The stress-strain behavior of WC-Co hardmetals

被引:15
|
作者
Golovchan, V. T. [1 ]
Litoshenko, N. V. [1 ]
机构
[1] Natl Acad Sci Ukraine, V Bakul Inst Superhard Mat, Dept Hardmet, UA-04074 Kiev, Ukraine
关键词
WC-Co hardmetals; Stress-strain curves; Calculating algorithm; Tensile strength; Compressive strength; In situ deformation properties of constituents; CARBIDE; ALLOYS;
D O I
10.1016/j.commatsci.2010.05.055
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The calculating algorithm for construction of the stress-strain curves of WC-Co hardmetals in simple tension and compression has been described. The algorithm is based on the mathematical means of mechanics of composite materials and in situ deformation properties of constituents. The mean field approach has been applied. The stress-strain behavior depends on such microstructural parameters as cobalt volume fraction, mean carbide grain size, and contiguity of carbide phase. The technological thermal residual microstresses have been taken into account. The wide comparison of theoretical and available experimental results has been done. It has been shown, that the given calculating algorithm has the good predictive capability. The analytical expressions of tensile and compressive strength of WC-Co hardmetals have been given. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:593 / 597
页数:5
相关论文
共 50 条
  • [31] ORIGIN OF WC SUBSTRUCTURE AND THE EFFECT OF PROCESSING ON THE MICROSTRUCTURE OF WC-Co HARDMETALS.
    Almond, Eric A.
    Roebuck, Bryan
    [J]. High Temperatures - High Pressures, 1982, 14 (02) : 143 - 154
  • [32] Effect of Heat Treatment on Structure and Properties of WC-Co Hardmetals
    Yang Jinhui Lai Hoyi (Institute of Mining and Mineral Engineering)(Department of Materials Science and Engineering
    [J]. 工程科学学报, 1991, (S2) : 29 - 34
  • [33] Surface finishing: Impact on tribological characteristics of WC-Co hardmetals
    Bonny, K.
    De Baets, P.
    Quintelier, J.
    Vleugels, J.
    Jiang, D.
    Van der Biest, O.
    Lauwers, B.
    Liu, W.
    [J]. TRIBOLOGY INTERNATIONAL, 2010, 43 (1-2) : 40 - 54
  • [34] Influence of microstructure on the abrasive edge wear of WC-Co hardmetals
    Krakhmalev, P. V.
    Rodil, T. Adeva
    Bergstrom, J.
    [J]. WEAR, 2007, 263 : 240 - 245
  • [35] CORROSION, EROSION CORROSION, AND THE FLEXURAL STRENGTH OF WC-CO HARDMETALS
    TOMLINSON, WJ
    MOLYNEUX, ID
    [J]. JOURNAL OF MATERIALS SCIENCE, 1991, 26 (06) : 1605 - 1608
  • [36] Fracture toughness measurement of WC-Co hardmetals by indentation method
    Szutkowska, M
    [J]. JOURNAL OF ADVANCED MATERIALS, 1999, 31 (03): : 3 - 7
  • [37] On the abrasion of ultrafine WC-Co hardmetals by small SiC abrasive
    Krakhmalev, P. V.
    [J]. TRIBOLOGY LETTERS, 2008, 30 (01) : 35 - 39
  • [38] DEFORMATION AND FRACTURE PROCESSES AND THE PHYSICAL METALLURGY OF WC-CO HARDMETALS
    ROEBUCK, B
    ALMOND, EA
    [J]. INTERNATIONAL MATERIALS REVIEWS, 1988, 33 (02) : 90 - 110
  • [39] Influence of cobalt content on the fatigue strength of WC-Co hardmetals
    Nakajima, Takeshi
    Hosokawa, Hiroyuki
    Shimojima, Koji
    [J]. PROGRESS IN POWDER METALLURGY, PTS 1 AND 2, 2007, 534-536 : 1201 - +
  • [40] Oxidation-induced strength degradation of WC-Co hardmetals
    Casas, B
    Ramis, X
    Anglada, M
    Salla, JM
    Llanes, L
    [J]. INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2001, 19 (4-6): : 303 - 309