Influence of heat treatment on degradation behavior of bio-degradable die-cast AZ63 magnesium alloy in simulated body fluid

被引:159
|
作者
Liu, Chenglong
Xin, Yunchang
Tang, Guoyi
Chu, Paul K.
机构
[1] City Univ Hong Kong, Dept Phys & Mat Sci, Kowloon, Hong Kong, Peoples R China
[2] Tsing Hua Univ, Shenzhen Grad Sch, Shenzhen 518055, Peoples R China
关键词
AZ63 magnesium alloy; aging; corrosion resistance; degradation; simulated body fluid;
D O I
10.1016/j.msea.2006.12.020
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effects of hybrid aging and solution treatments on the degradation of bio-degradable die-cast AZ63 magnesium alloy in 37 +/- 1 degrees C Tyrode's simulated body fluid have been investigated. The heat treatment is observed to alter the microstructure of the alloy. The amount Of beta-Mg17Al2 precipitates is larger and their distribution is more homogeneous. The homogeneous microstructure enhances the corrosion resistance of the alloy and the best corrosion rate achieved on the aged sample is approximately 1/2 of that of the untreated alloy. The corrosion mechanism of the aged alloy is dominated by filiform and pitting corrosion. Better understanding and control of surface corrosion will expedite the use of Mg alloys in biomedical implants. (C) 2006 Elsevier B.V. All rights reseved.
引用
收藏
页码:350 / 357
页数:8
相关论文
共 50 条
  • [21] Effect of pH Value on Wear Behavior of AZ80 Magnesium Alloy in Simulated Body Fluid
    Tao Zhu
    Ying Xiong
    Mingxue Shen
    Journal of Materials Engineering and Performance, 2023, 32 : 2853 - 2866
  • [22] Influence of Die Lubricants on Pickling and Conversion Treatment of High-Pressure Die-Cast AM30 Magnesium Alloy
    Blawert, Carsten
    da Conceicao, Thiago Ferreira
    Kainer, Karl Ulrich
    Izquierdo, Patrick
    Klose, Stephan G.
    Hoeche, Daniel
    ADVANCED ENGINEERING MATERIALS, 2012, 14 (04) : 227 - 235
  • [23] Modified nanostructured hydroxyapatite coating to control the degradation of magnesium alloy AZ31 in simulated body fluid
    Mohajernia, Sh.
    Hejazi, S.
    Eslami, A.
    Saremi, M.
    SURFACE & COATINGS TECHNOLOGY, 2015, 263 : 54 - 60
  • [24] Effect of Casting Method of AZ91 D Magnesium Alloy on the Degradation Behaviour in Simulated Body Fluid
    Akca, Cem
    MATERIALS TESTING, 2011, 53 (09) : 536 - 539
  • [25] Influence of neodymium on high cycle fatigue behavior of die cast AZ91D magnesium alloy
    Yang You
    Li Xuesong
    JOURNAL OF RARE EARTHS, 2010, 28 (03) : 456 - 460
  • [26] Influence of neodymium on high cycle fatigue behavior of die cast AZ91D magnesium alloy
    杨友
    李雪松
    JournalofRareEarths, 2010, 28 (03) : 456 - 460
  • [27] INFLUENCE OF THE HEAT TREATMENT ON THE TEXTURE OF TWIN-ROLL CAST AZ31 MAGNESIUM ALLOY
    Zimina, Mariia
    Zimina, Anna
    Pokova, Michaela
    Bohlen, Jan
    Letzig, Dietmar
    Kurz, Gerrit
    Knapek, Michal
    Cieslar, Miroslav
    METAL 2014: 23RD INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2014, : 1051 - 1056
  • [28] Corrosion Behavior of Different Coatings Prepared on the Surface of AZ80 Magnesium Alloy in Simulated Body Fluid
    Yongshui Shen
    Liuyong He
    Zengyuan Yang
    Ying Xiong
    Journal of Materials Engineering and Performance, 2020, 29 : 1609 - 1621
  • [29] Stress corrosion cracking behavior of AZ80 magnesium alloy with different orientations in simulated body fluid
    Xiong, Ying
    Zhang, Aoxuan
    Zhu, Tao
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2023, 46 (02) : 471 - 484
  • [30] Corrosion Behavior of Different Coatings Prepared on the Surface of AZ80 Magnesium Alloy in Simulated Body Fluid
    Shen, Yongshui
    He, Liuyong
    Yang, Zengyuan
    Xiong, Ying
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (03) : 1609 - 1621