Wear performance of different nitride-based coatings on plasma nitrided AISI M2 tool steel in dry and lubricated conditions

被引:45
|
作者
Hacisalihoglu, Ilyas [1 ]
Yildiz, Fatih [1 ]
Alsaran, Akgun [2 ]
机构
[1] Erzurum Tech Univ, Dept Mech Engn, TR-25240 Erzurum, Turkey
[2] Anadolu Univ, Dept Mech Engn, TR-26555 Eskisehir, Turkey
关键词
Wear; Plasma nitriding; Cathodic arc physical vapour deposition; Nitride coating; M2 tool steel; Cutting fluid; PVD;
D O I
10.1016/j.wear.2017.01.117
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
AISI M2 high speed tool steel is one of the widely used materials in the machining industry. The most common problems of this material are wearing of the cutting edge and adhesion of the work materials to the tool during the machining operations. To overcome these disadvantages, single and duplex surface treatments combining a diffusion process and a thin film ceramic coating are performed. In this study, various nitride-based coatings (TiN, TiCN, AITiN and CrN) were deposited on untreated and plasma nitrided AISI M2 high speed tool steel specimens using cathodic arc physical vapour deposition (CAPVD) technique. The plasma nitriding treatment was performed in 50%N-2-50%H-2 gas mixture at 500 degrees C for 2 h. The influences of different surface treatments on structural properties of AISI M2 steel were investigated by means of field emission scanning electron microscope, X-ray diffractometer, focused ion beam milling system, microhardness tester and optical profilometer. The tribological properties of specimens were examined in dry and cutting fluid conditions by using reciprocating sliding wear test with Al2O3 ball as a counter material. According to tribological test results, the solely coating treatment was more effective in improvement of the wear resistance of AISI M2 high-speed tool steel rather than duplex treatment. The lowest worn volume was obtained from the solely CrN coated surface. Whereas under cutting fluid condition, solely TiN and TiCN coated surfaces showed higher wear resistance. It was also observed that the friction coefficients of all specimens tested in boron-containing cutting fluid were lower and quite stable compared with dry sliding condition. (C) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:159 / 168
页数:10
相关论文
共 50 条
  • [21] Effect of Titanium Nitride, Diamond-Like Carbon and Chromium Carbonitride Coatings on the Life Time of an AISI M2 Steel Punch Forming Tool
    Yousefi M.
    Baghshahi S.
    Amiri Kerahroodi M.S.
    Journal of Bio- and Tribo-Corrosion, 2021, 7 (02)
  • [22] Wear performance and mechanisms of PCBN tool in dry hard turning of AISI D2 hardened steel
    Tang, Linhu
    Sun, Yongji
    Li, Baodong
    Shen, Jiancheng
    Meng, Guoliang
    TRIBOLOGY INTERNATIONAL, 2019, 132 : 228 - 236
  • [23] Microstructure and dry sliding wear resistance evaluation of plasma nitrided austenitic stainless steel type AISI 316LN against different sliders
    Devaraju, A.
    Elayaperumal, A.
    Alphonsa, J.
    Kailas, Satish V.
    Venugopal, S.
    SURFACE & COATINGS TECHNOLOGY, 2012, 207 : 406 - 412
  • [24] Surface morphology and mechanical strength of AISI M2 tool steel treated in abnormal glow region of plasma
    Naz M.Y.
    Shukrullah S.
    Ghaffar A.
    Shakir I.
    Ullah S.
    Sagir M.
    Pervaiz M.
    Surface Engineering and Applied Electrochemistry, 2015, 51 (1) : 58 - 64
  • [25] Dry sliding friction and wear behaviour of hardened AISI D2 tool steel with different hardness levels
    Tang, Linhu
    Gao, Chengxiu
    Huang, Jianlong
    Zhang, Hongyan
    Chang, Wenchun
    TRIBOLOGY INTERNATIONAL, 2013, 66 : 165 - 173
  • [26] Wear resistance of direct-energy-deposited AISI M2 tool steel with and without post-heat treatment
    Park, Young Keun
    Ha, Kyeongsik
    Shin, Kwang Yong
    Lee, Ki Yong
    Kim, Dong Joo
    Kwon, Se-Hun
    Lee, Wookjin
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2021, 116 (11-12): : 3917 - 3931
  • [27] Deep Cryogenic Treatment of AISI M2 Tool Steel and Optimisation of Its Wear Characteristics Using Taguchi‘s Approach
    Satish Kumar
    Mohan Nagraj
    Arunkumar Bongale
    Nitin Khedkar
    Arabian Journal for Science and Engineering, 2018, 43 : 4917 - 4929
  • [28] Wear resistance of direct-energy–deposited AISI M2 tool steel with and without post-heat treatment
    Young Keun Park
    Kyeongsik Ha
    Kwang Yong Shin
    Ki Yong Lee
    Dong Joo Kim
    Se-Hun Kwon
    Wookjin Lee
    The International Journal of Advanced Manufacturing Technology, 2021, 116 : 3917 - 3931
  • [29] LUBRICATED ROLLING WEAR OF SIC-WHISKER-REINFORCED AL2O3 COMPOSITES AGAINST M2 TOOL STEEL
    LIU, HY
    FINE, ME
    CHENG, HS
    GEIGER, AL
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (01) : 179 - 185
  • [30] Study of dry sliding wear characteristics of stellite 6B versus AISI M2 steel at various sliding velocities
    Gao, Wen
    Lian, Yong
    Xie, Guoliang
    Huang, Jinfeng
    Zhang, Le
    Ma, Minyu
    Zhao, Chao
    Zhang, Zunjun
    Liu, Kai
    Zhang, Shuguang
    Zhang, Jin
    WEAR, 2018, 402 : 169 - 178