摘要
Resistance to chloride penetration plays a crucial role in preventing premature corrosion reinforced concrete in marine environments or when using de-icing salts. For reinforced concrete with ordinary Portland cement (OPC), the curing of concrete is vital in ensuring that the designed chloride penetration resistance of concrete is achieved. The method and duration of curing especially important with alkali-activated slag (AAS) to allow proper reaction and development the pore structure. AAS generally needs to be cured under closed conditions for at least 28 d achieve the desired quality. The objective of this study was to analyse the effect of curing time the development of chloride diffusion resistance and pore structure of alkali-activated slag mortar. Chloride diffusion resistance was analysed at 7, 28, and 90 d using non-steady-state chloride migration according to NT BUILD 492 and accelerated chloride testing according NT BUILD 443, both of which were originally developed for OPC. Mercury intrusion porosimetry (MIP) was used to evaluate the effect of pore structure on chloride penetration. The diffusion results of alkali-activated mortar showed that high resistance to chlorides can be achieved after only 7 d of curing, which is attributed to the development of fine porosity of alkali-activated slag at an early age.
引用
收藏
页数:8
相关论文
共 50 条
  • [41] Effect of Steel Fiber Volume Fraction and Curing Conditions on the Compressive Behavior of Alkali-Activated Slag Concrete
    Kang, Dae Hyun
    Kim, Hye Ran
    Yun, Hyun Do
    Development of Industrial Manufacturing, 2014, 525 : 491 - 494
  • [42] EFFECT OF CURING TEMPERATURE IN THE ALKALI-ACTIVATED BLAST-FURNACE SLAG PASTE AND THEIR STRUCTURAL INFLUENCE OF POROSITY
    de Jesus Medina-Serna, Teresita
    Paola Arredondo-Rea, Susana
    Gomez-Soberon, Jose Manuel
    Antonio Rosas-Casarez, Carlos
    Corral-Higuera, Ramon
    ADVANCES IN SCIENCE AND TECHNOLOGY-RESEARCH JOURNAL, 2016, 10 (31): : 74 - 79
  • [43] Effect of chloride salt on the phase evolution in alkali-activated slag cements through thermodynamic modelling
    Zuo, Yibing
    Applied Geochemistry, 2022, 136
  • [44] Effect of Ferrochrome Slag Substitution on High Temperature Resistance and Setting Time of Alkali-Activated Slag Mortars
    Murat Dener
    Iranian Journal of Science and Technology, Transactions of Civil Engineering, 2023, 47 : 2833 - 2843
  • [45] Effect of Ferrochrome Slag Substitution on High Temperature Resistance and Setting Time of Alkali-Activated Slag Mortars
    Dener, Murat
    IRANIAN JOURNAL OF SCIENCE AND TECHNOLOGY-TRANSACTIONS OF CIVIL ENGINEERING, 2023, 47 (05) : 2833 - 2843
  • [46] Effect of chloride salt on the phase evolution in alkali-activated slag cements through thermodynamic modelling
    Zuo, Yibing
    APPLIED GEOCHEMISTRY, 2022, 136
  • [47] Effects of CO2 Curing on Alkali-Activated Slag Paste Cured in Different Curing Conditions
    Jun, Yubin
    Han, Seong Ho
    Shin, Tae Yong
    Kim, Jae Hong
    MATERIALS, 2019, 12 (21)
  • [48] A review on alkali-activated slag concrete
    Amer, Ismail
    Kohail, Mohamed
    El-Feky, M. S.
    Rashad, Ahmed
    Khalaf, Mohamed A.
    AIN SHAMS ENGINEERING JOURNAL, 2021, 12 (02) : 1475 - 1499
  • [49] Decalcification resistance of alkali-activated slag
    Komljenovic, Miroslav M.
    Bascarevic, Zvezdana
    Marjanovic, Natasa
    Nikolic, Violeta
    JOURNAL OF HAZARDOUS MATERIALS, 2012, 233 : 112 - 121
  • [50] Shrinkage mechanisms of alkali-activated slag
    Ye, Hailong
    Radlinska, Aleksandra
    CEMENT AND CONCRETE RESEARCH, 2016, 88 : 126 - 135