关键词:
tungsten;
tungsten coated carbon;
helium;
radiation effects;
low energy;
high flux;
D O I:
10.1016/S0022-3115(02)01362-4
中图分类号:
T [工业技术];
学科分类号:
08 ;
摘要:
Surface modification and helium retention on powder metallurgy tungsten and plasma sprayed tungsten coated CFC exposed by low energy (100 eV) high flux (3.83 x 10(21)-1.20 x 10(22) m(-2) s(-1)) helium plasma have been investigated. Fluence is about 10(26) He m(-2). It is found that fine surface morphology change occurs by the helium exposure. There is little difference of the surface modification between the powder metallurgy tungsten and the plasma sprayed tungsten. In the case that the surface morphology do not changed, two helium desorption peak appeared. The amount of desorption of helium is larger than that of deuterium from tungsten under the same exposure condition by heating up to 1273 K by TDS. In the case that fine surface morphology change occurs, desorption peak at high temperature newly appears. Surface modification such as blister is not formed on the surface exposed to helium under the same exposure condition which the blister is formed by deuterium exposure. (C) 2003 Elsevier Science B.V. All rights reserved.