Effect of curing time on the chloride diffusion of alkali-activated slag

被引:17
|
作者
Runci, Antonino [1 ]
Serdar, Marijana [1 ]
机构
[1] Univ Zagreb, Fac Civil Engn, Dept Mat, Zagreb, Croatia
基金
欧盟地平线“2020”;
关键词
Alkali activated slag; Chloride migration; Chloride diffusion; Pore structure; Electrical resistivity; Curing; FLY-ASH; PORE STRUCTURE; DURABILITY; TRANSPORT; CONCRETE; STRENGTH; CORROSION; HYDRATION; MORTARS; PASTES;
D O I
10.1016/j.cscm.2022.e00927
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Resistance to chloride penetration plays a crucial role in preventing premature corrosion reinforced concrete in marine environments or when using de-icing salts. For reinforced concrete with ordinary Portland cement (OPC), the curing of concrete is vital in ensuring that the designed chloride penetration resistance of concrete is achieved. The method and duration of curing especially important with alkali-activated slag (AAS) to allow proper reaction and development the pore structure. AAS generally needs to be cured under closed conditions for at least 28 d achieve the desired quality. The objective of this study was to analyse the effect of curing time the development of chloride diffusion resistance and pore structure of alkali-activated slag mortar. Chloride diffusion resistance was analysed at 7, 28, and 90 d using non-steady-state chloride migration according to NT BUILD 492 and accelerated chloride testing according NT BUILD 443, both of which were originally developed for OPC. Mercury intrusion porosimetry (MIP) was used to evaluate the effect of pore structure on chloride penetration. The diffusion results of alkali-activated mortar showed that high resistance to chlorides can be achieved after only 7 d of curing, which is attributed to the development of fine porosity of alkali-activated slag at an early age.
引用
收藏
页数:8
相关论文
共 50 条
  • [21] Internal Curing Effect of Pre-Soaked Zeolite Sand on the Performance of Alkali-Activated Slag
    Zhang, Guang-Zhu
    Lee, Han-Seung
    Wang, Xiao-Yong
    Han, Yi
    MATERIALS, 2021, 14 (04) : 1 - 14
  • [22] Effect of Fly Ash, MgO and Curing Solution on the Chemical Shrinkage of Alkali-Activated Slag Cement
    Fang, Yonghao
    Gu, Yamin
    Kang, Qiuboa
    ADVANCES IN BUILDING MATERIALS, PTS 1-3, 2011, 168-170 : 2008 - 2012
  • [23] Effect of Internal Curing by Super Absorbent Polymer on the Autogenous Shrinkage of Alkali-Activated Slag Mortars
    Wang, Pengju
    Chen, Haiming
    Chen, Peiyuan
    Pan, Jin
    Xu, Yangchen
    Wang, Hao
    Shen, Wenfeng
    Cao, Ke
    MATERIALS, 2020, 13 (19) : 1 - 13
  • [24] The Effect of Different Types of Internal Curing Liquid on the Properties of Alkali-Activated Slag (AAS) Mortar
    Zhang, Guang-Zhu
    Wang, Xiao-Yong
    Kim, Tae-Wan
    Lim, Jong-Yeon
    Han, Yi
    SUSTAINABILITY, 2021, 13 (04) : 1 - 16
  • [25] Effect of Electrical Double Layer on Chloride Transport in Alkali-Activated Slag Cementitious Materials
    Zhang Y.
    Fang Y.
    Xu Y.
    Xia Y.
    Yang Z.
    Jianzhu Cailiao Xuebao/Journal of Building Materials, 2023, 26 (09): : 949 - 954
  • [26] Effect of super plasticizer on properties of alkali-activated slag
    Chen, K. (kechen@cqu.edu.cn), 1600, China National Publications Import and Export (Group) Corporation (34):
  • [27] Effect of admixtures on properties of alkali-activated slag concrete
    Bakharev, T
    Sanjayan, JG
    Cheng, YB
    CEMENT AND CONCRETE RESEARCH, 2000, 30 (09) : 1367 - 1374
  • [28] Influence of Different Curing Regimes on the Performance and Microstructure of Alkali-Activated Slag Concrete
    El-Hassan, Hilal
    Shehab, Ehab
    Al-Sallamin, Abdelrahman
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2018, 30 (09)
  • [29] EFFECT OF CARBONATION ON PROPERTIES OF ALKALI-ACTIVATED SLAG BINDERS
    He, Juan
    Wu, Yonghua
    Yang, Changhui
    Gao, Qie
    Pu, Xiaolin
    REVISTA ROMANA DE MATERIALE-ROMANIAN JOURNAL OF MATERIALS, 2018, 48 (03): : 330 - 337
  • [30] Effect of Graphene Oxide on Properties of Alkali-Activated Slag
    Dong, Quanwen
    Wan, Lihua
    Luan, Congqi
    Wang, Jinbang
    Du, Peng
    MATERIALS, 2021, 14 (20)