High-temperature creep in an Al-8.5Fe-1.3V-1.7Si alloy processed by rapid solidification

被引:21
|
作者
Zhu, SJ [1 ]
Kucharová, K
Cadek, J
机构
[1] Univ Electrocommun, Dept Mech Engn & Intelligent Syst, Chofu, Tokyo 1828585, Japan
[2] Acad Sci Czech Republ, Inst Phys Mat, Brno 61662, Czech Republic
关键词
D O I
10.1007/s11661-000-0140-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The creep behavior of an Al-8.5Fe-1.3V-1.7Si alloy processed by rapid solidification is investigated at three temperatures ranging from 623 to 723 K. The measured minimum creep strain rates cover seven orders of magnitude. The creep behavior is associated with the true threshold stress, decreasing with increasing temperature more strongly than the shear modulus of aluminum. The minimum creep strain rate is controlled by the lattice diffusion in the alloy matrix, and the true stress exponent is close to 5. The apparent activation energy of creep depends strongly on both applied stress and temperature and is generally much higher than the activation enthalpy of lattice self-diffusion in aluminum. Also, the apparent stress exponent of minimum creep strain rate depends on applied stress as well as on temperature and is generally much higher than the true stress exponent. This behavior of both the apparent activation energy and apparent stress exponent is accounted for by the strong temperature dependence of the threshold stress-to-shear modulus ratio. The true threshold creep behavior of the alloy is interpreted in terms of athermal detachment of dislocations from fine incoherent Al-12(Fe,V)(3)Si phase particles, admitting a temperature dependence of the relaxation factor characterizing the strength of the attractive dislocation/particle interaction.
引用
收藏
页码:2229 / 2237
页数:9
相关论文
共 50 条
  • [41] Effect of Microstructure and Silicon Carbide on the Elevated Temperature Properties of Multi-layer Spray Deposition Al-8.5Fe-1.3V-1.7Si/SiCP Composite
    He, Yiqiang
    Xu, Zhengkun
    Feng, Lichao
    Chen, Jinsong
    Shang, Feng
    Chen, Hua
    Chen, Zhen-hua
    ADVANCED COMPOSITE MATERIALS, 2011, 20 (02) : 169 - 178
  • [42] 挤压对喷射成形Al-8.5Fe-1.3V-1.7Si铝合金组织与性能的影响
    张荣华
    张永安
    朱宝宏
    王峰
    材料导报, 2013, (14) : 123 - 125
  • [43] SiCp/Al-8.5Fe-1.3V-1.7Si复合材料的显微组织及室温力学性能
    陈振华
    贺毅强
    陈志钢
    尹显觉
    陈刚
    中国有色金属学报, 2007, (06) : 858 - 864
  • [44] HIGH-TEMPERATURE CREEP DEFORMATION IN A RAPIDLY SOLIDIFIED AL-FE-V-SI ALLOY
    PHARR, GM
    ZEDALIS, MS
    GILMAN, PS
    SKINNER, DJ
    JOURNAL OF METALS, 1987, 39 (10): : A21 - A21
  • [45] High temperature creep deformation of an Al-Fe-V-Si alloy
    Peng, LM
    Zhu, SJ
    Ma, ZY
    Bi, J
    Chen, HR
    Wang, FG
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 259 (01): : 25 - 33
  • [46] 晶须增强Al-8.5Fe-1.3V-1.7Si复合材料及晶须增强效果的评价
    马宗义,宁小光,潘进,李吉红,吕毓雄,毕敬
    金属学报, 1994, (21) : 420 - 426
  • [47] 旋压加工对喷射沉积Al-8.5Fe-1.3V-1.7Si合金挤压管组织和性能的影响
    肖于德
    吴永玉
    黎文献
    马正青
    王日初
    中南大学学报(自然科学版), 2005, (03) : 358 - 363
  • [48] 多道次搅拌摩擦加工改善传统铸造Al-8.5Fe-1.3V-1.7Si合金的摩擦学性能(英文)
    Z.NOURI
    R.TAGHIABADI
    TransactionsofNonferrousMetalsSocietyofChina, 2021, 31 (05) : 1262 - 1275
  • [49] Anomalous high temperature creep behaviour of an Al-8-5Fe-1.3V-1.7Si (8009Al type) alloy reinforced with alumina short fibres
    Cadek, J
    Kucharová, K
    KOVOVE MATERIALY-METALLIC MATERIALS, 2004, 42 (01): : 9 - 20
  • [50] Hardening of rapid solidification Al-Fe-V-Si alloy exposed at elevated temperature
    Xu, YH
    Long, CG
    Li, SR
    Li, WX
    Yang, SB
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 1996, 6 (04) : 130 - 132